Resin Technology Group UV-408 Low-Viscosity, High Clarity, UV Curable Adhesive

 

Subcategory: Adhesive; Thermoset

Material Notes:
UV 408 is a low viscosity, high clarity, UV curing adhesive with excellent adhesion to glass. The product is well suited for bonding close fitting parts and has excellent moisture resistance.

Applications:

Lens bonding, Glass assembly, Fiber optic bonding.

Processing:

UV light cure: Intensity of 200 mw/cm2; Spectral output of 300 to 500 nanometers; Optimum wavelength of 375 nanometers

Recommended Aurora UV light sources:

  • Aurora 455-S 5x5 High Intensity Flood
  • Aurora 461-S 1x6 High Intensity Beam
  • Aurora 100-S Spot Light Guide

Information provided by Resin Technology Group.

Available Properties
  • Viscosity
  • Thickness
  • Hardness, Shore D
  • Tensile Strength @ Break
  • Elongation at Break
  • CTE, linear 20°C
  • Flash Point
  • Shrinkage
  • Transmission, Visible
  • Color
  • Composition
  • Solubility
  • Toxicity
  • Water Resistance
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。