SABIC Innovative Plastics LEXAN LF1510A Polycarbonate (North America)
Subcategory: Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line. MatWeb has a separate entry for the European data sheet.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Original Value | Comments |
|
Density | 1.36 g/cc | ASTM D 792 |
Linear Mold Shrinkage | 0.002 - 0.003 cm/cm | Flow, 0.125 inch; ASTM D 955 |
Linear Mold Shrinkage, Transverse | 0.0035 - 0.005 cm/cm | 0.125 inch; ASTM D 955 |
Melt Flow | 8.1 g/10 min | 300C/1.2 kgf (O); ASTM D 1238 |
Mechanical Properties |
|
Tensile Strength @ Break | 10500 psi | Type I, 0.2 in/min; ASTM D 638 |
Tensile Strength @ Yield | 10500 psi | Type I, 0.2 in/min; ASTM D 638 |
Elongation at Break | 7 % | Type I, 0.2 in/min; ASTM D 638 |
Elongation at Yield | 7 % | Type I, 0.2 in/min; ASTM D 638 |
Flexural Modulus | 550000 psi | 0.05 in/min, 2" span; ASTM D 790 |
Flexural Strength | 17000 psi | 0.05 in/min, 2" span; ASTM D 790 |
Izod Impact, Unnotched | 9.5 ft-lb/in | 73F; ASTM D 4812 |
Gardner Impact @ 23°C | 150 in-lb | Instrumented Impact Total Energy, 73°F; ASTM D 3763 |
Izod Impact, Notched | 1.9 ft-lb/in | 73F; ASTM D 256 |
Electrical Properties |
|
Comparative Tracking Index | 175 - 250 V | (+/- 0.125 inch); PLC Code 3; UL 746A |
Hot Wire Ignition, HWI | Min 120 sec | (+/- 0.125 inch); PLC Code 0; UL 746A |
High Amp Arc Ignition, HAI | Min 120 arcs | Surface (+/- 0.125 inch); PLC Code 0; UL 746A |
Thermal Properties |
|
CTE, linear 68°F | 20 µin/in-°F | Flow, -40F to 100F; ASTM E 831 |
CTE, linear 68°F, Transverse to Flow | 30 µin/in-°F | from -40F to 100F; ASTM E 831 |
Deflection Temperature at 0.46 MPa (66 psi) | 271 °F | 0.125 inch, unannealed; ASTM D 648 |
Deflection Temperature at 1.8 MPa (264 psi) | 260 °F | 0.125 inch, unannealed; ASTM D 648 |
UL RTI, Electrical | 80 °C | UL 746B |
UL RTI, Mechanical with Impact | 80 °C | UL 746B |
UL RTI, Mechanical without Impact | 80 °C | UL 746B |
Flammability, UL94 | V-0 | 0.059 in. |
Descriptive Properties | |
UL File Number, USA | E121562 | |
|
Printer friendly version |
|