Degussa AG VESTAMID® X7099 nf (dry properties) Nylon 612
Subcategory: Nylon; Nylon 612; Polymer; Thermoplastic
Close Analogs: This former Creanova product line is a part of Degussa AG as of 2001.
Key Words: Polyamide
Material Notes: ISO data as provided by the manufacturer, Creanova, Inc.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Metric | English | Comments |
|
Density | 1.23 g/cc | 0.0444 lb/in³ | |
Water Absorption | 2 % | 2 % | |
Melt Flow | 10 g/10 min | 10 g/10 min | |
Mechanical Properties |
|
Tensile Strength, Ultimate | 130 MPa | 18900 psi | |
Elongation at Break | 5 % | 5 % | |
Modulus of Elasticity | 5.5 GPa | 798 ksi | |
Charpy Impact Unnotched | 8 J/cm² | 38.1 ft-lb/in² | |
Charpy Impact, Notched, Low Temp | 0.7 J/cm² | 3.33 ft-lb/in² | at -30°C |
Charpy Impact, Unnotched Low Temp | 2 J/cm² | 9.52 ft-lb/in² | at -30°C |
Charpy Impact, Notched | 1.2 J/cm² | 5.71 ft-lb/in² | |
Electrical Properties |
|
Electrical Resistivity | Min 1e+015 ohm-cm | Min 1e+015 ohm-cm | |
Surface Resistance | Min 1e+015 ohm | Min 1e+015 ohm | |
Dielectric Constant | 4 | 4 | 100 Hz |
Dielectric Constant, Low Frequency | 4 | 4 | 100 Hz |
Dielectric Strength | 38 kV/mm | 965 kV/in | |
Thermal Properties |
|
CTE, linear 20°C | Max 50 µm/m-°C | Max 27.8 µin/in-°F | |
Deflection Temperature at 0.46 MPa (66 psi) | 210 °C | 410 °F | |
Deflection Temperature at 1.8 MPa (264 psi) | 190 °C | 374 °F | |
Vicat Softening Point | 205 °C | 401 °F | 50°C/hr/50 N |
Flammability, UL94 | HB | HB | 3.2 mm |
Flammability, UL94 | HB | HB | 1.6 mm |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|