COMSOL CD

Degussa AG Vestamid® L-CF15 sw 15% Carbon Fiber Reinforced, Antistatic, Black, Electrically Conductive Nylon 12

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 12; Polymer; Thermoplastic

Key Words: PA12,MHR,16-080,CF15

Material Notes:
Description: 15% carbon fibers, medium-viscosity, heat-stabilized, with processing aid

Applications: Antistatic and electrically conductive moldings or extrudates for use in areas prone to explosions such as coal mining and other industries; e.g., housings for explosion-protected measuring equipment or for electric switches, ventilation fans for electric motors, chair castors, loudspeaker boxes, telephone and radio equipment, profiles for guide rails in assembly lines in the electronics industry. Also with electric shock protection.

Information provided by degussa.

Physical PropertiesMetricEnglishComments
Density1.08 g/cc0.039 lb/in³ ISO 1183
Moisture Absorption at Equilibrium0.5 %0.5 % 23°C/50% R.H. (1mm); ISO 62
Water Absorption at Saturation1.3 %1.3 % 1 mm; ISO 62
Linear Mold Shrinkage0.001 cm/cm0.001 in/in 127x12.7x3.2 mm (processing cond. acc. To ISO 1874-2)
Linear Mold Shrinkage, Transverse0.008 cm/cm0.008 in/in 127x12.7x3.2 mm (processing cond. acc. To ISO 1874-2)

Mechanical Properties
Tensile Strength at Break120 MPa17400 psi ISO 527-1/2
Elongation at Break5 %5 % ISO 527-1/2
Tensile Modulus8 GPa1160 ksi ISO 527-1/2
Charpy Impact Unnotched6 J/cm²28.6 ft-lb/in² 23°C; ISO 179/1eU
Charpy Impact, Notched, Low Temp1.3 J/cm²6.19 ft-lb/in² -30°C; ISO 179/1eA
Charpy Impact, Unnotched Low Temp7 J/cm²33.3 ft-lb/in² -30°C; ISO 179/1eU
Charpy Impact, Notched1.4 J/cm²6.66 ft-lb/in² 23°C; ISO 179/1eA

Electrical Properties
Volume Resistivity10000 ohm-cm10000 ohm-cm IEC 60093
Insulation Resistance10000 ohm10000 ohm Isolation Resistance (ROE DIN 43582:1983/VDE 0303 part 3; IEC 60167

Thermal Properties
CTE, linear 20°C150 µm/m-°C83.3 µin/in-°F 23-55°C (45x15x10 mm); ISO 11359
Melting Point178 °C352 °F Peak Temperature; ISO 3146, ISO 11357
Deflection Temperature at 0.46 MPa (66 psi)175 °C347 °F ISO 75
Deflection Temperature at 1.8 MPa (264 psi)170 °C338 °F ISO 75
Vicat Softening Point175 °C347 °F 10N; ISO 306
Vicat Softening Point175 °C347 °F 50N; ISO 306
Flammability, UL94HBHB 3.2 mm
Flammability, UL94HBHB 1.6 mm
Printer friendly version Printer friendly version


Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistant format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Instant Quotes for Quick Parts!Upload your 3D CAD model, select process, quantity, material, and instantly receive your unique, binding quote.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。