MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

COMSOL CD

Degussa AG VESTAMID® L2140B nf (dry properties) Nylon 12

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Nylon; Nylon 12; Polymer; Thermoplastic

Close Analogs: This former Creanova product line is a part of Degussa AG as of 2001.

Key Words: Polyamide

Material Notes:
ISO data as provided by the manufacturer, Creanova, Inc.

Uses: Tubing and profiles for food contact applications.

Physical PropertiesMetricEnglishComments
Density1.01 g/cc0.0365 lb/in³ 
Water Absorption1 %1 % 
Moisture Absorption at EquilibriumMax 0.5 %Max 0.5 % Humidity Absorption
Melt Flow36 g/10 min36 g/10 min 

Mechanical Properties
Tensile Strength, Yield47 MPa6820 psi 
Elongation at BreakMin 50 %Min 50 % 
Elongation at Yield5 %5 % 
Modulus of Elasticity1.5 GPa218 ksi 
Charpy Impact UnnotchedNBNB 
Charpy Impact, Notched, Low Temp0.9 J/cm²4.28 ft-lb/in² at -30°C
Charpy Impact, Unnotched Low TempNBNB at -30°C
Charpy Impact, Notched1.6 J/cm²7.61 ft-lb/in² 

Electrical Properties
Electrical ResistivityMin 1e+015 ohm-cmMin 1e+015 ohm-cm 
Surface ResistanceMin 1e+015 ohmMin 1e+015 ohm 
Dielectric Constant33 at 1 MHz.
Dielectric Constant, Low Frequency33 100 Hz
Dielectric Strength26 kV/mm660 kV/in 
Dissipation Factor0.0260.026 at 1 MHz.
Dissipation Factor, Low Frequency0.0390.039 100 Hz
Comparative Tracking Index600 V600 V 

Thermal Properties
CTE, linear 20°C100 µm/m-°C55.6 µin/in-°F in flow direction.
CTE, linear 20°C Transverse to Flow100 µm/m-°C55.6 µin/in-°F 
Deflection Temperature at 0.46 MPa (66 psi)110 °C230 °F 
Deflection Temperature at 1.8 MPa (264 psi)50 °C122 °F 
Vicat Softening Point140 °C284 °F 50°C/hr/50 N
Flammability, UL94HBHB 1.6 mm
Flammability, UL94HBHB 3.2 mm
Printer friendly version Printer friendly version


Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistant format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Instant Quotes for Quick Parts!Upload your 3D CAD model, select process, quantity, material, and instantly receive your unique, binding quote.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。