LNP (SABIC Innovative Plastics) LEXAN® BFL2000 Polycarbonate
Subcategory: Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes:
Information provided by LNP, a GE Plastics Company.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Original Value | Comments |
|
Specific Gravity | 1.29 g/cc | ASTM D792 |
Mechanical Properties |
|
Tensile Strength, Yield | 62.8 MPa | ASTM D638 |
Elongation at Break | 190 % | ASTM D638 |
Flexural Modulus | 2.38 GPa | ASTM D790 |
Flexural Strength | 92.2 MPa | ASTM D790 |
Thermal Properties |
|
Deflection Temperature at 0.46 MPa (66 psi) | 125 °C | Unannealed (3.20 mm); ASTM D648 |
|
Printer friendly version |
|