LNP (SABIC Innovative Plastics) LEXAN® BFL3501 Polycarbonate
Subcategory: Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes:
Information provided by LNP, a GE Plastics Company.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Original Value | Comments |
|
Specific Gravity | 1.26 g/cc | ASTM D792 |
Water Absorption | 0.15 % | at 24 hrs; ASTM D570 |
Linear Mold Shrinkage | 0.005 - 0.007 cm/cm | 3.20 mm; ASTM D955 |
Mechanical Properties |
|
Tensile Strength, Yield | 61 MPa | ASTM D638 |
Elongation at Break | 220 % | ASTM D638 |
Flexural Modulus | 2.41 GPa | ASTM D790 |
Flexural Strength | 92.6 MPa | ASTM D790 |
Izod Impact, Notched | 5.57 J/cm | ASTM D256 |
Thermal Properties |
|
CTE, linear 20°C | 70 µm/m-°C | TMA, -30°C to 30°C |
Deflection Temperature at 0.46 MPa (66 psi) | 131 °C | Unannealed (3.20 mm); ASTM D648 |
|