Degussa AG Vestamid® LX9104 Nylon 12
Subcategory: Nylon; Nylon 12; Polymer; Thermoplastic
Material Notes: Description: VESTAMID LX9104 is a halogen-free flame-retardant and flexible PA 12 compound of flammability class V-0 at0.8mm according to UL 94 and a LOI of 28%. Information provided by degussa.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Metric | English | Comments |
|
Density | 1.12 g/cc | 0.0405 lb/in³ | ISO 1183 |
Mechanical Properties |
|
Tensile Strength, Yield | 27 MPa | 3920 psi | ISO 527-2/1A |
Elongation at Break | Min 50 % | Min 50 % | ISO 527-2/1A |
Elongation at Yield | 24 % | 24 % | ISO 527-2/1A |
Tensile Modulus | 0.75 GPa | 109 ksi | ISO 527-1/2 |
Charpy Impact Unnotched | NB | NB | 23°C; ISO 179/1eU |
Charpy Impact, Notched, Low Temp | 0.3 J/cm² | 1.43 ft-lb/in² | -30°C; ISO 179/1eA |
Charpy Impact, Unnotched Low Temp | 15 J/cm² | 71.4 ft-lb/in² | -30°C, Partial Break; ISO 179/1eU |
Charpy Impact, Notched | 0.6 J/cm² | 2.86 ft-lb/in² | 23°C; ISO 179/1eA |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.

|