Degussa AG Vestamid® E62-S3 Heat & Light Stabilized Nylon 12/PEBA Elastomer for Fiber Optic Jacketing
Subcategory: Elastomer, TPE; Nylon; Nylon 12; Polyether Block Amide (PEBA); Polymer; Thermoplastic
Material Notes: Description: E62-S3 is a PA 12 block copolymer consisting of PA 12 segments and polyether segments. The compound exhibits high flexibility and high chemical and solvent resistance. Information provided by degussa.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Metric | English | Comments |
|
Density | 1.01 g/cc | 0.0365 lb/in³ | ISO 1183 |
Water Absorption at Saturation | 1.5 % | 1.5 % | ISO 62 |
Melt Flow | 20.2 g/10 min | 20.2 g/10 min | 250°C/2.16 kg; ISO 1133 |
Mechanical Properties |
|
Hardness, Shore D | 62 | 62 | ISO 868 |
Tensile Strength, Yield | 24 MPa | 3480 psi | ISO 527-2/1A |
Elongation at Break | Min 50 % | Min 50 % | ISO 527-2/1A |
Elongation at Yield | 31 % | 31 % | ISO 527-2/1A |
Tensile Modulus | 0.36 GPa | 52.2 ksi | ISO 527-1/2 |
Charpy Impact Unnotched | NB | NB | 23°C; ISO 179/1eU |
Charpy Impact, Notched, Low Temp | 0.8 J/cm² | 3.81 ft-lb/in² | -30°C; ISO 179/1eA |
Charpy Impact, Unnotched Low Temp | NB | NB | -30°C; ISO 179/1eU |
Charpy Impact, Notched | 12 J/cm² | 57.1 ft-lb/in² | 23°C, Partial Break; ISO 179/1eA |
Thermal Properties |
|
CTE, linear 20°C | 200 µm/m-°C | 111 µin/in-°F | 23-80°C; ISO 11359 |
Melting Point | 175 - 178 °C | 347 - 352 °F | DSC |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|