BASF Elastollan® 1185A Polyether Type Polyurethane Elastomer
Subcategory: Elastomer, TPE; Polymer; Polyurethane, TP; Thermoplastic
Key Words: TPU Rubbers
Material Notes: Processed by extrusion or injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes. They exhibit excellent low temperature properties, hydrolysis resistance and fungus resistance. These products can be injection and blow molded and extruded. As with all TPU products this grade must be dried prior to processing. Property values below are typical values based on test samples cured 20 hours at 100°C before testing. Information provided by BASF Corporation.
Click here to view available vendors for this material.
Physical Properties | Metric | English | Comments |
|
Density | 1.12 g/cc | 0.0405 lb/in³ | ASTM D792 |
Mechanical Properties |
|
Hardness, Shore A | 86 | 86 | ASTM D2240 |
Tensile Strength, Ultimate | 33 MPa | 4790 psi | ASTM D412 |
Tensile Strength, Yield | 12 MPa | 1740 psi | Tensile stress at 300% elongation.; ASTM D-412 |
Tensile Strength, Yield | 7.6 MPa | 1100 psi | Tensile stress at 100% elongation.; ASTM D-412 |
Elongation at Break | 640 % | 640 % | ASTM D412 |
Modulus of Elasticity | 0.025 GPa | 3.63 ksi | |
Poisson's Ratio | 0.25 | 0.25 | Calculated |
Shear Modulus | 0.01 GPa | 1.45 ksi | |
Tear Strength | 105 kN/m | 599 pli | ASTM D624 |
Taber Abrasion, mg/1000 Cycles | 30 | 30 | H-18 wheel; ASTM D-1044. |
Tensile Set | 70 % | 70 % | at break; ASTM D-412 |
Electrical Properties |
|
Comparative Tracking Index | Min 600 V | Min 600 V | DIN/IRC 112 |
Thermal Properties |
|
Vicat Softening Point | 85 °C | 185 °F | |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|