Degussa AG Vestamid® DX9301 Black Nylon 612 with 4% Graphite (Dry as Molded)
Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 612; Polymer; Thermoplastic
Key Words: PA612, MHR, 14-030, CD04
Material Notes: Description: medium-viscosity, heat-stabilized, similar to X7094, but suffers less wear from abrasion Applications: components exposed to friction Information provided by degussa.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Metric | English | Comments |
|
Density | 1.09 g/cc | 0.0394 lb/in³ | ISO 1183 |
Moisture Absorption at Equilibrium | 1 % | 1 % | 23°C/50% R.H.; ISO 62 |
Water Absorption at Saturation | 2.7 % | 2.7 % | ISO 62 |
Linear Mold Shrinkage | 0.012 cm/cm | 0.012 in/in | 127x12.7x3.2 mm (processing cond. acc. To DIN EN ISO 1874-2) |
Linear Mold Shrinkage, Transverse | 0.014 cm/cm | 0.014 in/in | 127x12.7x3.2 mm (processing cond. acc. To DIN EN ISO 1874-2) |
Mechanical Properties |
|
Tensile Strength at Break | 65 MPa | 9430 psi | ISO 527-2/1A |
Elongation at Break | 7 % | 7 % | ISO 527-2/1A |
Tensile Modulus | 2.65 GPa | 384 ksi | ISO 527-2/1A |
Charpy Impact Unnotched | 11.5 J/cm² | 54.7 ft-lb/in² | 23°C; ISO 179/1eU |
Charpy Impact, Notched, Low Temp | 0.3 J/cm² | 1.43 ft-lb/in² | -30°C; ISO 179/1eA |
Charpy Impact, Unnotched Low Temp | 11 J/cm² | 52.4 ft-lb/in² | -30°C; ISO 179/1eU |
Charpy Impact, Notched | 0.4 J/cm² | 1.9 ft-lb/in² | 23°C; ISO 179/1eA |
Thermal Properties |
|
CTE, linear 20°C | 110 µm/m-°C | 61.1 µin/in-°F | 23-55°C, Transverse; ISO 11359 |
CTE, linear 20°C | 130 µm/m-°C | 72.2 µin/in-°F | 23-55°C, Longitudinal; ISO 11359 |
Melting Point | 215 °C | 419 °F | Peak Temperature; ISO 11357 |
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C | 365 °F | ISO 75 |
Deflection Temperature at 1.8 MPa (264 psi) | 85 °C | 185 °F | ISO 75 |
Vicat Softening Point | 187 °C | 369 °F | 50N; ISO 306 |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|