Degussa AG Vestamid® DX9320 Black 10% Glass Reinforced Nylon 612 (Conditioned)
Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 612; Polymer; Thermoplastic
Key Words: PA612-HI, MH, 14-040, GF10
Material Notes: Description: impact-resistant, 10% glass fiber reinforced, medium-viscosity, heat-stabilized Applications: housings subject to impact, coverings with molded-on elastomer seals Information provided by degussa.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
| Physical Properties | Metric | English | Comments |
|
| Density | 1.12 g/cc | 0.0405 lb/in³ | ISO 1183 |
Mechanical Properties |
|
| Tensile Strength at Break | 62 MPa | 8990 psi | ISO 527-2/1A |
| Tensile Strength, Yield | 67 MPa | 9720 psi | ISO 527-2/1A |
| Elongation at Break | 12 % | 12 % | ISO 527-2/1A |
| Elongation at Yield | 5 % | 5 % | ISO 527-2/1A |
| Tensile Modulus | 3.1 GPa | 450 ksi | ISO 527-2/1A |
| Charpy Impact Unnotched | 8.5 J/cm² | 40.5 ft-lb/in² | 23°C; ISO 179/1eU |
| Charpy Impact, Notched, Low Temp | 0.5 J/cm² | 2.38 ft-lb/in² | -30°C; ISO 179/1eA |
| Charpy Impact, Unnotched Low Temp | 8.4 J/cm² | 40 ft-lb/in² | -30°C; ISO 179/1eU |
| Charpy Impact, Notched | 1.2 J/cm² | 5.71 ft-lb/in² | 23°C; ISO 179/1eA |
Thermal Properties |
|
| Melting Point | 215 °C | 419 °F | Peak Temperature; ISO 11357 |
| Deflection Temperature at 0.46 MPa (66 psi) | 201 °C | 394 °F | ISO 75 |
| Deflection Temperature at 1.8 MPa (264 psi) | 183 °C | 361 °F | ISO 75 |
| Vicat Softening Point | 199 °C | 390 °F | 50N; ISO 306 |
| Flammability, UL94 | HB | HB | 1.6 mm |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use