SABIC Innovative Plastics LEXAN FL933 Polycarbonate (North America)
Subcategory: Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line.
Physical Properties | Original Value | Comments |
|
Density | 1.29 g/cc | Molded Foam; ASTM D 792 |
Density | 1.43 g/cc | ASTM D 792 |
Water Absorption | 0.12 % | 24 hours @ 73F; ASTM D 570 |
Water Absorption at Saturation | 0.26 % | Equilibrium, 73F; ASTM D 570 |
Linear Mold Shrinkage | 0.002 - 0.004 cm/cm | Flow, 0.250 inch; ASTM D 955 |
Mechanical Properties |
|
Tensile Strength @ Yield | 10500 psi | 0.250"; ASTM D 638 |
Elongation at Break | 3 % | 0.250"; ASTM D 638 |
Tensile Modulus | 1.005e+006 psi | 0.250"; ASTM D 638 |
Flexural Modulus | 1e+006 psi | 0.250"; ASTM D 790 |
Flexural Yield Strength | 18500 psi | 0.250"; ASTM D 790 |
Izod Impact, Unnotched | 9 ft-lb/in | 73F; ASTM D 4812 |
Falling Dart Impact | 30 ft-lb | 73F; GE Test |
Electrical Properties |
|
Volume Resistivity | 2.4e+017 ohm-cm | ASTM D 257 |
Surface Resistivity per Square | Min 1.1e+017 ohm | ASTM D 257 |
Dielectric Constant | 2.61 | 1 MHz; ASTM D 150 |
Dielectric Constant | 2.7 | 100 Hz; ASTM D 150 |
Dielectric Strength | 279 V/mil | in air, 250 mils; ASTM D 149 |
Dissipation Factor | 0.0034 | 100 Hz; ASTM D 150 |
Dissipation Factor | 0.0075 | 1 MHz; ASTM D 150 |
Thermal Properties |
|
CTE, linear 68°F | 12 µin/in-°F | Flow, -40F to 200F; ASTM E 831 |
Specific Heat Capacity | 0.25 BTU/lb-°F | ASTM C 351 |
Thermal Conductivity | 0.16 W/m-K | ASTM C 177 |
Deflection Temperature at 0.46 MPa (66 psi) | 290 °F | 0.250 inch, unannealed; ASTM D 648 |
Deflection Temperature at 1.8 MPa (264 psi) | 282 °F | 0.250 inch, unannealed; ASTM D 648 |
Oxygen Index | 40.4 % | ASTM D 2863 |
Descriptive Properties | |
Foam Weight Reduction | 10% | Mechanical Properties Reported Herein (0.250") |
Foam Weight Reduction | 10% | Impact Properties Reported Herein (0.250") |
Foam Weight Reduction | 10% | Thermal Properties Reported Herein (0.250") |
Foam Weight Reduction | 10% | Physical Properties Reported Herein (0.250") |
Foam Weight Reduction | 20% | Electrical Properties Reported Herein (0.250") |
|