SABIC Innovative Plastics LEXAN EXL1330 Polycarbonate (Europe)
Subcategory: Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their European product line. This product is also a part of their North American product line.
Physical Properties | Original Value | Comments |
|
Density | 1.18 g/cc | ISO 1183 |
Linear Mold Shrinkage | 0.007 - 0.009 cm/cm | Flow; ASTM D 955 |
Melt Flow | 9 g/10 min | cm3/10min; Melt Volume Rate, MVR at 300C/1.2 kg; ISO 1133 |
Mechanical Properties |
|
Hardness, H358/30 | 90 MPa | ISO 2039/1 |
Tensile Strength, Ultimate | 56 MPa | 50 mm/min; ISO 527 |
Tensile Strength, Yield | 55 MPa | 50 mm/min; ISO 527 |
Elongation at Break | Min 100 % | 50 mm/min; ISO 527 |
Elongation at Yield | 5 % | 50 mm/min; ISO 527 |
Tensile Modulus | 2.1 GPa | 1 mm/min; ISO 527 |
Flexural Modulus | 2.1 GPa | 2 mm/min; ISO 178 |
Flexural Yield Strength | 85 MPa | 2 mm/min; ISO 178 |
Izod Impact, Notched (ISO) | 60 kJ/m² | 80*10*4 +23 C; ISO 180/ 1A |
Izod Impact, Notched, Low Temp (ISO) | 45 kJ/m² | 80*10*4 -30 C; ISO 180/ 1A |
Charpy Impact, Notched, Low Temp | 5 J/cm² | at -30C, V-notch Edgew 80*10*4 sp=62; ISO 179/1eA |
Charpy Impact, Notched | 6 J/cm² | 23C, V-notch Edgew 80*10*4 sp=62; ISO 179/1eA |
Thermal Properties |
|
CTE, linear 20°C | 72 µm/m-°C | 23C-80C, flow; ISO 11359-2 |
CTE, linear 20°C Transverse to Flow | 72 µm/m-°C | 23C-80C; ISO 11359-2 |
Deflection Temperature at 0.46 MPa (66 psi) | 136 °C | HDT/Be, 0.45MPa Edgew 120*10*4 sp=100mm; ISO 75/Be |
Deflection Temperature at 1.8 MPa (264 psi) | 125 °C | HDT/Ae, 1.82 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae |
Vicat Softening Point | 143 °C | B/50; ISO 306 |
Vicat Softening Point | 145 °C | B/120; ISO 306 |
Descriptive Properties | |
Ball Pressure Test, 125 C +/- 2 C | PASS | IEC 60035-1 |
|