SABIC Innovative Plastics LEXAN® ML7038 PC, Unfilled
Subcategory: Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Data provided by GE Plastics. This product grade was removed from GE's database of standard products in 1998.
Physical Properties | Metric | English | Comments |
|
Density | 1.2 g/cc | 0.0434 lb/in³ | ASTM D792 |
Melt Flow | 70 g/10 min | 70 g/10 min | 300°C/1.2kg |
Mechanical Properties |
|
Tensile Strength, Ultimate | 63 MPa | 9140 psi | ASTM D638 |
Elongation at Break | 40 % | 40 % | ASTM D638 |
Flexural Modulus | 2.067 GPa | 300 ksi | ASTM D790 |
Izod Impact, Notched | 2.65 J/cm | 4.96 ft-lb/in | 23°C (73.4°F) |
Thermal Properties |
|
Deflection Temperature at 1.8 MPa (264 psi) | 121 °C | 250 °F | ASTM D648 |
Processing Properties |
|
Processing Temperature | 304 - 332 °C | 579 - 630 °F | melt temperature |
Mold Temperature | 65 - 93 °C | 149 - 199 °F | |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|