BASF Elastollan® M85A55 Polyester Type Polyurethane Elastomer
Subcategory: Elastomer, TPE; Polymer; Polyurethane, TP; Thermoplastic
Key Words: TPU Rubbers
Material Notes: The Elastollan M Series of products listed are part of a new series of polyester-based thermoplastic polyurethanes (TPU). They are specifically formulated for fast cycling in Injection Molding applications. Cycle time improvements of up to 25% over standard polyester grade urethanes can be obtained with M-series grades. They exhibit excellent abrasion resistance, toughness, and resistance to fuels. As with all TPU products this grade must be dried prior to processing. Property values below are typical values based on molded plaques cured 20 hours at 100°C before testing. Information provided by BASF Corporation.
Click here to view available vendors for this material.
Physical Properties | Metric | English | Comments |
|
Density | 1.27 g/cc | 0.0459 lb/in³ | ASTM D792 |
Mechanical Properties |
|
Hardness, Shore A | 84 | 84 | ASTM D2240 |
Tensile Strength, Ultimate | 35.9 MPa | 5210 psi | ASTM D412 |
Tensile Strength, Yield | 19.7 MPa | 2860 psi | Tensile stress at 300% elongation.; ASTM D-412 |
Tensile Strength, Yield | 8.5 MPa | 1230 psi | Tensile stress at 100% elongation.; ASTM D-412 |
Elongation at Break | 590 % | 590 % | ASTM D412 |
Tear Strength | 135 kN/m | 770 pli | ASTM D624 |
Taber Abrasion, mg/1000 Cycles | 25 | 25 | H-18 wheel; ASTM D-1044. |
Processing Properties |
|
Drying Temperature | 80 - 90 °C | 176 - 194 °F | Must be dried. Typical condition. |
Dry Time | 2 - 4 hour | 2 - 4 hour | |
Moisture Content | Max 0.03 % | Max 0.03 % | |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|