SABIC Innovative Plastics LEXAN® SP7606 PC, Unfilled, Flame-Retarded
Subcategory: Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Data provided by GE Plastics. This product grade was removed from GE's database of standard products in 1998.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Original Value | Comments |
|
Density | 1.44 g/cc | ASTM D792 |
Water Absorption | 0.12 % | 24 hrs at 23°C; ASTM D570 |
Linear Mold Shrinkage | 0.0015 - 0.0025 cm/cm | at 3.2 mm. |
Mechanical Properties |
|
Tensile Strength, Ultimate | 116 MPa | ASTM D638 |
Flexural Modulus | 6.89 GPa | ASTM D790 |
Flexural Yield Strength | 176 MPa | ASTM D790 |
Izod Impact, Notched | 0.85 J/cm | 23°C (73.4°F) |
Electrical Properties |
|
Electrical Resistivity | 1e+017 ohm-cm | ASTM D257 |
Thermal Properties |
|
Deflection Temperature at 1.8 MPa (264 psi) | 100 °C | ASTM D648 |
Flammability, UL94 | V-0 | 0.8 mm |
|
Printer friendly version |
|