RTP Company RTP 1403 N L Polyethersulfone (PES) Glass Fiber 20% - Lubricated - High Viscosity
Subcategory: Polyethersulfone; Polymer; Thermoplastic
Close Analogs: Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Material Notes: Glass Fiber 20% - Lubricated - High Viscosity Comments: - Glass Fiber
- High Viscosity
- Lubricated
Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties. Information provided by RTP Company.
Click here to view available vendors for this material.
Physical Properties | Metric | English | Comments |
|
Specific Gravity | 1.5 g/cc | 0.0542 lb/in³ | ASTM D792 |
Filler Content | 20 % | 20 % | |
Water Absorption | 0.4 % | 0.4 % | 24 hours at 23°C; ASTM D570 |
Linear Mold Shrinkage | 0.002 cm/cm | 0.002 in/in | 1/8 inch (3.18 mm) section; ASTM D955 |
Linear Mold Shrinkage, 6.35 mm section | 0.003 cm/cm | 0.003 in/in | 1/4 inch (6.35 mm) section; ASTM D955 |
Mechanical Properties |
|
Hardness, Rockwell R | 122 | 122 | ASTM D785 |
Tensile Strength, Ultimate | 131 MPa | 19000 psi | ASTM D638 |
Elongation at Break | 3 % | 3 % | ASTM D638 |
Modulus of Elasticity | 6.89 GPa | 1000 ksi | ASTM D638 |
Flexural Modulus | 6.89 GPa | 1000 ksi | ASTM D790 |
Flexural Yield Strength | 190 MPa | 27500 psi | ASTM D790 |
Compressive Yield Strength | 138 MPa | 20000 psi | ASTM D695 |
Izod Impact, Unnotched | 6.41 J/cm | 12 ft-lb/in | 1/8 in (3.18 mm) section; ASTM D256 |
Izod Impact, Notched | 0.801 J/cm | 1.5 ft-lb/in | 1/8 in (3.18 mm) section; ASTM D256 |
Electrical Properties |
|
Electrical Resistivity | 1e+016 ohm-cm | 1e+016 ohm-cm | ASTM D257 |
Thermal Properties |
|
CTE, linear 68°F | 34.2 µm/m-°C | 19 µin/in-°F | Flow Direction; ASTM D696 |
Deflection Temperature at 1.8 MPa (264 psi) | 213 °C | 415 °F | ASTM D648 |
Flammability, UL94 | V-0 | V-0 | (V-0) at 1/16 in (1.59 mm); Per testing by RTP Company; ASTM D3801 |
Processing Properties |
|
Processing Temperature | 343 - 366 °C | 650 - 690 °F | |
Mold Temperature | 135 - 177 °C | 275 - 350 °F | |
Injection Pressure | 68.9 - 103 MPa | 10000 - 15000 psi | |
Descriptive Properties | |
Color | Natural/Black | |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|