LNP (SABIC Innovative Plastics) LEXAN® EXCP0101 Polycarbonate, 10% Carbon Fiber Reinforced
Subcategory: Filled/Reinforced Thermoplastic; Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Business and computer equipment. - Features: Flame Retardant
- Forms: Pellets
- Processing Method: Injection Molding
Information provided by LNP, a GE Plastics Company.
Physical Properties | Original Value | Comments |
|
Specific Gravity | 1.25 g/cc | ASTM D792 |
Linear Mold Shrinkage | 0.002 - 0.005 cm/cm | 3.18 mm; ASTM D955 |
Linear Mold Shrinkage, Transverse | 0.004 - 0.006 cm/cm | 3.18 mm; ASTM D955 |
Mechanical Properties |
|
Tensile Strength at Break | 100 MPa | Type I, 5mm/min; ASTM D638 |
Tensile Strength, Yield | 100 MPa | Type I, 5mm/min; ASTM D638 |
Elongation at Break | 3 % | Type I, 5mm/min; ASTM D638 |
Elongation at Yield | 3 % | Type I, 5mm/min; ASTM D638 |
Tensile Modulus | 6.48 GPa | 5 mm/min; ASTM D638 |
Flexural Modulus | 6.45 GPa | (50.8 mm Span) 1mm/min; ASTM D790 |
Flexural Strength | 170 MPa | at Break, (50.8 mm Span) 1mm/min; ASTM D790 |
Izod Impact, Notched | 0.534 J/cm | ASTM D256 |
Izod Impact, Unnotched | 5.6 J/cm | ASTM D256 |
Falling Dart Impact | 8.47 J | ASTM D3763 |
Electrical Properties |
|
Volume Resistivity | 4000 ohm-cm | IEC 60093 |
Surface Resistance | 100000 ohm | IEC 60093 |
Thermal Properties |
|
Deflection Temperature at 0.46 MPa (66 psi) | 142 °C | Unannealed (3.18 mm); ASTM D648 |
Deflection Temperature at 1.8 MPa (264 psi) | 138 °C | Unannealed (3.18 mm); ASTM D648 |
Processing Properties |
|
Rear Barrel Temperature | 266 - 288 °C | |
Middle Barrel Temperature | 277 - 299 °C | |
Front Barrel Temperature | 288 - 310 °C | |
Nozzle Temperature | 282 - 304 °C | |
Melt Temperature | 288 - 310 °C | |
Mold Temperature | 71.1 - 93.3 °C | |
Drying Temperature | 121 °C | |
Dry Time | 3 - 8 hour | |
Moisture Content | 0.02 % | Suggested |
Back Pressure | 0.345 - 0.689 MPa | |
Clamp Pressure | 41 - 69 MPa | |
Shot Size | 40 - 60 % | Suggested |
Vent Depth | 0.0025 - 0.0076 cm | |
Screw Speed | 40 - 70 rpm | |
|
Printer friendly version |
|