SABIC Innovative Plastics LEXAN LGK5030 Polycarbonate (North America)
Subcategory: Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line. MatWeb has a separate entry for the European data sheet.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Original Value | Comments |
|
Density | 1.61 g/cc | ASTM D 792 |
Water Absorption | 0.14 % | 24 hours @ 73F; ASTM D 570 |
Linear Mold Shrinkage | 0.0005 - 0.0025 cm/cm | Flow, 0.125 inch; ASTM D 955 |
Linear Mold Shrinkage, Transverse | 0.001 - 0.003 cm/cm | 0.125 inch; ASTM D 955 |
Mechanical Properties |
|
Tensile Strength @ Break | 20650 psi | Type I, 2.0 in/min; ASTM D 638 |
Elongation at Break | 4 % | Type I, 2.0 in/min; ASTM D 638 |
Flexural Modulus | 1.552e+006 psi | 0.05 in/min, 2" span; ASTM D 790 |
Flexural Strength | 27050 psi | 0.05 in/min, 2" span; ASTM D 790 |
Izod Impact, Notched | 2.3 ft-lb/in | 73F; ASTM D 256 |
Electrical Properties |
|
Dielectric Strength | 415 V/mil | in oil, 125 mils; ASTM D 149 |
Thermal Properties |
|
CTE, linear 68°F | 12 µin/in-°F | Flow, -22F to 86F; ASTM D 696 |
CTE, linear 68°F, Transverse to Flow | 22 µin/in-°F | From -22F to 86F; ASTM D 696 |
Deflection Temperature at 1.8 MPa (264 psi) | 291 °F | 0.250 inch, unannealed; ASTM D 648 |
Flammability, UL94 | V-1 | 0.058 in. |
Flammability, UL94 | V-0 | 0.11 in. |
Flammability, UL94 | 7 | 0.142 in. |
Descriptive Properties | |
UL File Number, JAPAN | E45587 | |
|
Printer friendly version |
|