MatWeb Material ListThis series of pages has links to all data sheets in MatWeb. We have several search tools, listed above, that give you more efficient methods to reach the information that you need.
- AISI 4320H Steel, single quenched and tempered: (carburized 925°C (1700°F) for 8 hrs., pot cooled, reheated to 830°C (1525°F), quenched in agitated oil, 230°C (450°F) temper); 1.9 mm case depth
- AISI 4320H Steel, double quenched and tempered: (carburized 925°C (1700°F) for 8 hrs., pot cooled, reheated to 815°C (1500°F), quenched in agitated oil, reheated to 775°C (1425°F), quenched in agitated oil, 230°C (450°F) temper); 1.9 mm case depth
- AISI 4320H Steel, normalized 925°C (1700°F), pseudocarburized at 925°C (1700°F) for 8 hrs., reheated to 775°C (1425°F) and oil quenched, 150°C (300°F) temper
- AISI 4320H Steel, normalized 925°C (1700°F), pseudocarburized at 925°C (1700°F) for 8 hrs., reheated to 800°C (1470°F) and oil quenched, 150°C (300°F) temper
- AISI 4320H Steel, normalized 925°C (1700°F), pseudocarburized at 925°C (1700°F) for 8 hrs., reheated to 830°C (1525°F) and oil quenched, 150°C (300°F) temper; tested in 12.8 mm rounds
- AISI 4320H Steel, normalized 925°C (1700°F), pseudocarburized at 925°C (1700°F) for 8 hrs., oil quenched, 150°C (300°F) temper
- AISI 4320H Steel, normalized 925°C (1700°F), pseudocarburized at 925°C (1700°F) for 8 hrs., reheated to 775°C (1425°F) and oil quenched, 150°C (300°F) temper; tested in 12.8 mm rounds
- AISI 4320H Steel, normalized 925°C (1700°F) in 32 mm rounds, machined to 13.7 mm rounds, pseudocarburized at 925°C (1700°F) for 8 hrs., box cooled to room temp., reheated to 800°C (1470°F) and oil quenched, 150°C (300°F) temper
- AISI 4320H Steel, normalized 925°C (1700°F) in 32 mm rounds, machined to 13.7 mm rounds, pseudocarburized at 925°C (1700°F) for 8 hrs., box cooled to room temp., reheated to 830°C (1525°F) and oil quenched, 150°C (300°F) temper
- AISI 4320H Steel, normalized 925°C (1700°F) in 32 mm rounds, machined to 13.7 mm rounds, pseudocarburized at 925°C (1700°F) for 8 hrs., box cooled to room temp., oil quenched, 150°C (300°F) temper
- AISI 4320H Steel, annealed (heated to 850°C (1560°F), furnace cooled 15°C/hr. to 420°C, air cooled), 25 mm round
- AISI 4320H Steel, normalized, heated to 895°C (1640°F), air cooled, 13 mm (0.5 in.) rounds
- AISI 4320H Steel, normalized: heated to 895°C (1640°F), air cooled, 25 mm round
- AISI 4320H Steel, normalized: heated to 895°C (1640°F), air cooled, 50 mm (2 in.) round
- AISI 4320H Steel, normalized: heated to 895°C (1640°F), air cooled, 100 mm (4 in.) round
- AISI 4320H Steel, mock carburized, oil quenched, 150°C (300°F) temper, 13 mm (0.5 in.) round
- AISI 4320H Steel, mock carburized, oil quenched, 150°C (300°F) temper, 25 mm round
- AISI 4320H Steel, mock carburized, oil quenched, 150°C (300°F) temper, 50 mm (2 in.) round
- AISI 4320H Steel, mock carburized, oil quenched, 150°C (300°F) temper, 100 mm (4 in.) round
- AISI 4320H Steel, mock carburized, oil quenched, 230°C (450°F) temper, 13 mm (0.5 in.) round
- AISI 4320H Steel, mock carburized, oil quenched, 230°C (450°F) temper, 25 mm round
- AISI 4340 Steel, annealed, 25 mm round
- AISI 4340 Steel, normalized, 13 mm (0.5 in.) round
- AISI 4340 Steel, normalized, 25 mm round
- AISI 4340 Steel, normalized, 50 mm (2 in.) round
- AISI 4340 Steel, normalized, 100 mm (4 in.) round
- AISI 4340 Steel, oil quenched 800°C (1470°F), 540°C (1000°F) temper, 13 mm (0.5 in.) round
- AISI 4340 Steel, oil quenched 800°C (1470°F), 540°C (1000°F) temper, 25 mm round
- AISI 4340 Steel, oil quenched 800°C (1470°F), 540°C (1000°F) temper, 50 mm (2 in.) round
- AISI 4340 Steel, oil quenched 800°C (1470°F), 540°C (1000°F) temper, 100 mm (4 in.) round
- AISI 4340 Steel, oil quenched 800°C (1470°F), 595°C (1100°F) temper, 13 mm (0.5 in.) round
- AISI 4340 Steel, oil quenched 800°C (1470°F), 595°C (1100°F) temper, 25 mm round
- AISI 4340 Steel, oil quenched 800°C (1470°F), 595°C (1100°F) temper, 50 mm (2 in.) round
- AISI 4340 Steel, oil quenched 800°C (1470°F), 595°C (1100°F) temper, 100 mm (4 in.) round
- AISI 4340 Steel, oil quenched 800°C (1470°F), 650°C (1200°F) temper, 13 mm (0.5 in.) round
- AISI 4340 Steel, oil quenched 800°C (1470°F), 650°C (1200°F) temper, 25 mm round
- AISI 4340 Steel, oil quenched 800°C (1470°F), 650°C (1200°F) temper, 50 mm (2 in.) round
- AISI 4340 Steel, oil quenched 800°C (1470°F), 650°C (1200°F) temper, 100 mm
- AISI 4340 Steel, oil quenched 845°C, 650°C (1200°F) temper, tested at 25°C (77°F)
- AISI 4340 Steel, oil quenched 845°C, 650°C (1200°F) temper, tested at -195°C (-320°F)
- AISI 4340 Steel, oil quenched 845°C, 425°C (800°F) temper, tested at 25°C (77°F)
- AISI 4340 Steel, oil quenched 845°C, 425°C (800°F) temper, tested at -195C
- AISI 4340 Steel, oil quenched 855°C (1570°F), 230°C (450°F) temper for 4 hrs., tested at 26°C
- AISI 4340 Steel, oil quenched 855°C (1570°F), 230°C (450°F) temper for 4 hrs., tested at - 78°C
- AISI 4340 Steel, oil quenched 855°C (1570°F), 230°C (450°F) temper for 4 hrs., tested at -195°C (-320°F)
- AISI 4340 Steel, oil quenched 855°C (1570°F), 230°C (450°F) temper for 4 hrs., tested at -255°C (-430°F)
- AISI 4340 Steel, oil quenched 830°C (1525°F), 540°C (1000°F) temper, not nitrided
- AISI 4340 Steel, oil quenched 830°C (1525°F), 540°C (1000°F) temper, pseudonitrided
- AISI 4340 Steel, oil quenched 830°C (1525°F), 540°C (1000°F) temper, nitrided
- AISI 4340H Steel, quenched 845°C, 540°C (1000°F) temper
- AISI 4340H Steel, quenched 845°C, 650°C (1200°F) temper
- AISI 4340H Steel, normalized 870°C (1600°F)
- AISI 4340H Steel, annealed 810°C (1490°F)
- AISI E4340 Steel, annealed, 25 mm round
- AISI E4340 Steel, normalized, 13 mm (0.5 in.) round
- AISI E4340 Steel, normalized, 25 mm round
- AISI E4340 Steel, normalized, 50 mm (2 in.) round
- AISI E4340 Steel, normalized, 100 mm (4 in.) round
- AISI E4340 Steel, oil quenched 800°C (1470°F), 540°C (1000°F) temper, 13 mm (0.5 in.) round
- AISI E4340 Steel, oil quenched 800°C (1470°F), 540°C (1000°F) temper, 25 mm round
- AISI E4340 Steel, oil quenched 800°C (1470°F), 540°C (1000°F) temper, 50 mm (2 in.) round
- AISI E4340 Steel, oil quenched 800°C (1470°F), 540°C (1000°F) temper, 100 mm (4 in.) round
- AISI E4340 Steel, oil quenched 800°C (1470°F), 595°C (1100°F) temper, 13 mm (0.5 in.) round
- AISI E4340 Steel, oil quenched 800°C (1470°F), 595°C (1100°F) temper, 25 mm round
- AISI E4340 Steel, oil quenched 800°C (1470°F), 595°C (1100°F) temper, 50 mm (2 in.) round
- AISI E4340 Steel, oil quenched 800°C (1470°F), 595°C (1100°F) temper, 100 mm (4 in.) round
- AISI E4340 Steel, oil quenched 800°C (1470°F), 650°C (1200°F) temper, 13 mm (0.5 in.) round
- AISI E4340 Steel, oil quenched 800°C (1470°F), 650°C (1200°F) temper, 25 mm round
- AISI E4340 Steel, oil quenched 800°C (1470°F), 650°C (1200°F) temper, 50 mm (2 in.) round
- AISI E4340 Steel, oil quenched 800°C (1470°F), 650°C (1200°F) temper, 100 mm (4 in.) round
- AISI E4340 Steel, oil quenched 845°C, 650°C (1200°F) temper, tested at 25°C (77°F)
- AISI E4340 Steel, oil quenched 845°C, 650°C (1200°F) temper, tested at -195°C (-320°F)
- AISI E4340 Steel, oil quenched 845°C, 425°C (800°F) temper, tested at 25°C (77°F)
- AISI E4340 Steel, oil quenched 845°C, 425°C (800°F) temper, tested at -195°C (-320°F)
- AISI E4340 Steel, oil quenched 855°C (1570°F), 230°C (450°F) temper for 4hrs., tested at 26°C
- AISI E4340 Steel, oil quenched 855°C (1570°F), 230°C (450°F) temper for 4hrs., tested at -78°C
- AISI E4340 Steel, oil quenched 855°C (1570°F), 230°C (450°F) temper for 4hrs., tested at -195°C (-320°F)
- AISI E4340 Steel, oil quenched 855°C (1570°F), 230°C (450°F) temper for 4hrs., tested at -255°C (-430°F)
- AISI E4340 Steel, heat treated, fatigue tested
- AISI E4340 Steel, heat treated, pseudonitrided, fatigue tested
- AISI E4340 Steel, heat treated, nitrided for 48 hrs., fatigue tested
- AISI E4340 Steel, heat treated, nitrided for 50 hrs., fatigue tested
- AISI E4340 Steel, quenched 845°C, 205°C (400°F) temper
- AISI E4340 Steel, quenched 845°C, 315°C (600°F) temper
- AISI E4340 Steel, quenched 845°C, 425°C (800°F) temper
- AISI E4340 Steel, quenched 845°C, 540°C (1000°F) temper
- AISI E4340 Steel, annealed 810°C
- AISI E4340 H Steel, annealed, 25 mm round
- AISI E4340 H Steel, normalized, 13 mm (0.5 in.) round
- AISI E4340 H Steel, normalized, 25 mm round
- AISI E4340 H Steel, normalized, 50 mm (2 in.) round
- AISI E4340 H Steel, normalized, 100 mm (4 in.) round
- AISI E4340 H Steel, oil quenched 800°C (1470°F), 540°C (1000°F) temper, 13 mm (0.5 in.) round
- AISI E4340 H Steel, oil quenched 800°C (1470°F), 540°C (1000°F) temper, 25 mm round
- AISI E4340 H Steel, oil quenched 800°C (1470°F), 540°C (1000°F) temper, 50 mm (2 in.) round
- AISI E4340 H Steel, oil quenched 800°C (1470°F), 540°C (1000°F) temper, 100 mm (4 in.) round
- AISI E4340 H Steel, oil quenched 800°C (1470°F), 595°C (1100°F) temper, 13 mm (0.5 in.) round
- AISI E4340 H Steel, oil quenched 800°C (1470°F), 595°C (1100°F) temper, 25 mm round
- AISI E4340 H Steel, oil quenched 800°C (1470°F), 595°C (1100°F) temper, 50 mm (2 in.) round
- AISI E4340 H Steel, oil quenched 800°C (1470°F), 595°C (1100°F) temper, 100mm round
- AISI E4340 H Steel, oil quenched 800°C (1470°F), 650°C (1200°F) temper, 13 mm (0.5 in.) round
- AISI E4340 H Steel, oil quenched 800°C (1470°F), 650°C (1200°F) temper, 25 mm round
- AISI E4340 H Steel, oil quenched 800°C (1470°F), 650°C (1200°F) temper, 50mm round
- AISI E4340 H Steel, oil quenched 800°C (1470°F), 650°C (1200°F) temper, 100 mm (4 in.) round
- AISI E4340 H Steel, oil quenched 845°C, 650°C (1200°F) temper, tested at 25°C (77°F)
- AISI E4340 H Steel, oil quenched 845°C, 650°C (1200°F) temper, tested at -195°C (-320°F)
- AISI E4340 H Steel, oil quenched 845°C, 425°C (800°F) temper, tested at 25°C (77°F)
- AISI E4340 H Steel, oil quenched 845°C, 425°C (800°F) temper, tested at -195°C (-320°F)
- AISI E4340 H Steel, oil quenched 855°C (1570°F), 230°C (450°F) temper for 4 hrs, tested at 26°C
- AISI E4340 H Steel, oil quenched 855°C (1570°F), 230°C (450°F) temper for 4 hrs., tested at -78°C
- AISI E4340 H Steel, oil quenched 855°C (1570°F), 230°C (450°F) temper for 4 hrs., tested at -195°C (-320°F)
- AISI E4340 H Steel, oil quenched 855°C (1570°F), 230°C (450°F) temper for 4 hrs., tested at -255°C (-430°F)
- AISI E4340 H Steel, normalized, oil quenched and tempered
- AISI E4340 H Steel, normalized, oil quenched and tempered, pseudonitrided for 48 hrs
- AISI E4340 H Steel, normalized, oil quenched and tempered, nitrided for 48 hrs
- AISI E4340 H Steel, normalized, oil quenched and tempered, nitrided for 50 hrs
- AISI E4340 H Steel, quenched 845°C, 205°C (400°F) temper
- AISI E4340 H Steel, quenched 845°C, 315°C (600°F) temper
- AISI E4340 H Steel, quenched 845°C, 425°C (800°F) temper
- AISI E4340 H Steel, quenched 845°C, 540°C (1000°F) temper
- AISI E4340 Steel, quenched 845°C, 650°C (1200°F) temper
- AISI E4340 Steel, normalized 870°C (1600°F)
- AISI E4340 Steel, annealed 810°C (1490°F)
- AISI 4422 Steel, heat treated in 25 mm rounds, reheated to 775°C (1425°F), 150°C (300°F) temper
- AISI 4422 Steel, heat treated in 25 mm rounds, reheated to 820°C (1510°F), 150°C (300°F) temper
- AISI 4422 Steel, heat treated in 25 mm rounds, reheated to 870°C (1600°F), 150°C (300°F) temper
- AISI 4422 Steel, heat treated in 25 mm rounds, oil quenched, 150°C (300°F) temper
- AISI 4422 Steel, heat treated in 13.7 mm rounds, reheated to 775°C (1425°F), 150°C (300°F) temper
- AISI 4422 Steel, heat treated in 13.7 mm rounds, reheated to 820°C (1510°F), 150°C (300°F) temper
- AISI 4422 Steel, heat treated in 13.7 mm rounds, reheated to 870°C (1600°F), 150°C (300°F) temper
- AISI 4422 Steel, heat treated in 13.7 mm rounds, oil quenched, 150°C (300°F) temper
- AISI 4427 Steel, heat treated in 25 mm rounds, reheated to 765°C (1410°F), 150°C (300°F) temper
- AISI 4427 Steel, heat treated in 25 mm rounds, reheated to 805°C (1480°F), 150°C (300°F) temper
- AISI 4427 Steel, heat treated in 25 mm rounds, reheated to 865°C (1590°F), 150°C (300°F) temper
- AISI 4427 Steel, heat treated in 25 mm rounds, oil quenched, 150°C (300°F) temper
- AISI 4427 Steel, heat treated in 13.7 mm rounds, reheated to 765°C (1410°F), 150°C (300°F) temper
- AISI 4427 Steel, heat treated in 13.7 mm rounds, reheated to 805°C (1480°F), 150°C (300°F) temper
- AISI 4427 Steel, heat treated in 13.7 mm rounds, reheated to 865°C (1590°F), 150°C (300°F) temper
- AISI 4427 Steel, heat treated in 13.7 mm rounds, oil quenched, 150°C (300°F) temper
- AISI 4615 Steel
- AISI 4626 Steel
- AISI 4626H Steel
- AISI 4620 Steel, annealed, 25 mm round
- AISI 4620 Steel, normalized, 13 mm (0.5 in.) round
- AISI 4620 Steel, normalized, 25 mm (1 in.) round
- AISI 4620 Steel, normalized, 50 mm (2 in.) round
- AISI 4620 Steel, normalized, 100 mm (4 in.) round
- AISI 4620 Steel, mock carburized, 150°C (300°F) temper, 13 mm (0.5 in.) round
- AISI 4620 Steel, mock carburized, 150°C (300°F) temper, 25 mm (1 in.) round
- AISI 4620 Steel, mock carburized, 150°C (300°F) temper, 50 mm (2 in.) round
- AISI 4620 Steel, mock carburized, 150°C (300°F) temper, 100 mm (4 in.) round
- AISI 4620 Steel, mock carburized, 230°C (450°F) temper, 13 mm (0.5 in.) round
- AISI 4620 Steel, mock carburized, 230°C (450°F) temper, 25 mm (1 in.) round
- AISI 4620 Steel, mock carburized, 230°C (450°F) temper, 50 mm (2 in.) round
- AISI 4620 Steel, mock carburized, 230°C (450°F) temper, 100 mm (4 in.) round
- AISI 4620 Steel, quenched 900°C (1650°F), 150°C (300°F) temper
- AISI 4620 Steel, quenched 900°C (1650°F), 425°C (800°F) temper
- AISI 4620 Steel, quenched 900°C (1650°F), 540°C (1000°F) temper
- AISI 4620 Steel, quenched 900°C (1650°F), 650°C (1200°F) temper
- AISI 4620 Steel, normalized, machined to 25 mm (1 in.) rounds, pseudocarburized, reheated to 775°C (1430°F), quenched and tempered
- AISI 4620 Steel, normalized, machined to 25 mm (1 in.) rounds, pseudocarburized, reheated to 800°C (1470°F), quenched and tempered
- AISI 4620 Steel, normalized, machined to 25 mm (1 in.) rounds, pseudocarburized, reheated to 830°C (1525°F), quenched and tempered
- AISI 4620 Steel, normalized, machined to 25 mm (1 in.) rounds, pseudocarburized, reheated to 925°C (1700°F), quenched and tempered
- AISI 4620 Steel, normalized, machined to 13.7 mm rounds, pseudocarburized, reheated to 775°C (1430°F), quenched and tempered
- AISI 4620 Steel, normalized, machined to 13.7 mm rounds, pseudocarburized, reheated to 800°C (1470°F), quenched and tempered
- AISI 4620 Steel, normalized, machined to 13.7 mm rounds, pseudocarburized, reheated to 830°C (1525°F), quenched and tempered
- AISI 4620 Steel, normalized, machined to 13.7 mm rounds, pseudocarburized, reheated to 925°C (1700°F), quenched and tempered
- AISI 4620 Steel, direct quench from pot, carburized, oil quenched, 150°C (300°F) temper
- AISI 4620 Steel, single quenched and tempered, carburized, oil quenched, 150°C (300°F) temper
- AISI 4620 Steel, double quenched and tempered, carburized, oil quenched, 150°C (300°F) temper
- AISI 4620 Steel, direct quench from pot, carburized, oil quenched, 230°C (450°F) temper
- AISI 4620 Steel, single quenched and tempered, carburized, oil quenched, 230°C (450°F) temper
- AISI 4620 Steel, double quenched and tempered, carburized, oil quenched, 230°C (450°F) temper
- AISI 4620H Steel, annealed, 25 mm (1 in.) round
- AISI 4620H Steel, normalized, 13 mm (0.5 in.) round
- AISI 4620H Steel, normalized, 25 mm (1 in.) round
- AISI 4620H Steel, normalized, 50 mm (2 in.) round
- AISI 4620H Steel, normalized, 100 mm (4 in.) round
- AISI 4620H Steel, mock carburized, 150°C (300°F) temper, 13 mm (0.5 in.) round
- AISI 4620H Steel, mock carburized, 150°C (300°F) temper, 25 mm (1 in.) round
- AISI 4620H Steel, mock carburized, 150°C (300°F) temper, 50 mm (2 in.) round
- AISI 4620H Steel, mock carburized, 150°C (300°F) temper, 100 mm (4 in.) round
- AISI 4620H Steel, mock carburized, 230°C (450°F) temper, 13 mm (0.5 in.) round
- AISI 4620H Steel, mock carburized, 230°C (450°F) temper, 25 mm (1 in.) round
- AISI 4620H Steel, mock carburized, 230°C (450°F) temper, 50 mm (2 in.) round
- AISI 4620H Steel, mock carburized, 230°C (450°F) temper, 100 mm (4 in.) round
- AISI 4620H Steel, quenched 900°C (1650°F), 150°C (300°F) temper
- AISI 4620H Steel, quenched 900°C (1650°F), 425°C (800°F) temper
- AISI 4620H Steel, quenched 900°C (1650°F), 540°C (1000°F) temper
- AISI 4620H Steel, quenched 900°C (1650°F), 650°C (1200°F) temper
- AISI 4620H Steel, normalized, machined to 25 mm (1 in.) rounds, pseudocarburized, reheated to 775°C (1430°F), quenched and tempered
- AISI 4620H Steel, normalized, machined to 25 mm (1 in.) rounds, pseudocarburized, reheated to 800°C (1470°F), quenched and tempered
- AISI 4620H Steel, normalized, machined to 25 mm (1 in.) rounds, pseudocarburized, reheated to 830°C (1525°F), quenched and tempered
- AISI 4620H Steel, normalized, machined to 25 mm (1 in.) rounds, pseudocarburized, reheated to 925°C (1700°F), quenched and tempered
- AISI 4620H Steel, normalized, machined to 13.7 mm rounds, pseudocarburized, reheated to 775°C (1430°F), quenched and tempered
- AISI 4620H Steel, normalized, machined to 13.7 mm rounds, pseudocarburized, reheated to 800°C (1470°F), quenched and tempered
- AISI 4620H Steel, normalized, machined to 13.7 mm rounds, pseudocarburized, reheated to 830°C (1525°F), quenched and tempered
- AISI 4620H Steel, normalized, machined to 13.7 mm rounds, pseudocarburized, reheated to 925°C (1700°F), quenched and tempered
- AISI 4620H Steel, direct quench from pot, carburized, oil quenched, 150°C (300°F) temper
- AISI 4620H Steel, single quenched and tempered, carburized, oil quenched, 150°C (300°F) temper
- AISI 4620H Steel, double quenched and tempered, carburized, oil quenched, 150°C (300°F) temper
- AISI 4620H Steel, direct quench from pot, carburized, oil quenched, 230°C (450°F) temper
- AISI 4620H Steel, single quenched and tempered, carburized, oil quenched, 230°C (450°F) temper
- AISI 4620H Steel, double quenched and tempered, carburized, oil quenched, 230°C (450°F) temper
- AISI 4718 Steel, psueudocarburized, reheated to 765°C (1700°F) and oil quenched, 150°C (300°F) temper, 25 mm round
- AISI 4718 Steel, psueudocarburized, reheated to 800°C (1470°F) and oil quenched, 150°C (300°F) temper, 25 mm round
- AISI 4718 Steel, psueudocarburized, reheated to 850°C (1560°F) and oil quenched, 150°C (300°F) temper, 25 mm round
- AISI 4718 Steel, psueudocarburized and oil quenched, 150°C (300°F) temper, 25 mm round
- AISI 4718 Steel, psueudocarburized, reheated to 765°C (1410°F) and oil quenched, 150°C (300°F) temper, 13.7 mm round
- AISI 4718 Steel, psueudocarburized, reheated to 800°C (1470°F) and oil quenched, 150°C (300°F) temper, 13.7 mm round
- AISI 4718 Steel, psueudocarburized, reheated to 850°C (1560°F) and oil quenched, 150°C (300°F) temper, 13.7 mm round
- AISI 4718 Steel, psueudocarburized and oil quenched, 150°C (300°F) temper, 13.7 mm round
- AISI 4718H Steel, psueudocarburized, reheated to 765°C (1700°F) and oil quenched, 150°C (300°F) temper, 25 mm round
- AISI 4718H Steel, psueudocarburized, reheated to 800°C (1470°F) and oil quenched, 150°C (300°F) temper, 25 mm round
- AISI 4718H Steel, psueudocarburized, reheated to 850°C (1560°F) and oil quenched, 150°C (300°F) temper, 25 mm round
- AISI 4718H Steel, psueudocarburized and oil quenched, 150°C (300°F) temper, 25 mm round
- AISI 4718H Steel, psueudocarburized, reheated to 765°C (1410°F) and oil quenched, 150°C (300°F) temper, 13.7 mm round
- AISI 4718H Steel, psueudocarburized, reheated to 800°C (1470°F) and oil quenched, 150°C (300°F) temper, 13.7 mm round
- AISI 4718H Steel, psueudocarburized, reheated to 850°C (1560°F) and oil quenched, 150°C (300°F) temper, 13.7 mm round
- AISI 4718H Steel, psueudocarburized and oil quenched, 150°C (300°F) temper, 13.7 mm round
- AISI 4720 Steel
- AISI 4720H Steel
- AISI 4815 Steel, pseudocarburized, reheated to 775°C (1430°F) and oil quenched, 150°C (300°F) temper, 25 mm (1 in.) round
- AISI 4815 Steel, pseudocarburized, reheated to 800°C (1470°F) and oil quenched, 150°C (300°F) temper, 25 mm (1 in.) round
- AISI 4815 Steel, pseudocarburized, reheated to 830°C (1525°F) and oil quenched, 150°C (300°F) temper, 25 mm (1 in.) round
- AISI 4815 Steel, pseudocarburized and oil quenched, 150°C (300°F) temper, 25 mm (1 in.) round
- AISI 4815 Steel, pseudocarburized, reheated to 775°C (1430°F) and oil quenched, 150°C (300°F) temper, 13.7 mm (1 in.) round
- AISI 4815 Steel, pseudocarburized, reheated to 800°C (1470°F) and oil quenched, 150°C (300°F) temper, 13.7 mm (1 in.) round
- AISI 4815 Steel, pseudocarburized, reheated to 830°C (1525°F) and oil quenched, 150°C (300°F) temper, 13.7 mm (1 in.) round
- AISI 4815 Steel, pseudocarburized and oil quenched, 150°C (300°F) temper, 13.7 mm (1 in.) round
- AISI 4815H Steel, pseudocarburized, reheated to 775°C (1430°F) and oil quenched, 150°C (300°F) temper, 25 mm (1 in.) round
- AISI 4815H Steel, pseudocarburized, reheated to 800°C (1470°F) and oil quenched, 150°C (300°F) temper, 25 mm (1 in.) round
- AISI 4815H Steel, pseudocarburized, reheated to 830°C (1525°F) and oil quenched, 150°C (300°F) temper, 25 mm (1 in.) round
- AISI 4815H Steel, pseudocarburized and oil quenched, 150°C (300°F) temper, 25 mm (1 in.) round
- AISI 4815H Steel, pseudocarburized, reheated to 775°C (1430°F) and oil quenched, 150°C (300°F) temper, 13.7 mm (1 in.) round
- AISI 4815H Steel, pseudocarburized, reheated to 800°C (1470°F) and oil quenched, 150°C (300°F) temper, 13.7 mm (1 in.) round
- AISI 4815H Steel, pseudocarburized, reheated to 830°C (1525°F) and oil quenched, 150°C (300°F) temper, 13.7 mm (1 in.) round
- AISI 4815H Steel, pseudocarburized and oil quenched, 150°C (300°F) temper, 13.7 mm (1 in.) round
- AISI 4817 Steel
- AISI 4817H Steel
- AISI 4820 Steel, annealed 815°C (1500°F)
- AISI 4820 Steel, normalized 860°C (1580°F)
- AISI 4820 Steel, direct quenched from pot, tempered 150°C (300°F), 0.99 mm case depth
- AISI 4820 Steel, single quenched and tempered, 150°C (300°F), 1.2 mm case depth
- AISI 4820 Steel, double quenched and tempered (150°C (300°F)), 1.2 mm case depth
- AISI 4820 Steel, direct quenched from pot, tempered (230°C (450°F)), 0.99 mm case depth
- AISI 4820 Steel, single quenched and tempered (230°C (450°F)), 1.2 mm case depth
- AISI 4820 Steel, double quenched and tempered (230°C (450°F)), 1.2 mm case depth
- AISI 4820 Steel, heat treated, machined to 25 mm, pseudocarburized, reheated to 730°C (1350°F), 150°C (300°F) temper
- AISI 4820 Steel, heat treated, machined to 25 mm, pseudocarburized, reheated to 755°C (1390°F), 150°C (300°F) temper
- AISI 4820 Steel, heat treated, machined to 25 mm, pseudocarburized, reheated to 835°C, 150°C (300°F) temper (300°F)
- AISI 4820 Steel, heat treated, machined to 25 mm, pseudocarburized, 150°C (300°F) temper
- AISI 4820 Steel, heat treated, machined to 13.7 mm, pseudocarburized, reheated to 730°C (1350°F), 150°C (300°F) temper
- AISI 4820 Steel, heat treated, machined to 13.7 mm, pseudocarburized, reheated to 755°C (1390°F), 150°C (300°F) temper
- AISI 4820 Steel, heat treated, machined to 13.7 mm, pseudocarburized, reheated to 835°C, 150°C (300°F) temper
- AISI 4820 Steel, heat treated, machined to 13.7 mm, pseudocarburized, 150°C (300°F) temper
- AISI 4820 Steel, annealed 815°C (1500°F), 25 mm (1 in.) round
- AISI 4820 Steel, normalized 860°C (1580°F), 13 mm (0.5 in.) round
- AISI 4820 Steel, normalized 860°C (1580°F), 25 mm (1 in.) round
- AISI 4820 Steel, normalized 860°C (1580°F), 50 mm (2 in.) round
- AISI 4820 Steel, normalized 860°C (1580°F), 100 mm (4 in.) round
- AISI 4820 Steel, mock carburized, reheated to 800°C (1470°F), 150°C (300°F) temper, 13 mm (0.5 in.) round
- AISI 4820 Steel, mock carburized, reheated to 800°C (1470°F), 150°C (300°F) temper, 25 mm (1 in.) round
- AISI 4820 Steel, mock carburized, reheated to 800°C (1470°F), 150°C (300°F) temper, 50 mm (2 in.) round
- AISI 4820 Steel, mock carburized, reheated to 800°C (1470°F), 150°C (300°F) temper, 100 mm (4 in.) round
- AISI 4820 Steel, mock carburized, reheated to 800°C (1470°F), 230°C (450°F) temper, 13 mm (0.5 in.) round
- AISI 4820 Steel, mock carburized, reheated to 800°C (1470°F), 230°C (450°F) temper, 25 mm (1 in.) round
- AISI 4820 Steel, mock carburized, reheated to 800°C (1470°F), 230°C (450°F) temper, 50 mm (2 in.) round
- AISI 4820 Steel, mock carburized, reheated to 800°C (1470°F), 230°C (450°F) temper, 100 mm (4 in.) round
- AISI 4820H Steel, direct quenched from pot, tempered (150°C (300°F)), 0.99 mm case depth
- AISI 4820H Steel, single quenched and tempered (150°C (300°F)), 1.2 mm case depth
- AISI 4820H Steel, double quenched and tempered (150°C (300°F)), 1.2 mm case depth
- AISI 4820H Steel, direct quenched from pot, tempered (230°C (450°F)), 0.99 mm case depth
- AISI 4820H Steel, single quenched and tempered (230°C (450°F)), 1.2 mm case depth
- AISI 4820H Steel, double quenched and tempered (230°C (450°F)), 1.2mm case depth
- AISI 4820H Steel, heat treated, machined to 25 mm, pseudocarburized, reheated to 730°C (1350°F), 150°C (300°F) temper
- AISI 4820H Steel, heat treated, machined to 25 mm, pseudocarburized, reheated to 755°C (1390°F), 150°C (300°F) temper
- AISI 4820H Steel, heat treated, machined to 25 mm, pseudocarburized, reheated to 835°C, 150°C (300°F) temper
- AISI 4820H Steel, heat treated, machined to 25 mm, pseudocarburized, 150°C (300°F) temper
- AISI 4820H Steel, heat treated, machined to 13.7 mm, pseudocarburized, reheated to 730°C (1350°F), 150°C (300°F) temper
- AISI 4820H Steel, heat treated, machined to 13.7 mm, pseudocarburized, reheated to 755°C (1390°F), 150°C (300°F) temper
- AISI 4820H Steel, heat treated, machined to 13.7 mm, pseudocarburized, reheated to 835°C, 150°C (300°F) temper
- AISI 4820H Steel, heat treated, machined to 13.7 mm, pseudocarburized, 150°C (300°F) temper
- AISI 4820H Steel, annealed 815°C (1500°F), 25 mm (1 in.) round
- AISI 4820H Steel, normalized 860°C (1580°F), 13 mm (0.5 in.) round
- AISI 4820H Steel, normalized 860°C (1580°F), 25 mm (1 in.) round
- AISI 4820H Steel, normalized 860°C (1580°F), 50 mm (2 in.) round
- AISI 4820H Steel, normalized 860°C (1580°F), 100 mm (4 in.) round
- AISI 4820H Steel, mock carburized, reheated to 800°C (1470°F), 150°C (300°F) temper, 13 mm (0.5 in.) round
- AISI 4820H Steel, mock carburized, reheated to 800°C (1470°F), 150°C (300°F) temper, 25 mm (1 in.) round
- AISI 4820H Steel, mock carburized, reheated to 800°C (1470°F), 150°C (300°F) temper, 50 mm (2 in.) round
- AISI 4820H Steel, mock carburized, reheated to 800°C (1470°F), 150°C (300°F) temper, 100 mm (4 in.) round
- AISI 4820H Steel, mock carburized, reheated to 800°C (1470°F), 230°C (450°F) temper, 13 mm (0.5 in.) round
- AISI 4820H Steel, mock carburized, reheated to 800°C (1470°F), 230°C (450°F) temper, 25 mm (1 in.) round
- AISI 4820H Steel, mock carburized, reheated to 800°C (1470°F), 230°C (450°F) temper, 50 mm (2 in.) round
- AISI 4820H Steel, mock carburized, reheated to 800°C (1470°F), 230°C (450°F) temper, 100 mm (4 in.) round
- AISI 4820H Steel, annealed 815°C (1500°F)
- AISI 4820H Steel, normalized 860°C (1580°F)
- AISI E50100 Steel
- AISI 50B40 Steel
- AISI 50B40H Steel
- AISI 50B44 Steel
- AISI 50B44H Steel
- AISI 5046 Steel
- AISI 5046H Steel
- AISI 50B46 Steel
- AISI 50B46H Steel
- AISI 50B50 Steel
- AISI 50B50H Steel
- AISI 5060 Steel
- AISI 50B60 Steel
- AISI 50B60H Steel
- AISI E51100 Steel
- AISI 5120 Steel, heat treated, machined to 25 mm, pseudocarburized, reheated to 775°C (1430°F), 150°C (300°F) temper
- AISI 5120 Steel, heat treated, machined to 25 mm, pseudocarburized, reheated to 800°C (1470°F), 150°C (300°F) temper
- AISI 5120 Steel, heat treated, machined to 25 mm, pseudocarburized, reheated to 845°C (1550°F), 150°C (300°F) temper
- AISI 5120 Steel, heat treated, machined to 25 mm, pseudocarburized, 150°C (300°F) temper
- AISI 5120 Steel, heat treated, machined to 13.7 mm, pseudocarburized, reheated to 775°C (1430°F), 150°C (300°F) temper
- AISI 5120 Steel, heat treated, machined to 13.7 mm, pseudocarburized, reheated to 800°C (1470°F), 150°C (300°F) temper
- AISI 5120 Steel, heat treated, machined to 13.7 mm, pseudocarburized, reheated to 845°C (1550°F), 150°C (300°F) temper
- AISI 5120 Steel, heat treated, machined to 13.7 mm, pseudocarburized, 150°C (300°F) temper
- AISI 5120H Steel, heat treated, machined to 25 mm, pseudocarburized, reheated to 775°C (1430°F), 150°C (300°F) temper
- AISI 5120H Steel, heat treated, machined to 25 mm, pseudocarburized, reheated to 800°C (1470°F), 150°C (300°F) temper
- AISI 5120H Steel, heat treated, machined to 25 mm, pseudocarburized, reheated to 845°C (1550°F), 150°C (300°F) temper
- AISI 5120H Steel, heat treated, machined to 25 mm, pseudocarburized, 150°C (300°F) temper
- AISI 5120H Steel, heat treated, machined to 13.7 mm, pseudocarburized, reheated to 775°C (1430°F), 150°C (300°F) temper
- AISI 5120H Steel, heat treated, machined to 13.7 mm, pseudocarburized, reheated to 800°C (1470°F), 150°C (300°F) temper
- AISI 5120H Steel, heat treated, machined to 13.7 mm, pseudocarburized, reheated to 845°C (1550°F), 150°C (300°F) temper
- AISI 5120H Steel, heat treated, machined to 13.7 mm, pseudocarburized, 150°C (300°F) temper
- AISI 5130 Steel
- AISI 5130H Steel
- AISI 5132 Steel
- AISI 5132H Steel
- AISI 5135 Steel
- AISI 5135H Steel
- ASTM A514 Steel, grade P, plate thickness <= 19 mm
- ASTM A514 Steel, grade P, plate thickness 19 - 64 mm
- ASTM A514 Steel, grade P, plate thickness 64 - 150 mm
- ASTM A514 Steel, grade Q, plate thickness <= 19 mm
- ASTM A514 Steel, grade Q, plate thickness 19 - 64 mm
- ASTM A514 Steel, grade Q, plate thickness 64 - 120 mm
- AISI 5140 Steel, annealed 830°C (1525°F)
- AISI 5140 Steel, normalized, 13 mm (0.5 in.) round
- AISI 5140 Steel, normalized, 25 mm (1 in.) round
- AISI 5140 Steel, normalized, 50 mm (2 in.) round
- AISI 5140 Steel, normalized, 100 mm (4 in.) round
- AISI 5140 Steel, oil quenched 845°C (1550°F), 540°C (1000°F) temper, 13 mm (0.5 in.) round
- AISI 5140 Steel, oil quenched 845°C (1550°F), 540°C (1000°F) temper, 25 mm (1 in.) round
- AISI 5140 Steel, oil quenched 845°C (1550°F), 540°C (1000°F) temper, 50 mm (2 in.) round
- AISI 5140 Steel, oil quenched 845°C (1550°F), 540°C (1000°F) temper, 100 mm (4 in.) round
- AISI 5140 Steel, oil quenched 845°C (1550°F), 595°C (1100°F) temper, 13 mm (0.5 in.) round
- AISI 5140 Steel, oil quenched 845°C (1550°F), 595°C (1100°F) temper, 25 mm (1 in.) round
- AISI 5140 Steel, oil quenched 845°C (1550°F), 595°C (1100°F) temper, 50 mm (2 in.) round
- AISI 5140 Steel, oil quenched 845°C (1550°F), 595°C (1100°F) temper, 100 mm (4 in.) round
- AISI 5140 Steel, oil quenched 845°C (1550°F), 650°C (1200°F) temper, 13 mm (0.5 in.) round
- AISI 5140 Steel, oil quenched 845°C (1550°F), 650°C (1200°F) temper, 25 mm (1 in.) round
- AISI 5140 Steel, oil quenched 845°C (1550°F), 650°C (1200°F) temper, 50 mm (2 in.) round
- AISI 5140 Steel, oil quenched 845°C (1550°F), 650°C (1200°F) temper, 100 mm (4 in.) round
- AISI 5140 Steel, normalized 870°C (1600°F)
- AISI 5140 Steel, annealed 830°C (1525°F), 25 mm (1 in.) round
- AISI 5140H Steel, annealed 830°C
- AISI 5140H Steel, normalized, 13 mm (0.5 in.) round
- AISI 5140H Steel, normalized, 25 mm (1 in.) round
- AISI 5140H Steel, normalized, 50 mm (2 in.) round
- AISI 5140H Steel, normalized, 100 mm (4 in.) round
- AISI 5140H Steel, oil quenched 845°C (1550°F), 540°C (1000°F) temper, 13 mm (0.5 in.) round
- AISI 5140H Steel, oil quenched 845°C (1550°F), 540°C (1000°F) temper, 25 mm (1 in.) round
- AISI 5140H Steel, oil quenched 845°C (1550°F), 540°C (1000°F) temper, 50 mm (2 in.) round
- AISI 5140H Steel, oil quenched 845°C (1550°F), 540°C (1000°F) temper, 100 mm (4 in.) round
- AISI 5140H Steel, oil quenched 845°C (1550°F), 595°C (1100°F) temper, 13 mm (0.5 in.) round
- AISI 5140H Steel, oil quenched 845°C (1550°F), 595°C (1100°F) temper, 25 mm (1 in.) round
- AISI 5140H Steel, oil quenched 845°C (1550°F), 595°C (1100°F) temper, 50 mm (2 in.) round
- AISI 5140H Steel, oil quenched 845°C (1550°F), 595°C (1100°F) temper, 100 mm (4 in.) round
- AISI 5140H Steel, oil quenched 845°C (1550°F), 650°C (1200°F) temper, 13 mm (0.5 in.) round
- AISI 5140H Steel, oil quenched 845°C (1550°F), 650°C (1200°F) temper, 25 mm (1 in.) round
- AISI 5140H Steel, oil quenched 845°C (1550°F), 650°C (1200°F) temper, 50 mm (2 in.) round
- AISI 5140H Steel, oil quenched 845°C (1550°F), 650°C (1200°F) temper, 100 mm (4 in.) round
- AISI 5140H Steel, normalized 870°C (1600°F)
- AISI 5140H Steel, annealed 830°C (1525°F), 25 mm (1 in.) round
- AISI 5150 Steel, annealed, 25 mm (1 in.) round
- AISI 5150 Steel, normalized, 13 mm (0.5 in.) round
- AISI 5150 Steel, normalized, 25 mm (1 in.) round
- AISI 5150 Steel, normalized, 50 mm (2 in.) round
- AISI 5150 Steel, normalized, 100 mm (4 in.) round
- AISI 5150 Steel, oil quenched from 830°C (1525°F), 540°C (1000°F) temper, 13 mm (0.5 in.) round
- AISI 5150 Steel, oil quenched from 830°C (1525°F), 540°C (1000°F) temper, 25 mm (1 in.) round
- AISI 5150 Steel, oil quenched from 830°C (1525°F), 540°C (1000°F) temper, 50 mm (2 in.) round
- AISI 5150 Steel, oil quenched from 830°C (1525°F), 540°C (1000°F) temper, 100 mm (4 in.) round
- AISI 5150 Steel, oil quenched from 830°C (1525°F), 595°C (1100°F) temper, 13 mm (0.5 in.) round
- AISI 5150 Steel, oil quenched from 830°C (1525°F), 595°C (1100°F) temper, 25 mm (1 in.) round
- AISI 5150 Steel, oil quenched from 830°C (1525°F), 595°C (1100°F) temper, 50 mm (2 in.) round
- AISI 5150 Steel, oil quenched from 830°C (1525°F), 595°C (1100°F) temper, 100 mm (4 in.) round
- AISI 5150 Steel, oil quenched from 830°C (1525°F), 650°C (1200°F) temper, 13 mm (0.5 in.) round
- AISI 5150 Steel, oil quenched from 830°C (1525°F), 650°C (1200°F) temper, 25 mm (1 in.) round
- AISI 5150 Steel, oil quenched from 830°C (1525°F), 650°C (1200°F) temper, 50 mm (2 in.) round
- AISI 5150 Steel, oil quenched from 830°C (1525°F), 650°C (1200°F) temper, 100 mm (4 in.) round
- AISI 5150H Steel, annealed, 25 mm (1 in.) round
- AISI 5150H Steel, normalized, 13 mm (0.5 in.) round
- AISI 5150H Steel, normalized, 25 mm (1 in.) round
- AISI 5150H Steel, normalized, 50 mm (2 in.) round
- AISI 5150H Steel, normalized, 100 mm (4 in.) round
- AISI 5150H Steel, oil quenched from 830°C (1525°F), 540°C (1000°F) temper, 13 mm (0.5 in.) round
- AISI 5150H Steel, oil quenched from 830°C (1525°F), 540°C (1000°F) temper, 25 mm (1 in.) round
- AISI 5150H Steel, oil quenched from 830°C (1525°F), 540°C (1000°F) temper, 50 mm (2 in.) round
- AISI 5150H Steel, oil quenched from 830°C (1525°F), 540°C (1000°F) temper, 100 mm (4 in.) round
- AISI 5150H Steel, oil quenched from 830°C (1525°F), 595°C (1100°F) temper, 13 mm (0.5 in.) round
- AISI 5150H Steel, oil quenched from 830°C (1525°F), 595°C (1100°F) temper, 25 mm (1 in.) round
- AISI 5150H Steel, oil quenched from 830°C (1525°F), 595°C (1100°F) temper, 50 mm (2 in.) round
- AISI 5150H Steel, oil quenched from 830°C (1525°F), 595°C (1100°F) temper, 100 mm (4 in.) round
- AISI 5150H Steel, oil quenched from 830°C (1525°F), 650°C (1200°F) temper, 13 mm (0.5 in.) round
- AISI 5150H Steel, oil quenched from 830°C (1525°F), 650°C (1200°F) temper, 25 mm (1 in.) round
- AISI 5150H Steel, oil quenched from 830°C (1525°F), 650°C (1200°F) temper, 50 mm (2 in.) round
- AISI 5150H Steel, oil quenched from 830°C (1525°F), 650°C (1200°F) temper, 100 mm (4 in.) round
- AISI 5155 Steel
- AISI 5155H Steel
- AISI 5160 Steel, annealed, 25 mm (1 in.) round
- AISI 5160 Steel, normalized, 13 mm (0.5 in.) round
- AISI 5160 Steel, normalized, 25 mm (1 in.) round
- AISI 5160 Steel, normalized, 50 mm (2 in.) round
- AISI 5160 Steel, normalized, 100 mm (4 in.) round
- AISI 5160 Steel, oil quenched from 830°C (1525°F), 540°C (1000°F) temper, 13 mm (0.5 in.) round
- AISI 5160 Steel, oil quenched from 830°C (1525°F), 540°C (1000°F) temper, 25 mm (1 in.) round
- AISI 5160 Steel, oil quenched from 830°C (1525°F), 540°C (1000°F) temper, 50 mm (2 in.) round
- AISI 4419 Steel, annealed at 915°C (1675°F), 25 mm (1 in.) round
- AISI 4419 Steel, normalized at 955°C (1750°F), 14 mm (0.55 in.) round
- AISI 4419 Steel, normalized at 955°C (1750°F), 25 mm (1 in.) round
- AISI 4419 Steel, normalized at 955°C (1750°F), 50 mm (2 in.) round
- AISI 4419 Steel, normalized at 955°C (1750°F), 100 mm (4 in.) round
- AISI 4419 Steel, mock carburized, 150°C (300°F) temper, 14 mm (0.55 in.) round
- AISI 4419 Steel, mock carburized, 150°C (300°F) temper, 25 mm (1 in.) round
- AISI 4419 Steel, mock carburized, 150°C (300°F) temper, 50 mm (2 in.) round
- AISI 4419 Steel, mock carburized, 150°C (300°F) temper, 100 mm (4 in.) round
- AISI 4419 Steel, mock carburized, 230°C (450°F) temper, 14 mm (0.55 in.) round
- AISI 4419 Steel, mock carburized, 230°C (450°F) temper, 25 mm (1 in.) round
- AISI 4419 Steel, mock carburized, 230°C (450°F) temper, 50mm round
- AISI 4419 Steel, mock carburized, 230°C (450°F) temper, 100 mm (4 in.) round
- AISI 4419 Steel, direct quenched from pot, 150°C (300°F) temper
- AISI 4419 Steel, single quenched, 150°C (300°F) temper
- AISI 4419 Steel, double quenched, 150°C (300°F) temper
- AISI 4419 Steel, direct quenched from pot, 230°C (450°F) temper
- AISI 4419 Steel, single quenched, 230°C (450°F) temper
- AISI 4419 Steel, double quenched, 230°C (450°F) temper
- AISI 4419H Steel, annealed at 915°C (1675°F), 25 mm (1 in.) round
- AISI 4419H Steel, normalized at 955°C (1750°F), 14 mm (0.55 in.) round
- AISI 4419H Steel, normalized at 955°C (1750°F), 25 mm (1 in.) round
- AISI 4419H Steel, normalized at 955°C (1750°F), 50 mm (2 in.) round
- AISI 4419H Steel, normalized at 955°C (1750°F), 100 mm (4 in.) round
- AISI 4419H Steel, mock carburized, 150°C (300°F) temper, 14 mm (0.55 in.) round
- AISI 4419H Steel, mock carburized, 150°C (300°F) temper, 25 mm (1 in.) round
- AISI 4419H Steel, mock carburized, 150°C (300°F) temper, 50 mm (2 in.) round
- AISI 4419H Steel, mock carburized, 150°C (300°F) temper, 100 mm (4 in.) round
- AISI 4419H Steel, mock carburized, 230°C (450°F) temper, 14 mm (0.55 in.) round
- AISI 4419H Steel, mock carburized, 230°C (450°F) temper, 25 mm (1 in.) round
- AISI 4419H Steel, mock carburized, 230°C (450°F) temper, 50 mm (2 in.) round
- AISI 4419H Steel, mock carburized, 230°C (450°F) temper, 100 mm (4 in.) round
- AISI 4419H Steel, direct quenched from pot and tempered, 150°C (300°F)
- AISI 4419H Steel, single quenched and tempered, 150°C (300°F)
- AISI 4419H Steel, double quenched and tempered, 150°C (300°F)
- AISI 4419H Steel, direct quenched from pot and tempered, 230°C (450°F)
- AISI 4419H Steel, single quenched and tempered, 230°C (450°F)
- AISI 4419H Steel, double quenched and tempered, 230°C (450°F)
- AISI 4320 Steel, normalized at 895°C (1640°F)
- AISI 4320 Steel, annealed at 850°C (1560°F)
- AISI 4320 Steel, direct quench from pot (carburized 925°C (1700°F) for 8 hrs., quenched in agitated oil, 150°C (300°F) temper), 1.5 mm case depth
- AISI 4320 Steel, single quenched and tempered (carburized 925°C (1700°F) for 8hrs, pot cooled, reheated to 830°C (1525°F), quenched in agitated oil, 150°C (300°F) temper)
- AISI 4320 Steel, double quenched and tempered (carburized 925°C (1700°F) for 8hrs, pot cooled, reheated to 815°C (1500°F), quenched in agitated oil, reheated to 775°C, quenched in agitated oil, 150°C (300°F) temper), 1.9 mm case depth
- AISI 4320 Steel, direct quench from pot (carburized 925°C (1700°F) for 8 hrs., quenched in agitated oil, 230°C (450°F) temper), 1.5 mm case depth
- AISI 4320 Steel, single quenched and tempered (carburized 925°C (1700°F) for 8hrs, pot cooled, reheated to 815°C (1500°F), quenched in agitated oil, 230°C (450°F) temper), 1.9 mm case depth
- AISI 4320 Steel, double quenched and tempered (carburized 925°C (1700°F) for 8hrs, pot cooled, reheated to 815°C (1500°F), quenched in agitated oil, reheated to 775°C, quenched in agitated oil, 230°C (450°F) temper), 230°C (450°F) temper
- AISI 4320 Steel, normalized 925°C (1700°F) in 32 mm rounds, machined to 25 mm (1 in.) rounds, pseudocarburized 925°C (1700°F) for 8 hrs., box cooled to room temp., reheated to 775°C, oil quenched, 150°C (300°F) temper, tested in 12.8 mm rounds
- AISI 4320 Steel, normalized 925°C (1700°F) in 32 mm rounds, machined to 25 mm (1 in.) rounds, pseudocarburized 925°C (1700°F) for 8 hrs., box cooled to room temp., reheated to 800°C (1470°F), oil quenched, 150°C (300°F) temper, tested in 12.8 mm rounds
- AISI 4320 Steel, normalized 925°C (1700°F) in 32 mm rounds, machined to 25 mm (1 in.) rounds, pseudocarburized 925°C (1700°F) for 8 hrs., box cooled to room temp., reheated to 830°C (1525°F), oil quenched, 150°C (300°F) temper, tested in 12.8 mm rounds
- AISI 4320 Steel, normalized 925°C (1700°F) in 32 mm rounds, machined to 25 mm (1 in.) rounds, pseudocarburized 925°C (1700°F) for 8 hrs., oil quenched, 150°C (300°F) temper, tested in 12.8 mm rounds
- AISI 4320 Steel, normalized 925°C (1700°F) in 32 mm rounds, machined to 13.7 mm rounds, pseudocarburized 925°C (1700°F) for 8 hrs., box cooled to room temp., reheated to 775°C, oil quenched, 150°C (300°F) temper, tested in 12.8 mm rounds
- AISI 4320 Steel, normalized 925°C (1700°F) in 32 mm rounds, machined to 13.7 mm rounds, pseudocarburized 925°C (1700°F) for 8 hrs., box cooled to room temp., reheated to 800°C (1470°F), oil quenched, 150°C (300°F) temper, tested in 12.8 mm rounds
- AISI 4320 Steel, normalized 925°C (1700°F) in 32 mm rounds, machined to 13.7 mm rounds, pseudocarburized 925°C (1700°F) for 8 hrs., box cooled to room temp., reheated to 830°C (1525°F), oil quenched, 150°C (300°F) temper, tested in 12.8 mm rounds
- AISI 4320 Steel, normalized 925°C (1700°F) in 32 mm rounds, machined to 13.7 mm rounds, pseudocarburized 925°C (1700°F) for 8 hrs., oil quenched, 150°C (300°F) temper, tested in 12.8 mm rounds
- AISI 4320 Steel, annealed (heated to 850°C (1560°F), furnace cooled 15°C/hr. to 420°C, air cooled), 25 mm (1 in.) round
- AISI 4320 Steel, normalized 895°C (1640°F), air cooled, 13 mm (0.5 in.) round
- AISI 4320 Steel, normalized 895°C (1640°F), air cooled, 25 mm (1 in.) round
- AISI 4320 Steel, normalized 895°C (1640°F), air cooled, 50 mm (2 in.) round
- AISI 4320 Steel, normalized 895°C (1640°F), air cooled, 100 mm (4 in.) round
- AISI 4320 Steel, mock carburized 925°C (1700°F) for 8 hrs., reheated to 815°C (1500°F), oil quenched, 150°C (300°F) temper, 13 mm (0.5 in.) round
- AISI 4320 Steel, mock carburized 925°C (1700°F) for 8 hrs., reheated to 815°C (1500°F), oil quenched, 150°C (300°F) temper, 25 mm (1 in.) round
- AISI 4320 Steel, mock carburized 925°C (1700°F) for 8 hrs., reheated to 815°C (1500°F), oil quenched, 150°C (300°F) temper, 50 mm (2 in.) round
- AISI 4320 Steel, mock carburized 925°C (1700°F) for 8 hrs., reheated to 815°C (1500°F), oil quenched, 150°C (300°F) temper, 100 mm (4 in.) round
- AISI 4320 Steel, mock carburized 925°C (1700°F) for 8 hrs., reheated to 815°C (1500°F), oil quenched, 230°C (450°F) temper, 13 mm (0.5 in.) rounds
- AISI 4320 Steel, mock carburized 925°C (1700°F) for 8 hrs., reheated to 815°C (1500°F), oil quenched, 230°C (450°F) temper, 25 mm (1 in.) rounds
- AISI 4320 Steel, mock carburized 925°C (1700°F) for 8 hrs., reheated to 815°C (1500°F), oil quenched, 230°C (450°F) temper, 50 mm (2 in.) round
- AISI 4320 Steel, mock carburized 925°C (1700°F) for 8 hrs., reheated to 815°C (1500°F), oil quenched, 230°C (450°F) temper, 100 mm (4 in.) round
- AISI 4320 Steel, quenched 900°C (1650°F), 205°C (400°F) temper
- AISI 4320 Steel, quenched 900°C (1650°F), 425°C (800°F) temper
- AISI 4320 Steel, quenched 900°C (1650°F), 540°C (1000°F) temper
- AISI 4320 Steel, quenched 900°C (1650°F), 650°C (1200°F) temper
- AISI 4320H Steel, normalized at 895°C (1640°F)
- AISI 4320H Steel, annealed at 850°C (1560°F)
- AISI 4320H Steel, direct quenched from pot: (carburized 925°C (1700°F) for 8 hrs., quenched in agitated in oil, 150°C (300°F) temper); 1.5 mm case depth
- AISI 4320H Steel, single quenched and tempered: (carburized 925°C (1700°F) for 8 hrs., pot cooled, reheated to 830°C (1525°F), quenched in agitated oil, 150°C (300°F) temper); 1.9 mm case depth
- AISI 4320H Steel, double quenched and tempered: (carburized 925°C (1700°F) for 8 hrs., pot cooled, reheated to 815°C (1500°F), quenched in agitated oil, reheated to 775°C (1425°F), quenched in agitated oil, 150°C (300°F) temper); 1.9 mm case depth