SABIC Innovative Plastics LEXAN® SP7700 Polycarbonate, 10% Carbon Filled, Injection Grade
Subcategory: Filled/Reinforced Thermoplastic; Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Data for 3.2 mm (1/8 in) samples unless otherwise noted. Data provided by GE Plastics.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Original Value | Comments |
|
Density | 1.25 g/cc | ASTM D792 |
Linear Mold Shrinkage | 0.001 - 0.003 cm/cm | 3.2 mm sample |
Mechanical Properties |
|
Tensile Strength, Ultimate | 104 MPa | ASTM D638 |
Elongation at Break | 8 % | ASTM D638 |
Flexural Modulus | 6.7 GPa | 3.2 mm sample; ASTM D790 |
Flexural Yield Strength | 163 MPa | ASTM D790 |
Izod Impact, Notched | 1 J/cm | 3.2 mm sample; ASTM D256 |
Thermal Properties |
|
Deflection Temperature at 1.8 MPa (264 psi) | 100 °C | 6.4 mm (0.25 in.) sample; ASTM D648 |
Flammability, UL94 | V-0 | 1.2 mm |
|