Physical Properties | Original Value | Comments |
|
Density | 1.2 g/cc | ASTM D 792 |
Density | 1.2 g/cc | ISO 1183 |
Linear Mold Shrinkage | 0.005 - 0.007 cm/cm | Flow; ASTM D 955 |
Linear Mold Shrinkage | 0.006 - 0.008 cm/cm | Flow, 0.125 inch; ASTM D 955 |
Melt Flow | 13 g/10 min | Melt Volume Rate, MVR at 250C/1.2 kg; cm3/10min; ISO 1133 |
Melt Flow | 13.5 g/10 min | 250C/1.2 kgf; ASTM D 1238 |
Mechanical Properties |
|
Tensile Strength, Ultimate | 45 MPa | 50 mm/min; ISO 527 |
Tensile Strength @ Break | 8550 psi | Type I, 2.0 in/min; ASTM D 638 |
Tensile Strength, Yield | 60 MPa | 50 mm/min; ISO 527 |
Tensile Strength @ Yield | 8600 psi | Type I, 2.0 in/min; ASTM D 638 |
Elongation at Break | Min 30 % | 50 mm/min; ISO 527 |
Elongation at Break | 25.2 % | Type I, 2.0 in/min; ASTM D 638 |
Elongation at Yield | 3.8 % | Type I, 2.0 in/min; ASTM D 638 |
Elongation at Yield | 6 % | 50 mm/min; ISO 527 |
Tensile Modulus | 2.35 GPa | 1 mm/min; ISO 527 |
Tensile Modulus | 360000 psi | 2.0 in/min; ASTM D 638 |
Flexural Modulus | 2.35 GPa | 2 mm/min; ISO 178 |
Flexural Modulus | 382000 psi | 0.05 in/min, 2" span; ASTM D 790 |
Flexural Yield Strength | 90 MPa | 2 mm/min; ISO 178 |
Flexural Yield Strength | 14300 psi | 0.05 in/min, 2" span; ASTM D 790 |
Izod Impact, Notched (ISO) | 10 kJ/m² | 80*10*4 +23 C; ISO 180/ 1A |
Izod Impact, Unnotched (ISO) | NB | 80*10*4 +23 C; ISO 180/ 1U |
Izod Impact, Unnotched Low Temp (ISO) | NB | 80*10*4 -30 C; ISO 180/ 1U |
Izod Impact, Notched, Low Temp (ISO) | 6 kJ/m² | 80*10*4; -30 C; ISO 180/ 1A |
Charpy Impact Unnotched | NB | 23C, Edgew 80*10*4 sp=62; ISO 179/1eU |
Charpy Impact, Notched, Low Temp | 0.3 J/cm² | at -30C, V-notch Edgew 80*10*4 sp=62; ISO 179/1eA |
Charpy Impact, Unnotched Low Temp | NB | at -30C, Edgew 80*10*4 sp=62; ISO 179/1eU |
Charpy Impact, Notched | 0.9 J/cm² | 23C, V-notch Edgew 80*10*4 sp=62; ISO 179/1eA |
Gardner Impact @ 23°C | 516 in-lb | Instrumented Impact Total Energy, 73°F; ASTM D 3763 |
Izod Impact, Notched | 6.2 ft-lb/in | 73F; ASTM D 256 |
Thermal Properties |
|
CTE, linear 20°C | 70 µm/m-°C | Flow, 23C-80C; ISO 11359-2 |
CTE, linear 68°F | 12 µin/in-°F | Flow, -40F to 100F; ASTM E 831 |
CTE, linear 20°C Transverse to Flow | 70 µm/m-°C | 23C-80C; ISO 11359-2 |
CTE, linear 68°F, Transverse to Flow | 12 µin/in-°F | from -40F to 100F; ASTM E 831 |
Thermal Conductivity | 0.2 W/m-K | ISO 8302 |
Deflection Temperature at 0.46 MPa (66 psi) | 132 °C | HDT/Be, 0.45MPa Edgew 120*10*4 sp=100mm; ISO 75/Be |
Deflection Temperature at 0.46 MPa (66 psi) | 271 °F | 0.125 inch, unannealed; ASTM D 648 |
Deflection Temperature at 1.8 MPa (264 psi) | 122 °C | HDT/Ae, 1.82 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae |
Deflection Temperature at 1.8 MPa (264 psi) | 242 °F | 0.125 inch, unannealed; ASTM D 648 |
Vicat Softening Point | 136 °C | B/50; ISO 306 |
Vicat Softening Point | 140 °C | B/120; ISO 306 |
Vicat Softening Point | 278 °F | Rate B; ASTM D 1525 |
Optical Properties |
|
Transmission, Visible | 89 % | 0.100 inch; ASTM D 1003 |
Descriptive Properties |
|
Hardness, H358/30 (MPa) | 95 | ISO 2039/1 |
Yellowness Index, 0.100 | 1.2 | ASTM D 1925 |
|
Printer friendly version |