LNP (SABIC Innovative Plastics) VALOX® PDR7904 Polycarbonate + PBT Alloy
Subcategory: Polybutylene Terephthalate (PBT); Polycarbonate; Polyester, TP; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes:
Information provided by LNP, a GE Plastics Company.
Physical Properties | Metric | English | Comments |
|
Specific Gravity | 1.58 g/cc | 0.0571 lb/in³ | ASTM D792 |
Water Absorption | 0.06 % | 0.06 % | at 24 hrs; ASTM D570 |
Linear Mold Shrinkage | 0.002 - 0.003 cm/cm | 0.002 - 0.003 in/in | 3.20 mm; ASTM D955 |
Linear Mold Shrinkage | 0.003 - 0.005 cm/cm | 0.003 - 0.005 in/in | 6.40 mm; ASTM D955 |
Mechanical Properties |
|
Tensile Strength, Yield | 142 MPa | 20600 psi | ASTM D638 |
Elongation at Break | 4 % | 4 % | ASTM D638 |
Flexural Modulus | 9.77 GPa | 1420 ksi | ASTM D790 |
Flexural Strength | 192 MPa | 27800 psi | ASTM D790 |
Izod Impact, Notched | 1.02 J/cm | 1.91 ft-lb/in | ASTM D256 |
Thermal Properties |
|
CTE, linear 20°C | 30 µm/m-°C | 16.7 µin/in-°F | TMA, -30°C to 30°C |
Deflection Temperature at 0.46 MPa (66 psi) | 192 °C | 378 °F | Unannealed (3.20 mm); ASTM D648 |
Deflection Temperature at 1.8 MPa (264 psi) | 210 °C | 410 °F | Unannealed (3.20 mm); ASTM D648 |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to