MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

Specialty Compounds RTP Company

RTP Company RTP 1483 HEC Polyethersulfone (PES) Nickel-Coated Carbon Fiber - EMI/RFI/ESD Protection

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)Material suppliers Material suppliers
 Export data to your CAD/FEA program

Subcategory: Polyethersulfone; Polymer; Thermoplastic

Click here to view available vendors for this material.

Physical PropertiesMetricEnglishComments
Specific Gravity1.49 g/cc0.0538 lb/in³ ASTM D792
Filler Content20 %20 % Primary Additive
Linear Mold Shrinkage0.0015 cm/cm0.0015 in/in 1/8 in (3.2 mm); ASTM D955

Mechanical Properties
Tensile Strength @ Break110 MPa16000 psi ASTM D638
Elongation at Break1.3 %1.3 % ASTM D638
Tensile Modulus10.3 GPa1500 ksi ASTM D638
Flexural Modulus11 GPa1600 ksi ASTM D638
Flexural Yield Strength193 MPa28000 psi ASTM D790
Izod Impact, Unnotched3.58 J/cm6.7 ft-lb/in 1/8 in (3.2 mm); ASTM D4812
Izod Impact, Notched0.374 J/cm0.7 ft-lb/in 1/8 in (3.2 mm); ASTM D256

Electrical Properties
Volume ResistivityMax 10 ohm-cmMax 10 ohm-cm ASTM D257
Surface ResistanceMax 1000 ohmMax 1000 ohm ESD S11.11
Surface Resistivity per SquareMax 10000 ohmMax 10000 ohm ASTM D257; ESD S11.11
Static DecayMax 2 secMax 2 sec FTMS101C; 4046.1

Thermal Properties
Deflection Temperature at 1.8 MPa (264 psi)210 °C410 °F ASTM D648
Flammability, UL94V-0V-0 1/16 in (1.5 mm)

Processing Properties
Melt Temperature343 - 377 °C650 - 710 °F 
Mold Temperature135 - 177 °C275 - 350 °F 
Drying Temperature149 °C300 °F 6 hrs
Moisture Content0.04 %0.04 % 
Dew Point-31.7 °C-25 °F 
Injection Pressure68.9 - 103 MPa10000 - 15000 psi 
Printer friendly version Printer friendly version


Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistant format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Specialty Compounds RTP Company

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。