Assab Steel 705M Machinery Steel
Subcategory: Alloy Steel
Close Analogs: AISI /SAE 4340, DIN 34CrNiMo6, W.nr. 1.6582, BS 817M40 (EN 24), AFNOR 35NCD6, JIS SNCM8, SS 2541
Material Notes: ASSAB 705M is an alloyed machinery steel with good hardenability also in heavier sizes. It combines high strength with best toughness. As standard ASSAB 705M is supplied tough hardened with no further heat treatment required. It can be oil hardened to higher mechanical properties if required. Applications: ASSAB 705M is suitable for induction hardening and can also be nitrided or tuffrided to a surface hardness of 600-650 Vickers. ASSAB 705M is not suitable for welding but can with certain precautions be repair welded.
| Available Properties |
- Hardness, Brinell
- Hardness, Rockwell C
- Tensile Strength, Ultimate
- Tensile Strength, Ultimate at Elevated Temperature
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break
- Reduction of Area
- Impact Test
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|