COMSOL CD

Degussa AG Vestamid® L-CD22-M Black Flame Retardant Nylon 12

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Nylon; Nylon 12; Polymer; Thermoplastic

Key Words: PA12,MHL,18-030,CD22

Material Notes:
Description: Graphite filled, medium-viscosity, heat-stabilized

Applications: Dust caps for ignition distributor, parts with improved frictional performance

Information provided by degussa.

Physical PropertiesMetricEnglishComments
Density1.17 g/cc0.0423 lb/in³ ISO 1183
Moisture Absorption at Equilibrium0.5 %0.5 % 23°C/50% R.H. (1mm); ISO 62
Water Absorption at Saturation1.2 %1.2 % 1 mm; ISO 62
Linear Mold Shrinkage0.006 cm/cm0.006 in/in 127x12.7x3.2 mm (processing cond. acc. To ISO 1874-2)
Linear Mold Shrinkage, Transverse0.009 cm/cm0.009 in/in 127x12.7x3.2 mm (processing cond. acc. To ISO 1874-2)

Mechanical Properties
Tensile Strength at Break45 MPa6530 psi ISO 527-1/2
Tensile Strength, Yield45 MPa6530 psi ISO 527-1/2
Elongation at Break6 %6 % ISO 527-1/2
Elongation at Yield5 %5 % ISO 527-1/2
Tensile Modulus2.8 GPa406 ksi ISO 527-1/2
Charpy Impact Unnotched3.4 J/cm²16.2 ft-lb/in² 23°C; ISO 179/1eU
Charpy Impact, Notched, Low Temp0.6 J/cm²2.86 ft-lb/in² -30°C; ISO 179/1eA
Charpy Impact, Unnotched Low Temp3.4 J/cm²16.2 ft-lb/in² -30°C; ISO 179/1eU
Charpy Impact, Notched0.6 J/cm²2.86 ft-lb/in² 23°C; ISO 179/1eA

Electrical Properties
Volume Resistivity1e+012 ohm-cm1e+012 ohm-cm IEC 60093
Dielectric Constant55 23°C/1 MHz; IEC 60250
Dielectric Constant, Low Frequency77 23°C/100 Hz; IEC 60250
Dielectric Strength7 kV/mm178 kV/in K20/P50; IEC 60243-1
Dissipation Factor0.0330.033 23°C/1 MHz; IEC 60250
Dissipation Factor, Low Frequency0.0580.058 23°C/100 Hz; IEC 60250
Comparative Tracking Index175 V175 V Test Solution A, 100 drops; IEC 60112
Comparative Tracking Index200 V200 V Test Solution A, 50 drops; IEC 60112

Thermal Properties
CTE, linear 20°C80 µm/m-°C44.4 µin/in-°F 23-55°C (45x15x10 mm); ISO 11359
Melting Point178 °C352 °F Peak Temperature; ISO 3146, ISO 11357
Deflection Temperature at 0.46 MPa (66 psi)160 °C320 °F ISO 75
Deflection Temperature at 1.8 MPa (264 psi)80 °C176 °F ISO 75
Vicat Softening Point160 °C320 °F 50N; ISO 306
Vicat Softening Point175 °C347 °F 10N; ISO 306
Flammability, UL94HBHB 3.2 mm
Flammability, UL94HBHB 1.6 mm

Descriptive Properties
Electrolytic CorrosionA1 Step IEC 60426
Printer friendly version Printer friendly version


Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistant format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Instant Quotes for Quick Parts!Upload your 3D CAD model, select process, quantity, material, and instantly receive your unique, binding quote.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。