SABIC Innovative Plastics LEXAN® ML1913 Polycarbonate, Unfilled, Injection Grade
Subcategory: Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Data for 3.2 mm (1/8 in) samples unless otherwise noted. Data provided by GE Plastics.
Physical Properties | Original Value | Comments |
|
Density | 1.28 g/cc | ASTM D792 |
Water Absorption | 0.09 % | 24 hrs; 20°C; ASTM D570 |
Mechanical Properties |
|
Tensile Strength, Ultimate | 64 MPa | ASTM D638 |
Elongation at Break | 15 % | ASTM D638 |
Flexural Modulus | 3.4 GPa | 3.2 mm sample; ASTM D790 |
Flexural Yield Strength | 103 MPa | ASTM D790 |
Izod Impact, Notched | 0.9 J/cm | 3.2 mm sample; ASTM D256 |
Thermal Properties |
|
Deflection Temperature at 1.8 MPa (264 psi) | 132 °C | 6.4 mm (0.25 in.) sample; ASTM D648 |
|