Pyrotek MC-1 Metal Ceramic Thermocouple Protection Tube

 

Material Notes:
For casting, MC-1 thermocouple protection tubes are a unique blend of metal and ceramic, exhibiting properties not found solely in either individual material. MC-1 tubes offer high thermal conductivity and excellent sensitivity to temperature changes in high temperature applications. Preheating to 482°C before immersion in molten metal at 1093°C or higher is recommended.

Applications

  • Molten copper and brass to 1149°C
  • Corrosive SO2 and SO3 gas to 1371°C and SO3 and HF gas to 1093°C
  • Molten zinc to 871°C
  • Molten lead to 343°C
  • Atmosphere directly above molten glass in an open hearth glass furnace
  • Carbon bake furnaces
  • Steel mill soaking pits
  • Not recommended for use in molten aluminum or glass, carburizing or nitrating atmospheres, cryolite, or copper alloys above 1149°C

Advantages

  • Excellent oxidation resistance
  • Thermal conductivity comparable to stainless steel
  • Resists wetting by many metals and alloys, and basic furnace slags
  • Resistant to oxidizing atmospheres over 1204°C
  • Good wear resistance
  • Resistant to sliding friction
  • Good strength at temperatures up to 1538°C
  • Low porosity prohibits gas ingress

Information provided by Pyrotek.

Available Properties
  • Density
  • Flexural Strength
  • Compressive Strength
  • CTE, linear 20°C
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Maximum Service Temperature, Inert
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。