ASTM 897 Grade 5 (230-185-00), Austempered Ductile Iron

 

Subcategory: Ductile Iron; Alloy Cast Iron; Metal

Key Words: ADI; ASTM 897 Grade 5

Material Notes:
ASTM 897 (in-lb units) 230-185-00
ASTM 897M (SI units) 1600-1300-00. The values below are typical properties, not guaranteed minimums.

Austempered Ductile Iron (ADI) offers low cost, design flexibility, good machinability, high strength-to-weight ratio and good toughness, wear resistance and fatigue strength because it can be cast like any other member of the Ductile Iron family, thus offering all the production advantages of a conventional Ductile Iron casting. Subsequently it is subjected to the austempering process to produce mechanical properties that are superior to conventional ductile iron, cast and forged aluminum and many cast and forged steels.

The mechanical properties of Ductile Iron and ADI are primarily determined by the metal matrix. The matrix in conventional Ductile Iron is a controlled mixture of pearlite and ferrite. (Tempered martensitic matrices may be developed for wear resistance, but lack the ductility of either as-cast Ductile Iron or ADI). The properties of ADI are due to its unique matrix of acicular ferrite and carbon stabilized austenite; called Ausferrite. ADI is a group of materials whose mechanical properties can be varied over a wide range by a suitable choice of heat treatment, as seen in the various entries in MatWeb.

The composition reported herein does not guarantee ADI properties, nor is it mandatory. However, this composition is a typical, industrially successful ADI composition. A good controlled chemistry like this one combined with a consistently high nodule count and nodularity and a consistent pearlite/ferrite ratio in clean, shrink-free Ductile Iron will provide the most robust process for the production of ADI.

Information supplied to MatWeb by Applied Process, Inc.

Available Properties
  • Density
  • Hardness, Brinell
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Reduction of Area
  • Modulus of Elasticity
  • Compressive Yield Strength
  • Poissons Ratio
  • Charpy Impact
  • Charpy Impact, Unnotched
  • Fracture Toughness
  • Shear Modulus
  • Shear Strength
  • CTE, linear 20°C
  • Thermal Conductivity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。