SABIC Innovative Plastics LEXAN LF1510A Polycarbonate (North America)
Subcategory: Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line. MatWeb has a separate entry for the European data sheet.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Metric | English | Comments |
|
Density | 1.36 g/cc | 0.0491 lb/in³ | ASTM D 792 |
Linear Mold Shrinkage | 0.002 - 0.003 cm/cm | 0.002 - 0.003 in/in | Flow, 0.125 inch; ASTM D 955 |
Linear Mold Shrinkage, Transverse | 0.0035 - 0.005 cm/cm | 0.0035 - 0.005 in/in | 0.125 inch; ASTM D 955 |
Melt Flow | 8.1 g/10 min | 8.1 g/10 min | 300C/1.2 kgf (O); ASTM D 1238 |
Mechanical Properties |
|
Tensile Strength @ Break | 72.4 MPa | 10500 psi | Type I, 0.2 in/min; ASTM D 638 |
Tensile Strength @ Yield | 72.4 MPa | 10500 psi | Type I, 0.2 in/min; ASTM D 638 |
Elongation at Break | 7 % | 7 % | Type I, 0.2 in/min; ASTM D 638 |
Elongation at Yield | 7 % | 7 % | Type I, 0.2 in/min; ASTM D 638 |
Flexural Modulus | 3.79 GPa | 550 ksi | 0.05 in/min, 2" span; ASTM D 790 |
Flexural Strength | 117 MPa | 17000 psi | 0.05 in/min, 2" span; ASTM D 790 |
Izod Impact, Unnotched | 5.07 J/cm | 9.5 ft-lb/in | 73F; ASTM D 4812 |
Gardner Impact @ 23°C | 16.9 J | 12.5 ft-lb | Instrumented Impact Total Energy, 73°F; ASTM D 3763 |
Izod Impact, Notched | 1.01 J/cm | 1.9 ft-lb/in | 73F; ASTM D 256 |
Electrical Properties |
|
Comparative Tracking Index | 175 - 250 V | 175 - 250 V | (+/- 0.125 inch); PLC Code 3; UL 746A |
Hot Wire Ignition, HWI | Min 120 sec | Min 120 sec | (+/- 0.125 inch); PLC Code 0; UL 746A |
High Amp Arc Ignition, HAI | Min 120 arcs | Min 120 arcs | Surface (+/- 0.125 inch); PLC Code 0; UL 746A |
Thermal Properties |
|
CTE, linear 68°F | 36 µm/m-°C | 20 µin/in-°F | Flow, -40F to 100F; ASTM E 831 |
CTE, linear 68°F, Transverse to Flow | 54 µm/m-°C | 30 µin/in-°F | from -40F to 100F; ASTM E 831 |
Deflection Temperature at 0.46 MPa (66 psi) | 133 °C | 271 °F | 0.125 inch, unannealed; ASTM D 648 |
Deflection Temperature at 1.8 MPa (264 psi) | 127 °C | 260 °F | 0.125 inch, unannealed; ASTM D 648 |
UL RTI, Electrical | 80 °C | 176 °F | UL 746B |
UL RTI, Mechanical with Impact | 80 °C | 176 °F | UL 746B |
UL RTI, Mechanical without Impact | 80 °C | 176 °F | UL 746B |
Flammability, UL94 | V-0 | V-0 | 0.059 in. |
Descriptive Properties | |
UL File Number, USA | E121562 | |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|