MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

COMSOL CD

Degussa AG Vestamid® EX9200 Heat & Light Stabilized Nylon 12/PEBA Elastomer

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Elastomer, TPE; Nylon; Nylon 12; Polyether Block Amide (PEBA); Polymer; Thermoplastic

Material Notes:
Description: Compared to other contending thermoplastic elastomers, PA 12 elastomers are distinguished by the following properties:

  • They have low density.
  • They are highly resistant to chemicals and solvents.
  • They are easy to process and color and are easy to overmold.
  • They can be decorated easily by means of heat transfer printing.
  • They have excellent impact strength at low temperatures.
  • Their hardness and flexibility can be varied over a wide range.
  • They have high elasticity and good recovery.
  • Their mechanical properties are only slightly temperature-dependent.
  • They are free of volatile or migrating plasticizers.

Applications: decorative and protective films for sports articles and interior/exterior designs on automobiles

Information provided by degussa.

Physical PropertiesMetricEnglishComments
Density1.01 g/cc0.0365 lb/in³ ISO 1183
Water Absorption at Saturation1.5 %1.5 % ISO 62
Viscosity Test190 cm³/g190 cm³/g Viscosity Number; ISO 307

Mechanical Properties
Hardness, Shore D6868 ISO 868
Tensile Strength, Yield31 MPa4500 psi ISO 527-1, ISO 527-2
Elongation at BreakMin 200 %Min 200 % ISO 527-1, ISO 527-2
Elongation at Yield19 %19 % ISO 527-1, ISO 527-2
Tensile Modulus0.7 GPa102 ksi ISO 527-1, ISO 527-2
50% Modulus0.027 GPa3.92 ksi ISO 527-1, ISO 527-2
Charpy Impact UnnotchedNBNB 23°C; ISO 179/1eU
Charpy Impact, Notched, Low Temp0.6 J/cm²2.86 ft-lb/in² -30°C; ISO 179/1eA
Charpy Impact, Unnotched Low TempNBNB -30°C; ISO 179/1eU
Charpy Impact, Notched3.3 J/cm²15.7 ft-lb/in² 23°C, Partial Break; ISO 179/1eA

Electrical Properties
Volume Resistivity1e+011 ohm-cm1e+011 ohm-cm Spec.; IEC 60093
Surface Resistance1e+013 ohm1e+013 ohm Spec.; IEC 60093
Dielectric Constant4.64.6 23°C/1 MHz; IEC 60250
Dielectric Constant, Low Frequency7.47.4 23°C/100 Hz; IEC 60250
Dielectric Strength30 kV/mm762 kV/in K20/P50; IEC 60243-1
Dissipation Factor0.0760.076 23°C/1 MHz; IEC 60250
Dissipation Factor, Low Frequency0.150.15 23°C/100 Hz; IEC 60250
Comparative Tracking Index600 V600 V Test Solution A; IEC 60112

Thermal Properties
CTE, linear 20°C160 µm/m-°C88.9 µin/in-°F 23-55°C, Longitudinal; ISO 11359
CTE, linear 20°C160 µm/m-°C88.9 µin/in-°F 23-55°C, Transverse; ISO 11359
Deflection Temperature at 0.46 MPa (66 psi)100 °C212 °F ISO 75-2
Deflection Temperature at 1.8 MPa (264 psi)45 °C113 °F ISO 75-1
Vicat Softening Point130 °C266 °F 50N; ISO 306
Vicat Softening Point170 °C338 °F 10N; ISO 306
Flammability, UL94HBHB 1.6 mm
Printer friendly version Printer friendly version


Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistant format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Instant Quotes for Quick Parts!Upload your 3D CAD model, select process, quantity, material, and instantly receive your unique, binding quote.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。