PolyPlastics Duranex® 3400 Polybutylene Terephthalate (PBT), Standard, 40% GF filled
Subcategory: Filled/Reinforced Thermoplastic; Polybutylene Terephthalate (PBT); Polyester, TP; Polymer; Thermoplastic
Material Notes: DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers or other inorganic filler additives. Therefore, as grades can be optimally designed depending on the application, various grades are provided, including flame-retardant grades, reinforced grades, and impact-resistant grades. DURANEX®, due to its mechanical strength, heat stability, electrical resistivity and wear and abrasion-resistance, offers great potential as a well-balanced, highly reliable material, having a wide variety of applications including electronic / electro-mechanical and automobile parts and various other functional parts. Not only does it have well-balanced properties as a raw material, DURANEX® also assures moldability, dimensional stability, glossy surfaces and various fabrication capabilities providing higher added value. Information provided by PolyPlastics.
| Physical Properties | Original Value | Comments |
|
| Density | 1.64 g/cc | ISO 1183 |
| Filler Content | 40 % | Glass fiber |
Mechanical Properties |
|
| Tensile Strength, Ultimate | 155 MPa | ISO 527-1, 2 |
| Elongation at Break | 2 % | ISO 527-1, 2 |
| Flexural Modulus | 12.5 GPa | ISO 178 |
| Flexural Strength | 245 MPa | ISO 178 |
| Charpy Impact, Notched | 1.2 J/cm² | ISO 179/1eA |
Electrical Properties |
|
| Volume Resistivity | 3e+016 ohm-cm | IEC 60093 |
| Surface Resistance | 2e+016 ohm | IEC 60093 |
| Dielectric Strength | 24 kV/mm | IEC 60243-1 |
Thermal Properties |
|
| Deflection Temperature at 1.8 MPa (264 psi) | 214 °C | ISO 75-1, 2 |
| Flammability, UL94 | HB | |
|