RTP Company RTP 1400 R-4300 UV Polyethersulfone (PES) PC Alloy - UV Stable
Subcategory: Polyethersulfone; Polymer; Thermoplastic
Close Analogs: Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Material Notes: PC Alloy - UV Stable Comments: Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties. Information provided by RTP Company.
Click here to view available vendors for this material.
Physical Properties | Metric | English | Comments |
|
Specific Gravity | 1.32 g/cc | 0.0477 lb/in³ | ASTM D792 |
Linear Mold Shrinkage | 0.0065 cm/cm | 0.0065 in/in | 1/8 inch (3.18 mm) section; ASTM D955 |
Mechanical Properties |
|
Tensile Strength, Ultimate | 76.5 MPa | 11100 psi | ASTM D638 |
Elongation at Break | Min 10 % | Min 10 % | ASTM D638 |
Modulus of Elasticity | 2.62 GPa | 380 ksi | ASTM D638 |
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
Flexural Yield Strength | 114 MPa | 16500 psi | ASTM D790 |
Izod Impact, Unnotched | 18.2 J/cm | 34 ft-lb/in | 1/8 in (3.18 mm) section; ASTM D256 |
Izod Impact, Notched | 2.14 J/cm | 4 ft-lb/in | 1/8 in (3.18 mm) section; ASTM D256 |
Electrical Properties |
|
Electrical Resistivity | 1e+015 ohm-cm | 1e+015 ohm-cm | ASTM D257 |
Thermal Properties |
|
Deflection Temperature at 1.8 MPa (264 psi) | 182 °C | 360 °F | ASTM D648 |
Processing Properties |
|
Processing Temperature | 343 - 366 °C | 650 - 690 °F | |
Mold Temperature | 135 - 177 °C | 275 - 350 °F | |
Injection Pressure | 68.9 - 103 MPa | 10000 - 15000 psi | |
Descriptive Properties | |
Color | Natural/Black | |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|