SABIC Innovative Plastics LEXAN OQ4320R Polycarbonate (North America)
Subcategory: Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Original Value | Comments |
|
Density | 1.2 g/cc | ASTM D 792 |
Water Absorption | 0.15 % | 24 hours @ 73F; ASTM D 570 |
Linear Mold Shrinkage | 0.005 - 0.007 cm/cm | Flow, 0.125 inch; ASTM D 955 |
Melt Flow | 12.5 g/10 min | 300C/1.2 kgf (O); ASTM D 1238 |
Mechanical Properties |
|
Tensile Strength @ Yield | 9000 psi | Type I, 2.0 in/min; ASTM D 638 |
Elongation at Break | 130 % | Type I, 2.0 in/min; ASTM D 638 |
Elongation at Yield | 7 % | Type I, 2.0 in/min; ASTM D 638 |
Flexural Modulus | 340000 psi | 0.05 in/min, 2" span; ASTM D 790 |
Flexural Yield Strength | 14000 psi | 0.05 in/min, 2" span; ASTM D 790 |
Gardner Impact @ 23°C | 565 in-lb | Instrumented Impact Energy @ peak, 73F; ASTM D 3763 |
Falling Dart Impact | 125 ft-lb | 73F; ASTM D 3029 |
Izod Impact, Notched | 14 ft-lb/in | 73F; ASTM D 256 |
Thermal Properties |
|
Deflection Temperature at 0.46 MPa (66 psi) | 280 °F | 0.250 inch, unannealed; ASTM D 648 |
Deflection Temperature at 1.8 MPa (264 psi) | 270 °F | 0.250 inch, unannealed; ASTM D 648 |
Vicat Softening Point | 310 °F | Rate B; ASTM D 1525 |
|