LNP (SABIC Innovative Plastics) VALOX® VC108 Polybutylene Terephthalate
Subcategory: Polybutylene Terephthalate (PBT); Polyester, TP; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes:
Information provided by LNP, a GE Plastics Company.
Physical Properties | Metric | English | Comments |
|
Specific Gravity | 1.43 g/cc | 0.0517 lb/in³ | ASTM D792 |
Linear Mold Shrinkage | 0.003 - 0.005 cm/cm | 0.003 - 0.005 in/in | 3.20 mm; ASTM D955 |
Linear Mold Shrinkage | 0.008 - 0.01 cm/cm | 0.008 - 0.01 in/in | 6.40 mm; ASTM D955 |
Mechanical Properties |
|
Tensile Strength, Yield | 98.1 MPa | 14200 psi | ASTM D638 |
Elongation at Break | 3 % | 3 % | ASTM D638 |
Flexural Modulus | 5.98 GPa | 867 ksi | ASTM D790 |
Flexural Strength | 148 MPa | 21500 psi | ASTM D790 |
Izod Impact, Notched | 0.39 J/cm | 0.731 ft-lb/in | ASTM D256 |
Electrical Properties |
|
Surface Resistance | 1e+008 - 1e+012 ohm | 1e+008 - 1e+012 ohm | ASTM D257 |
Thermal Properties |
|
CTE, linear 20°C | 80 µm/m-°C | 44.4 µin/in-°F | TMA, -30°C to 30°C |
Deflection Temperature at 0.46 MPa (66 psi) | 199 °C | 390 °F | Unannealed (3.20 mm); ASTM D648 |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|