SABIC Innovative Plastics LEXAN WR5210R Polycarbonate (North America)
Subcategory: Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line. MatWeb has a separate entry for the European data sheet.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Original Value | Comments |
|
Linear Mold Shrinkage | 0.004 - 0.006 cm/cm | Flow, 0.125 inch; ASTM D 955 |
Melt Flow | 21.5 g/10 min | 300C/1.2 kgf (O); ASTM D 1238 |
Mechanical Properties |
|
Tensile Strength @ Break | 8000 psi | Type I, 2.0 in/min; ASTM D 638 |
Tensile Strength @ Yield | 7800 psi | Type I, 2.0 in/min; ASTM D 638 |
Elongation at Break | 75 % | Type I, 2.0 in/min; ASTM D 638 |
Flexural Modulus | 295000 psi | 0.05 in/min, 2" span; ASTM D 790 |
Flexural Yield Strength | 12100 psi | 0.05 in/min, 2" span; ASTM D 790 |
Gardner Impact @ 23°C | 344 in-lb | Instrumented Impact Energy @ peak, 73F; ASTM D 3763 |
Izod Impact, Notched | 3.4 ft-lb/in | 73F; ASTM D 256 |
Electrical Properties |
|
Comparative Tracking Index | 175 - 250 V | (+/- 0.125 inch); PLC Code 3; UL 746A |
Hot Wire Ignition, HWI | 30 - 60 sec | (+/- 0.125 inch); PLC Code 2; UL 746A |
High Amp Arc Ignition, HAI | Min 120 arcs | Surface (+/- 0.125 inch); PLC Code 0; UL 746A |
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80 mm/min | (+/- 0.125 inch); PLC Code 2; UL 746A |
Thermal Properties |
|
Deflection Temperature at 1.8 MPa (264 psi) | 260 °F | 0.250 inch, unannealed; ASTM D 648 |
UL RTI, Electrical | 80 °C | UL 746B |
UL RTI, Mechanical with Impact | 80 °C | UL 746B |
UL RTI, Mechanical without Impact | 80 °C | UL 746B |
Flammability, UL94 | HB | 0.059 in. |
Optical Properties |
|
Gloss | 52 % | Untextured, 60 degrees; ASTM D 523 |
Descriptive Properties | |
UL File Number, USA | E121562 | |
|