PolyOne Geon® 90072 Vinyl Compound - Flexible (FPVC)
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
Description/Features: Market: Processing Method: PolyOne First ChoiceInformation provided by PolyOne Corporation.
| Physical Properties | Metric | English | Comments |
|
| Specific Gravity | 1.26 g/cc | 0.0455 lb/in³ | ASTM D792 |
Mechanical Properties |
|
| Hardness, Shore A | 88 | 88 | 15 sec; ASTM D2240 |
| Tensile Strength, Ultimate | 19.5 MPa | 2828 psi | Type 4 - Flexibles, 20 in/min; ASTM D638 |
| Elongation at Break | 260 % | 260 % | Type 4 - Flexibles, 20 in/min; ASTM D638 |
| Tear Strength | 87.7 kN/m | 500 pli | Die C (graves), 2 in/min; ASTM D1004 |
Thermal Properties |
|
| Brittleness Temperature | -28 °C | -18.4 °F | ASTM D746 |
Processing Properties |
|
| Melt Temperature | 177 - 188 °C | 350 - 370 °F | |
Descriptive Properties | |
| Automotive Approval | Aftermarket Only, None | |
| Product Form | Pellets | |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|