ITW Devcon Rubber Repair / Castable Urethane Flexane® Fast Cure, Black
Subcategory: Adhesives, Sealants, and Coatings; Polymer; Polyurethane, TS; Thermoset
Material Notes:
Information provided by ITW Devcon
Physical Properties | Original Value | Comments |
|
Density | 0.0426 lb/in³ | |
Mechanical Properties |
|
Hardness, Shore A | 88 | Cured; ASTM D2240 |
Tensile Strength @ Break | 2400 psi | ASTM D412 |
Elongation at Break | Max 500 % | ASTM D412 |
Tear Strength | 275 pli | ASTM D624 |
Taber Abrasion, mg/1000 Cycles | 220 | H-18 wheel (1000 gram load) |
Electrical Properties |
|
Dielectric Strength | 350 V/mil | ASTM D149 |
Thermal Properties |
|
Maximum Service Temperature, Air | 120 °F | wet |
Maximum Service Temperature, Air | 180 °F | dry |
Shrinkage | 0.14 % | Cured; ASTM D2566 |
Processing Properties |
|
Cure Time | 3 hour | Functional cure |
Pot Life | 8 min | at 75°F |
Descriptive Properties | |
Coverage per pound, in² @ 1/4" thickness | 94 | |
Mix ratio by weight (Resin:Hardener) | 80:20 | |
|