ZYLAR acrylic copolymers - The Clear Alternative to Polycarbonate and ABS
SABIC Innovative Plastics Lexan® 9034 Polycarbonate Sheet
Subcategory: Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Lexan® 9034 uncoated polycarbonate sheet is the standard grade of LEXAN sheet for transparent protective glazing. High-impact LEXAN 9034 sheet can be utilized for primary glazing, or on either side of existing glazing for economical protection against breakage or intrusion. A better insulator than glass, LEXAN 9034 sheet contributes to lower energy costs. Information provided by Aurora Technologies.
Physical Properties | Original Value | Comments |
|
Water Absorption | 0.15 % | |
Mechanical Properties |
|
Hardness, Rockwell M | 70 | |
Tensile Strength, Yield | 9000 psi | |
Flexural Strength | 13500 psi | |
Compressive Strength | 12.5 ksi | |
Shear Strength | 6000 psi | |
Izod Impact, Notched | 12 - 16 ft-lb/in | Edgewise |
Electrical Properties |
|
Dielectric Constant | 2.96 | 10 Hz |
Dielectric Constant | 3.17 | 60 Hz |
Dissipation Factor | 0.0009 | 60 Hz |
Dissipation Factor | 0.01 | 1 MHz |
Arc Resistance | 10 - 11 sec | Stainless Steel Strips |
Arc Resistance | 120 sec | Tungsten Electrodes |
Thermal Properties |
|
Flammability Test | Min 1 | inches; Horizontal Burn (Flame Spread) |
Optical Properties |
|
Transmission, Visible | 88 % | 1/8 in disk |
Descriptive Properties | |
Color | Clear | |
|