Degussa AG Vestamid® D22 Nylon 612 (Conditioned)
Subcategory: Nylon; Nylon 612; Polymer; Thermoplastic
Key Words: PA612, LN, 18-020
Material Notes: Description: high-viscosity base product Applications: monofilaments, bristles with high recovery for paint brushes and tooth brushes, abrasive bristles, tubes Information provided by degussa.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
| Physical Properties | Metric | English | Comments |
|
| Density | 1.06 g/cc | 0.0383 lb/in³ | ISO 1183 |
Mechanical Properties |
|
| Tensile Strength, Yield | 49 MPa | 7110 psi | ISO 527-2/1A |
| Elongation at Break | Min 50 % | Min 50 % | ISO 527-2/1A |
| Elongation at Yield | 20 % | 20 % | ISO 527-2/1A |
| Tensile Modulus | 1.7 GPa | 247 ksi | ISO 527-2/1A |
| Charpy Impact Unnotched | NB | NB | 23°C; ISO 179/1eU |
| Charpy Impact, Notched, Low Temp | 0.6 J/cm² | 2.86 ft-lb/in² | -30°C; ISO 179/1eA |
| Charpy Impact, Unnotched Low Temp | NB | NB | -30°C; ISO 179/1eU |
| Charpy Impact, Notched | 1 J/cm² | 4.76 ft-lb/in² | 23°C; ISO 179/1eA |
Electrical Properties |
|
| Volume Resistivity | 1e+014 ohm-cm | 1e+014 ohm-cm | IEC 60093 |
| Dielectric Constant | 3.7 | 3.7 | 23°C/1 MHz; IEC 60250 |
| Dielectric Constant, Low Frequency | 5 | 5 | 23°C/100 Hz; IEC 60250 |
| Dielectric Strength | 27 kV/mm | 686 kV/in | K20/P50; IEC 60243-1 |
| Dissipation Factor | 0.055 | 0.055 | 23°C/1 MHz; IEC 60250 |
| Dissipation Factor, Low Frequency | 0.065 | 0.065 | 23°C/100 Hz; IEC 60250 |
| Comparative Tracking Index | Min 600 V | Min 600 V | Test Solution A, 100 drops; IEC 60112 |
Thermal Properties |
|
| Melting Point | 215 °C | 419 °F | Peak Temperature; ISO 3146, ISO 11357 |
| Deflection Temperature at 0.46 MPa (66 psi) | 170 °C | 338 °F | When conditioned at 180°C for 1 hour; ISO 75 |
| Deflection Temperature at 1.8 MPa (264 psi) | 55 °C | 131 °F | ISO 75 |
| Deflection Temperature at 1.8 MPa (264 psi) | 75 °C | 167 °F | When conditioned at 180°C for 1 hour; ISO 75 |
| Vicat Softening Point | 180 °C | 356 °F | 50N; ISO 306 |
| Flammability, UL94 | HB | HB | 3.2 mm |
| Flammability, UL94 | HB | HB | 1.6 mm |
Descriptive Properties | |
| Electrolytic Corrosion | A1 Step | IEC 60426 |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.

|