SABIC Innovative Plastics LEXAN® ML7038 PC, Unfilled
Subcategory: Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Data provided by GE Plastics. This product grade was removed from GE's database of standard products in 1998.
Physical Properties | Original Value | Comments |
|
Density | 1.2 g/cc | ASTM D792 |
Melt Flow | 70 g/10 min | 300°C/1.2kg |
Mechanical Properties |
|
Tensile Strength, Ultimate | 63 MPa | ASTM D638 |
Elongation at Break | 40 % | ASTM D638 |
Flexural Modulus | 2.067 GPa | ASTM D790 |
Izod Impact, Notched | 2.65 J/cm | 23°C (73.4°F) |
Thermal Properties |
|
Deflection Temperature at 1.8 MPa (264 psi) | 121 °C | ASTM D648 |
Processing Properties |
|
Processing Temperature | 304 - 332 °C | melt temperature |
Mold Temperature | 65 - 93 °C | |
|