Degussa AG Vestamid®®/Trogamid® RD 5080 HNBR Rubber/Plastic Composite
Subcategory: Polymer; Thermoplastic
Material Notes:
Formulation| Zetpol® 3110 | 100 | | Carbon Black N 550 | 65 | | Rhenosin® W-759 | 10 | | ZnO | 2 | | HVA 2 | 4 | | Perkadox® 14/40 | 7 | Information provided by degussa.
| Physical Properties | Metric | English | Comments |
|
| Viscosity Measurement | 0.32 | 0.32 | min, Reometer at 170°C t10 |
| Viscosity Measurement | 2 | 2 | min, Reometer at 170°C t90 |
Mechanical Properties |
|
| Hardness, Shore A | 79 | 79 | 23°C |
| Tensile Strength at Break | 21.2 MPa | 3070 psi | |
| Elongation at Break | 154 % | 154 % | |
| 100% Modulus | 0.0128 GPa | 1.86 ksi | |
| Rebound | 32 % | 32 % | 23°C |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|