Degussa AG VESTAMID® X7324 nf (dry properties) Nylon 12
Subcategory: Nylon; Nylon 12; Polymer; Thermoplastic
Close Analogs: This former Creanova product line is a part of Degussa AG as of 2001. This grade is not part of the current Degussa product line.
Key Words: Polyamide
Material Notes: ISO data as provided by the manufacturer, Creanova, Inc. Uses: Bearing housing for windshield wipers.
| Physical Properties | Metric | English | Comments |
|
| Density | 1.24 g/cc | 0.0448 lb/in³ | |
| Water Absorption | 1 % | 1 % | |
| Moisture Absorption at Equilibrium | Max 0.5 % | Max 0.5 % | Humidity Absorption |
Mechanical Properties |
|
| Tensile Strength, Yield | 69 MPa | 10000 psi | |
| Elongation at Break | 12 % | 12 % | |
| Elongation at Yield | 4 % | 4 % | |
| Modulus of Elasticity | 4 GPa | 580 ksi | |
| Charpy Impact Unnotched | 7 J/cm² | 33.3 ft-lb/in² | |
| Charpy Impact, Notched, Low Temp | 1.1 J/cm² | 5.24 ft-lb/in² | at -30°C |
| Charpy Impact, Unnotched Low Temp | 6.5 J/cm² | 30.9 ft-lb/in² | at -30°C |
| Charpy Impact, Notched | 1 J/cm² | 4.76 ft-lb/in² | |
Electrical Properties |
|
| Electrical Resistivity | 5e+014 ohm-cm | 5e+014 ohm-cm | |
| Surface Resistance | Min 1e+015 ohm | Min 1e+015 ohm | |
| Dielectric Constant | 4 | 4 | at 1 MHz. |
| Dielectric Constant, Low Frequency | 4 | 4 | 100 Hz |
| Dissipation Factor | 0.0042 | 0.0042 | at 1 MHz. |
| Dissipation Factor, Low Frequency | 0.065 | 0.065 | 100 Hz |
| Comparative Tracking Index | 600 V | 600 V | |
Thermal Properties |
|
| CTE, linear 20°C | Max 50 µm/m-°C | Max 27.8 µin/in-°F | Parallel direction |
| CTE, linear 20°C Transverse to Flow | Max 50 µm/m-°C | Max 27.8 µin/in-°F | |
| Deflection Temperature at 0.46 MPa (66 psi) | 170 °C | 338 °F | |
| Deflection Temperature at 1.8 MPa (264 psi) | 130 °C | 266 °F | |
| Vicat Softening Point | 170 °C | 338 °F | 50°C/hr/50 N |
| Flammability, UL94 | HB | HB | 1.6 mm |
| Flammability, UL94 | HB | HB | 3.2 mm |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use