MatWeb Material ListThis series of pages has links to all data sheets in MatWeb. We have several search tools, listed above, that give you more efficient methods to reach the information that you need.
- Copper, UNS C70400, H04 Temper
- Copper, UNS C70400, H06 Temper
- Copper, UNS C70400, H08 Temper
- Copper, UNS C70400, H55 Temper
- Copper nickel 10%, UNS C70600
- Copper nickel 10%, UNS C70600, OSO50 Temper flat products
- Copper nickel 10%, UNS C70600, OSO35 Temper flat products
- Copper nickel 10%, UNS C70600, OSO25 Temper flat products
- Copper nickel 10%, UNS C70600, H01 Temper flat products
- Copper nickel 10%, UNS C70600, H02 Temper flat products
- Copper nickel 10%, UNS C70600, H04 Temper flat products
- Copper nickel 10%, UNS C70600, H06 Temper flat products
- Copper nickel 10%, UNS C70600, H08 Temper flat products
- Copper nickel 10%, UNS C70600, H10 Temper flat products
- Copper nickel 10%, UNS C70600, H55 Temper flat products
- Copper nickel 10%, UNS C70600, OSO25 Temper tubing
- Copper nickel 10%, UNS C70600, H10 Temper wire
- Copper nickel 20%, UNS C71000
- Copper nickel 20%, UNS C71000, OSO50 Temper flat products
- Copper nickel 20%, UNS C71000, OSO35 Temper flat products
- Copper nickel 20%, UNS C71000, OSO25 Temper flat products
- Copper nickel 20%, UNS C71000, H01 Temper flat products
- Copper nickel 20%, UNS C71000, H02 Temper flat products
- Copper nickel 20%, UNS C71000, H04 Temper flat products
- Copper nickel 20%, UNS C71000, H06 Temper flat products
- Copper nickel 20%, UNS C71000, H08 Temper flat products
- Copper nickel 20%, UNS C71000, H10 Temper flat products
- Copper nickel 20%, UNS C71000, H55 Temper flat products
- Copper nickel 20%, UNS C71000, OSO25 Temper tubing
- Copper nickel 20%, UNS C71000, H10 Temper wire
- Cupronickel 75-25, UNS C71300 Copper Coinage Alloy
- Copper nickel 30%, UNS C71500
- Copper nickel 30%, UNS C71500, M20 Temper 25 mm plate
- Copper nickel 30%, UNS C71500, O61 Temper 1 mm strip
- Copper nickel 30%, UNS C71500, H80 Temper 1 mm strip
- Copper nickel 30%, UNS C71500, H02 Temper 25 mm rod
- Copper nickel 30%, UNS C71500, OSO25 Temper 25 mm tubing
- Copper nickel 30%, UNS C71500, OSO35 Temper 114 mm tubing
- Copper, 27% Nickel Clad
- Copper nickel 30%, UNS C71500, O61 Temper < 25 mm rod
- Copper nickel 30%, UNS C71500, O61 Temper 19 mm tubing
- Copper nickel 30%, UNS C71500, H80 Temper < 25 mm rod
- Copper nickel 30%, UNS C71500, H80 Temper 19 mm tubing
- Copper Nickel, UNS C71640 Copper Alloy
- Copper, UNS C71700
- Chromium-Bearing Copper-Nickel, UNS C71900, Heat Treated
- Chromium-Bearing Copper-Nickel, UNS C71900, Half-Hard Temper
- Chromium-Bearing Copper-Nickel, UNS C71900, Hard Temper
- Chromium-Bearing Copper-Nickel, UNS C71900, Spring Temper
- Tin-Bearing Copper Nickel, UNS C72500
- Tin-Bearing Copper Nickel, UNS C72500, Annealed flat products
- Tin-Bearing Copper Nickel, UNS C72500, Quarter Hard flat products
- Tin-Bearing Copper Nickel, UNS C72500, Half Hard flat products
- Tin-Bearing Copper Nickel, UNS C72500, Hard flat products
- Tin-Bearing Copper Nickel, UNS C72500, Extra Hard flat products
- Tin-Bearing Copper Nickel, UNS C72500, Spring flat products
- Tin-Bearing Copper Nickel, UNS C72500, Super Spring flat products
- Tin-Bearing Copper Nickel, UNS C72500, Annealed wire
- Copper Nickel Tin, UNS C72800
- Copper, UNS C73500
- Nickel silver 65-10, UNS C74500
- Nickel silver 65-10, UNS C74500, OSO70 Temper flat products
- Nickel silver 65-10, UNS C74500, OSO50, Temper flat products
- Nickel silver 65-10, UNS C74500, OSO35, Temper flat products
- Nickel silver 65-10, UNS C74500, OSO25, Temper flat products
- Nickel silver 65-10, UNS C74500, OSO15, Temper flat products
- Nickel silver 65-10, UNS C74500, H00 Temper flat products
- Nickel silver 65-10, UNS C74500, H00 (10%) Temper wire
- Nickel silver 65-10, UNS C74500, H01, Temper flat products
- Nickel silver 65-10, UNS C74500, H01 (20%) Temper wire
- Nickel silver 65-10, UNS C74500, H02 Temper flat products
- Nickel silver 65-10, UNS C74500, H02 (37%) Temper wire
- Nickel silver 65-10, UNS C74500, H04 Temper flat products
- Nickel silver 65-10, UNS C74500, H04 (60%) Temper wire
- Nickel silver 65-10, UNS C74500, H06 Temper flat products
- Nickel silver 65-10, UNS C74500, H06 (75%) Temper wire
- Nickel silver 65-10, UNS C74500, H08 (84%) Temper wire
- Nickel silver 65-10, UNS C74500, OSO70 Temper wire
- Nickel silver 65-10, UNS C74500, OSO50, Temper wire
- Nickel silver 65-10, UNS C74500, OSO35, Temper wire
- Nickel silver 65-10, UNS C74500, OSO25, Temper wire
- Nickel silver 65-10, UNS C74500, OSO15, Temper wire
- Nickel silver 65-18, UNS C75200
- Nickel silver 65-18, UNS C75200, OSO35 Temper flat products
- Nickel silver 65-18, UNS C75200, OSO15 Temper flat products
- Nickel silver 65-18, UNS C75200, H01, Temper flat products
- Nickel silver 65-18, UNS C75200, H02, Temper flat products
- Nickel silver 65-18, UNS C75200, H02 (20%) Temper rod
- Nickel silver 65-18, UNS C75200, H04 Temper flat products
- Nickel silver 65-18, UNS C75200, OSO35 Temper rod
- Nickel silver 65-18, UNS C75200, OSO35 Temper wire
- Nickel silver 65-18, UNS C75200, OSO15 Temper wire
- Nickel silver 65-18, UNS C75200, H01, Temper wire
- Nickel silver 65-18, UNS C75200, H02, Temper wire
- Nickel silver 65-18, UNS C75200, H04 Temper wire
- Nickel silver 65-15, UNS C75400
- Nickel silver 65-15, UNS C75400, OSO70 Temper sheet or strip
- Nickel silver 65-15, UNS C75400, OSO50 Temper sheet or strip
- Nickel silver 65-15, UNS C75400, OSO35 Temper sheet or strip
- Nickel silver 65-15, UNS C75400, OSO25 Temper sheet or strip
- Nickel silver 65-15, UNS C75400, OSO15 Temper sheet or strip
- Nickel silver 65-15, UNS C75400, H00 Temper sheet or strip
- Nickel silver 65-15, UNS C75400, H01 Temper sheet or strip
- Nickel silver 65-15, UNS C75400, H02 Temper sheet or strip
- Nickel silver 65-15, UNS C75400, H04 Temper sheet or strip
- Nickel silver 65-15, UNS C75400, H06 Temper sheet or strip
- Nickel silver 65-12, UNS C75700
- Nickel silver 65-12, UNS C75700, OSO70 Temper sheet or strip
- Nickel silver 65-12, UNS C75700, OSO50 Temper sheet or strip
- Nickel silver 65-12, UNS C75700, OSO35 Temper sheet or strip
- Nickel silver 65-12, UNS C75700, OSO25 Temper sheet or strip
- Nickel silver 65-12, UNS C75700, OSO15 Temper sheet or strip
- Nickel silver 65-12, UNS C75700, H00 Temper sheet or strip
- Nickel silver 65-12, UNS C75700, H01 Temper sheet or strip
- Nickel silver 65-12, UNS C75700, H02 Temper sheet or strip
- Nickel silver 65-12, UNS C75700, H04 Temper sheet or strip
- Nickel silver 65-12, UNS C75700, H06Temper sheet or strip
- Copper, UNS C76200
- Nickel silver 55-18, UNS C77000
- Nickel silver 55-18, UNS C77000, OSO35 Temper flat products
- Nickel silver 55-18, UNS C77000, H04 Temper flat products
- Nickel silver 55-18, UNS C77000, H06 Temper flat products
- Nickel silver 55-18, UNS C77000, H08 Temper flat products
- Nickel silver 55-18, UNS C77000, H08 (68%) Temper wire
- Nickel silver 55-18, UNS C77000, OSO35 Temper wire
- Nickel Silver, CDA 764
- Copper-Nickel, Chromium Bearing, UNS C72200
- Leaded nickel silver 65-8-2, UNS C78200
- Copper, UNS C78200, OSO35 Temper
- Copper, UNS C78200, OSO15 Temper
- Copper, UNS C78200, H01 Temper
- Copper, UNS C78200, H02 Temper
- Copper, UNS C78200, H03 Temper
- Copper, UNS C78200, H04 Temper
- Copper, UNS C78200, H06 Temper
- Shibuichi
- Kuromi-do
- Shakudo
- UNS C80100, Copper Casting Alloy
- UNS C80300, Copper Casting Alloy
- UNS C80500, Copper Casting Alloy
- UNS C80700, Copper Casting Alloy
- UNS C80900, Copper Casting Alloy
- UNS C81100, Copper Casting Alloy
- UNS C81300, Copper Casting Alloy
- UNS C81400, Copper Casting Alloy
- UNS C81500, Copper Casting Alloy
- UNS C81700, Copper Casting Alloy
- Beryllium-Copper Alloy 50C, UNS C81800, As-cast
- Beryllium-Copper Alloy 50C, UNS C81800, Cast and Aged
- Beryllium-Copper Alloy 50C, UNS C81800, TB00 Temper
- Beryllium-Copper Alloy 50C, UNS C81800, TF00 Temper
- Beryllium Copper Alloy 10C, UNS C82000 UNS C82000 As-cast
- Beryllium Copper Alloy 10C, UNS C82000 UNS C82000 Cast and Aged
- Beryllium Copper Alloy 10C, UNS C82000 UNS C82000 TB00 Temper
- Beryllium Copper Alloy 10C, UNS C82000 UNS C82000 TF00 Temper
- UNS C82100, Copper Casting Alloy
- Beryllium-Copper Alloy 30C, UNS C82200, As-Cast
- Beryllium-Copper Alloy 30C, UNS C82200, Cast and Aged
- Beryllium-Copper Alloy 30C, UNS C82200, TB00 Temper
- Beryllium-Copper Alloy 30C, UNS C82200, TF00 Temper
- Beryllium-Copper Alloy 30C, UNS C82400, As-Cast
- Beryllium-Copper Alloy 30C, UNS C82400, Cast and Aged
- Beryllium-Copper Alloy 30C, UNS C82400, TB00 Temper
- Beryllium-Copper Alloy 30C, UNS C82400, TF00 Temper
- UNS C82400, Beryllium Copper Casting Alloy, Annealed
- UNS C82400, Beryllium Copper Casting Alloy, Heat Treated
- Beryllium-Copper Alloy 20C, UNS C82500, As Cast
- Beryllium-Copper Alloy 20C, UNS C82500, Cast and Aged
- Beryllium-Copper Alloy 20C, UNS C82500, TB00 Temper
- Beryllium-Copper Alloy 20C, UNS C82500, TF00 Temper
- Beryllium-Copper Casting Alloy 245C, UNS C82600, As-Cast
- Beryllium-Copper Casting Alloy 245C, UNS C82600, Cast and Aged
- Beryllium-Copper Casting Alloy 245C, UNS C82600, TB00 Temper
- Beryllium-Copper Casting Alloy 245C, UNS C82600, TF00 Temper
- UNS C82700, Copper Casting Alloy
- Beryllium-Copper Casting Alloy 275C, UNS C82800, As-Cast
- Beryllium-Copper Casting Alloy 275C, UNS C82800, Cast and Aged
- Beryllium-Copper Casting Alloy 275C, UNS C82800, TB00 Temper
- Beryllium-Copper Casting Alloy 275C, UNS C82800, TF00 Temper
- Contact Metal, UNS C83300, Copper Casting Alloy
- UNS C83400, Copper Casting Alloy
- Leaded Red Brass, UNS C83600, Copper Casting Alloy
- Hydraulic Bronze, UNS C83800, Copper Casting Alloy
- UNS C84200, Copper Casting Alloy
- Valve Metal, UNS C84400, Copper Casting Alloy
- UNS C84500, Copper Casting Alloy
- Leaded Semi-Red Brass, UNS C84800, Copper Casting Alloy
- Leaded Yellow Brass, UNS C85200, Copper Casting Alloy
- Leaded Yellow Brass, UNS C85400, Copper Casting Alloy
- UNS C85500, Copper Casting Alloy
- Leaded Yellow Brass, UNS C85700, Copper Casting Alloy, Sand and Centrifugal Castings
- Leaded Yellow Brass, UNS C85800, Copper Casting Alloy, Die Castings
- Manganese Bronze, UNS C86100, Copper Casting Alloy
- Manganese Bronze, UNS C86200, Copper Casting Alloy
- Manganese Bronze, UNS C86300, Copper Casting Alloy
- Leaded High-Strength Yellow Brass, UNS C86400, Copper Casting Alloy
- High-Strength Yellow Brass, UNS C86500, Copper Casting Alloy
- Leaded High-Strength Yellow Brass, UNS C86700, Copper Casting Alloy
- Nickel-Manganese Bronze, UNS C86800, Copper Casting Alloy
- Everdur, UNS C87300, Copper Casting Alloy
- UNS C87400, Copper Casting Alloy
- Tombasil, UNS C87500, Copper Casting Alloy
- Low-Zinc Silicon Brass, UNS C87600, Copper Casting Alloy
- UNS C87610, Copper Casting Alloy
- Tombasil, UNS C87800, Copper Casting Alloy
- Silicon Yellow Brass, UNS C87900, Copper Casting Alloy
- UNS C90200, Copper Casting Alloy
- Tin Bronze UNS C90300, Copper Casting Alloy
- Tin Bronze, UNS C90500, Copper Casting Alloy
- Tin Bronze, UNS C90700, Copper Casting Alloy
- UNS C90800, Copper Casting Alloy
- UNS C90900, Copper Casting Alloy
- UNS C91000, Copper Casting Alloy
- UNS C91100, Copper Casting Alloy
- UNS C91300, Copper Casting Alloy
- UNS C91600, Copper Casting Alloy
- Nickel Gear Bronze, UNS C91700, Copper Casting Alloy
- Navy "M" Bronze, UNS C92200, Copper Casting Alloy
- Leaded Tin Bronze, UNS C92300, Copper Casting Alloy
- UNS C92400, Copper Casting Alloy
- Leaded Tin Bronze, UNS C92500, Copper Casting Alloy
- Leaded Tin Bronze, UNS C92600, Copper Casting Alloy
- Leaded Tin Bronze, UNS C92700, Copper Casting Alloy
- UNS C92800, Copper Casting Alloy
- Leaded Nickel-Tin Bronze, UNS C92900, Copper Casting Alloy
- High-Leaded Tin Bronze, UNS C93200, Copper Casting Alloy, Bearing Bronze 660
- High-Leaded Tin Bronze, UNS C93400, Copper Casting Alloy
- High-Leaded Tin Bronze, UNS C93500, Copper Casting Alloy
- High-Leaded Tin Bronze, UNS C93600, Copper Casting Alloy
- High-Leaded Tin Bronze, UNS C93700, Copper Casting Alloy
- High-Leaded Tin Bronze, UNS C93800, Copper Casting Alloy, Sand-Cast
- High-Leaded Tin Bronze, UNS C93800, Copper Casting Alloy, Centrifugally Cast
- High-Leaded Tin Bronze, UNS C93900, Copper Casting Alloy
- UNS C94000, Copper Casting Alloy
- UNS C94100, Copper Casting Alloy
- High-Leaded Tin Bronze, UNS C94300, Copper Casting Alloy
- UNS C94400, Copper Casting Alloy
- Medium Bronze, UNS C94500, Copper Casting Alloy
- UNS C94700, Copper Casting Alloy
- UNS C94800, Copper Casting Alloy
- UNS C94900, Copper Casting Alloy
- Aluminum Bronze, UNS C95200, Copper Casting Alloy
- Aluminum Bronze, UNS C95300, Copper Casting Alloy
- Aluminum Bronze, UNS C95400, Copper Casting Alloy
- Aluminum Bronze, UNS C95410, Copper Casting Alloy
- Aluminum Bronze, UNS C95500, Copper Casting Alloy
- Sluminum-Silicon Bronze, UNS C95600, Copper Casting Alloy
- Manganese-Aluminum Bronze, UNS C95700, Copper Casting Alloy
- Alpha Nickel-Aluminum Bronze, UNS C95800, Copper Casting Alloy
- UNS C96200, Copper Casting Alloy
- UNS C96300, Copper Casting Alloy
- UNS C96400, Copper Casting Alloy
- Beryllium Cupro-Nickel, UNS C96600, Copper Casting Alloy
- Copper Nickel Tin UNS C96800, Copper Casting Alloy
- UNS C96700, Copper Casting Alloy
- Leaded Nickel Brass, UNS C97300, Copper Casting Alloy
- UNS C97400, Copper Casting Alloy
- Leaded Nickel Bronze, UNS C97600, Copper Casting Alloy
- Leaded Nickel Bronze, UNS C97800, Copper Casting Alloy
- UNS C98200, Copper Casting Alloy
- UNS C98400, Copper Casting Alloy
- UNS C98600, Copper Casting Alloy
- UNS C98800, Copper Casting Alloy
- UNS C99300, Copper Casting Alloy
- Nondezincification Alloy, UNS C99400, Copper Casting Alloy
- NDZ-S, UNS C99500, Copper Casting Alloy
- UNS C99600, Copper Casting Alloy
- White Manganese Brass, UNS C99700, Copper Casting Alloy
- UNS C99750, Copper Casting Alloy
- Beryllium Copper 21C Copper Casting Alloy As-Cast
- Beryllium Copper 21C Copper Casting Alloy Cast and Aged
- Beryllium Copper 21C Copper Casting Alloy Solution Treated
- Beryllium Copper 21C Copper Casting Alloy Solution Treated and Aged
- Beryllium Copper Nickel 72C Copper Casting Alloy
- Beryllium Copper Nickel 72C Copper Casting Alloy
- Tin-Bearing Copper (SCuR3), 1/2 Hard Temper
- Titanium Copper (TiCuR1), 1/4 Hard Temper
- Titanium Copper (TiCuR1), EH Temper
- Ductile Iron grade 60-40-18
- Ductile Iron grade 80-60-03
- Ductile Iron grade 60-40-18, low temperature service
- Ductile Iron grade 65-45-12
- Ductile Iron grade 80-55-06
- Ductile Iron grade 100-70-03
- Ductile Iron grade 120-90-02
- Ductile Iron grade D4018
- Ductile Iron grade D4512
- Ductile Iron grade D5506
- Ductile Iron grade D7003
- Ductile Iron grade class A
- Ductile Iron grade class B
- Ductile Iron grade class C
- Ductile Iron tension grade 60-40-18
- Ductile Iron tension grade 65-45-12
- Ductile Iron tension grade 80-55-06
- Ductile Iron tension grade 120-90-02
- Ductile Iron compression grade 60-40-18
- Ductile Iron compression grade 65-45-12
- Ductile Iron compression grade 80-55-06
- Ductile Iron compression grade 120-90-02
- Ductile Iron torsion grade 60-40-18
- Ductile Iron torsion grade 65-45-12
- Ductile Iron torsion grade 80-55-06
- Ductile Iron torsion grade 120-90-02
- High Silicon Ductile Iron at RT 4Si nominal alloy content
- High Silicon Ductile Iron at RT 4Si-0.5Mo nominal alloy content
- High Silicon Ductile Iron at RT 4Si-1.0Mo nominal alloy content
- High Silicon Ductile Iron at RT 4Si-1.5Mo nominal alloy content
- High Silicon Ductile Iron at RT 4Si-2.0Mo nominal alloy content
- High Silicon Ductile Iron at RT 4Si-2.5Mo nominal alloy content
- High Silicon Ductile Iron at RT 2.8Si-1.0Mo nominal alloy content
- High Silicon Ductile Iron at RT 4Si-0.9V nominal alloy content
- ASTM A439 Austenitic Ductile Iron type D2
- ASTM A439 Austenitic Ductile Iron type D2B
- ASTM A439 Austenitic Ductile Iron type D2C
- ASTM A439 Austenitic Ductile Iron type D3
- ASTM A439 Austenitic Ductile Iron type D3A
- ASTM A439 Austenitic Ductile Iron type D4
- ASTM A439 Austenitic Ductile Iron type D5
- ASTM A439 Austenitic Ductile Iron type D5B
- ASTM A439 Austenitic Ductile Iron type D5S
- ASTM 897/A897M-06 Grade 110-70-11 Austempered Ductile Iron
- ASTM 897 Grade 1 (125-80-10), Austempered Ductile Iron (Obsolete with ASTM A897/A897M-06)
- ASTM 897/A897M-06 Grade 130-90-09 Austempered Ductile Iron
- ASTM 897 Grade 2 (150-100-07), Austempered Ductile Iron
- ASTM 897 Grade 3 (175-125-04), Austempered Ductile Iron
- ASTM 897 Grade 4 (200-155-01), Austempered Ductile Iron
- ASTM 897 Grade 5 (230-185-00), Austempered Ductile Iron
- SAE J2477 AD 750 Automotive Austempered Ductile Iron
- SAE J2477 AD 900 Automotive Austempered Ductile Iron
- SAE J2477 AD 1050 Automotive Austempered Ductile Iron
- SAE J2477 AD 1200 Automotive Austempered Ductile Iron
- SAE J2477 AD 1400 Automotive Austempered Ductile Iron
- SAE J2477 AD 1600 Automotive Austempered Ductile Iron
- Alpha-2 Titanium Aluminide, Ti3Al
- Gamma Titanium Aluminide, TiAl
- Titanium Aluminide, TiAl3
- Nickel Aluminide, Ni3Al
- Nickel Aluminide, NiAl
- Iron Aluminide, Fe3Al
- Iron Aluminide, FeAl
- Molybdenum Disilicide, MoSi2
- Lead-Base Babbitt Alloy, UNS L53346
- Lead-Base Babbitt Alloy 7, UNS L53581 (UNS L53585)
- Lead-Base Babbitt Alloy 8, UNS L53565
- Babbitt Alloy, SAE 14
- Lead-Base Babbitt Alloy 15, UNS L53620
- Lead-Tin Babbit Alloy
- Pure Lead (Corroding Lead), UNS L50042, Sand Cast
- Pure Lead (Corroding Lead), UNS L50042, Chill Cast
- 98Pb-1Sn-1Ag Lead Solder Alloy, UNS L50131
- 93.5Pb-5.5Sn-1Ag Lead Solder Alloy, UNS L50134
- Lead Solder Alloy, UNS L50172
- Arsenical Lead Cable-Sheathing Alloy, UNS L50310, Cable Sheath, Extruded, Air-cooled
- Arsenical Lead Cable-Sheathing Alloy, UNS L50310, Pipe, Extruded, Air-cooled
- Arsenical Lead Cable-Sheathing Alloy, UNS L50310, Cable Sheath, Extruded at 425°C (800°F), Water Quenched
- Arsenical Lead Cable-Sheathing Alloy, UNS L50310, Pipe, Extruded at 425°C (800°F), Water Quenched
- Arsenical Lead Cable-Sheathing Alloy, UNS L50310, Cable Sheath, Extruded at 450°C (800°F), Water Quenched
- Arsenical Lead Cable-Sheathing Alloy, UNS L50310, Pipe, Extruded at 450°C (800°F), Water Quenched
- Arsenical Lead Cable-Sheathing Alloy, UNS L50310, Pipe, Extruded at 550°C (1020°F), Quenched
- Battery Grid Alloy (Pb-Ca), UNS L50737
- Battery Grid Alloy (Pb-Ca), UNS L50740
- Battery Grid Alloy (Pb-Ca), UNS L50750
- Battery Grid Alloy (Pb-Ca), UNS L50760
- Battery Grid Alloy (Pb-Ca), UNS L50775
- Battery Grid Alloy (Pb-Ca), UNS L50780
- Battery Grid Alloy (Pb-Ca), UNS L50790
- Chemical Lead, UNS L51120
- Copper-Bearing Lead (Acid-Copper Lead), UNS L51121
- Lead-Tellurium-Copper Alloy, UNS L51123
- Copperized Soft Lead, UNS L51125
- Lead-Indium Alloy, UNS L51535
- Lead-Indium Alloy, UNS L51570
- Lead 1% Sb Sheathing Alloy, UNS L52605
- Hard Lead (96Pb-4Sb), UNS L52901, Cold-Rolled
- Hard Lead (96Pb-4Sb), UNS L52901, Heat Treated
- Hard Lead (94Pb-6Sb), UNS L53105, Chill Cast
- Hard Lead (94Pb-6Sb), UNS L53105, Cold Rolled
- Hard Lead (94Pb-6Sb), UNS L53105, Extruded
- Lead-Antimony Alloy, UNS L53230, Cold-Rolled
- Lead-Antimony Alloy, UNS L53230, Heat Treated
- Lead-Antimony Alloy, UNS L53305
- Lead-Indium-Silver Solder Alloy, UNS L51510
- 97.5Pb-2.5Ag Lead-Silver Solder, ASTM Class 2.5S UNS L50132
- 94.5Pb-5.5Ag Lead-Silver Solder, ASTM Class 5.5S; UNS L50180
- 97.5Pb-1.0Sn-1.5Ag Lead-Tin-Silver Solder, ASTM Class 1.5S
- 97Pb-2.5Sn-0.5Ag Lead-Tin-Silver Solder
- 94.5Pb-5Sn-0.5Ag Lead-Tin-Silver Solder
- 36Pb-62Sn-2Ag Lead-Tin-Silver Solder
- 36Pb-62Sn-2Ag Lead-Tin-Silver Solder, ASTM B 32 Grade Sn62
- 88Pb-10Sn-2Ag Lead-Tin-Silver Solder, ASTM B 32 Grade Sn10B
- 5% Sn Antimonial Lead Solder, UNS L54321
- 5/95 Solder (95Pb-5Sn), UNS L54320
- 10/90 (90Pb-10Sn) Solder - ASTM B32 Grade Sn10A, UNS L54520
- 85Pb-15Sn Antimonial Solder, ASTM Class 15B
- 20/80 (80Pb-20Sn) Solder- ASTM B 32 Grade Sn20A, UNS L54711
- 79Pb-20Sn-1.0Sb Tin-Lead-Antimony Solder, ASTM Class 20C
- 75Pb-25Sn Solder, ASTM Class 25A
- 73.7Pb-25Sn-1.3 Tin-Lead-Antimony Solder, ASTM Class 25C
- 30/70 (70Pb-30Sn) Solder- ASTM B 32 Grade Sn30A, UNS L54280
- 68.4Pb-30Sn-1.6Sb Tin-Lead-Antimony Solder, ASTM Class 30C
- 68Pb-30Sn-1.5Sb Tin-Lead-Antimony Solder, ASTM B 32 Grade Sn30B
- 65Pb-35Sn Solder, ASTM Class 35A
- 63.2Pb-35Sn-1.8Sb Tin-Lead-Antimony Solder, ASTM Class 35C
- 63Pb-35Sn-2Sb Tin-Lead-Antimony Solder, ASTM B 32 Grade Sn35B
- 40/60 (60Pb-40Sn) Solder- ASTM B 32 Grade Sn40A, UNS L54915
- 58Pb-40Sn-2.0Sb Tin-Lead-Antimony Solder, ASTM Class 40C
- 58Pb-40Sn-2Sb Tin-Lead-Antimony Solder, ASTM B 32 Grade Sn40B
- 55Pb-45Sn Solder, ASTM Class 45A
- 50/50 (50Pb-50Sn) Solder- ASTM B 32 Grade Sn50, UNS L55030
- 60-40 Soft Solder (60 Sn-40Pb) - ASTM B 32 Grade Sn60
- Eutectic Solder (63Sn-37Pb) - ASTM B 32 Grade Sn63
- 70-30 Soft Solder (70Sn-30Pb) - ASTM B 32 Grade Sn70
- Tin-Silver Solder (95Sn-5Ag), ASTM B 32 Grade Sn95
- Antimonial-Tin Solder (95Sn-5Sb), ASTM B 32 Grade S65
- 96Sn-4Ag Tin-Silver Solder, ASTM Class 96TS
- 98Pb-2Sn Solder, ASTM B 32 Grade Sn2
- Pewter, Annealed Sheet
- Pewter, Cold-Rolled Sheet
- Tin, ASTM B 23, Alloy 1
- Tin, ASTM B 23, Alloy 2
- Tin, ASTM B 23, Alloy 3
- Tin, ASTM B 102, Alloy PY 1815A, Die Cast
- White Metal (92Sn-8Sb), Chill cast
- White Metal (92Sn-8Sb), Extruded Wire
- Magnesium Alloys, General
- Magnesium AE42-F, Die Cast
- Magnesium AM100A-T61, Sand Cast
- Magnesium AM100A-F, Cast
- Magnesium AM100A-T4, Cast
- Magnesium AM100A-T5, Cast
- Magnesium AM100A-T7, Cast
- Magnesium AM100A-T6, Cast
- Magnesium AM20-F, Die Cast
- Magnesium AM50A-F, Die Cast
- Magnesium - AM50A, Thixomolded®
- Magnesium AM60A-F, Die Cast
- Magnesium - AM60A, Thixomolded®
- Magnesium AM60B-F, Die Cast
- Magnesium AS21X1, Die Cast
- Magnesium AS21-F, Die Cast
- Magnesium AS41XA-F, Die Cast
- Magnesium AS41A-F, Die Cast
- Magnesium AS41B-F, Die Cast
- Magnesium AS41XB-F, Die Cast
- Magnesium AZ10A-F, Extruded
- Magnesium AZ21X1-F, Extruded Bars and Shapes
- Magnesium AZ31B-F, Extruded Solid Shapes
- Magnesium AZ31C-F, Extruded Solid Shapes
- Magnesium AZ31B-O, Annealed Sheet
- Magnesium AZ31B-H24, Hard Rolled Sheet
- Magnesium AZ31B, Extruded Hollow Shapes
- Magnesium AZ31B, Forgings
- Magnesium AZ31B-H26, Hard Rolled Sheet
- Magnesium AZ61A-F, Extruded Hollow Shapes
- Magnesium AZ61A-F, Extruded Solid Shapes
- Magnesium AZ61A-F, Forgings
- Magnesium AZ63A-T6, Sand Cast
- Magnesium AZ63A-F, Sand Cast
- Magnesium AZ63A-T4, Sand Cast
- Magnesium AZ63A-T5, Sand Cast
- Magnesium AZ63A-T7, Sand Cast
- Magnesium AZ80A-T5, Extruded
- Magnesium AZ80A-F, Extruded
- Magnesium AZ80A-T5, Forged
- Magnesium AZ80A-F, Forged
- Magnesium AZ81A-T4, Cast
- Magnesium AZ80A-T6, Forged
- Magnesium AZ91C-T6, Cast
- Magnesium AZ91C-T4, Cast
- Magnesium AZ91C-F, Cast
- Magnesium AZ91E-F, Cast
- Magnesium AZ91E-T4, Cast
- Magnesium AZ91E-T6, Cast
- Magnesium AZ91A-F, Die Cast
- Magnesium AZ91B-F, Die Cast
- Magnesium AZ91D-F, Cast
- Magnesium - AZ91D, Thixomolded®
- Magnesium AZ92A-T6, Cast
- Magnesium AZ92A-F, Cast
- Magnesium AZ92A-T4, Cast
- Magnesium AZ92A-T5, Cast
- Magnesium AZ92A-T7, Cast
- Electrolytic Copper Tough Pitch, 50% hard-drawn rod
- Electrolytic Copper Tough Pitch, 538°C (1000°F) annealed rod
- Electrolytic Copper Tough Pitch, hot forged rod
- Electrolytic Copper Tough Pitch, 5-40% cold reduction rod
- Electrolytic Copper Tough Pitch, cold forged 40% cold reduction rod
- Electrolytic Copper Tough Pitch, 0.015-0.045 mm grain size hardened strip
- Electrolytic Copper Tough Pitch, strip 427°C (800°F) anneal for 1 hour
- Phosphorized Copper Tube extruded and cold drawn to 19.05 mm
- Phosphorized Copper Tube 371°C (700°F) anneall for 1 hour
- High-Conductivity Oxygen-Free Copper hardened 0.015-0.040 mm grain size
- High-Conductivity Oxygen-Free Copper 704°C anneal for 1 hour
- Silver-Bearing Copper Strip hardened 0.015-0.040 mm grain size
- Silver-Bearing Copper Strip 649°C (1200°F) anneal for 1 hour
- Phosphorized Arsenical Copper Tube extruded and cold drawn to 19 by 1.25 mm
- Phosphorized Arsenical Copper Tube 699°C anneal for 30 minutes
- Arsenical Tough-Pitch Copper hardened 0.020-0.050 mm grain size
|