MatWeb Material ListThis series of pages has links to all data sheets in MatWeb. We have several search tools, listed above, that give you more efficient methods to reach the information that you need.
- Elkem Minsil® 2-6 mm Granulated Ferrosilicon
- Elkem Low Al Ferrosilicon FeSi 0.50 Al
- Elkem Low Al Ferrosilicon FeSi 0.30 Al
- Elkem Low Al Ferrosilicon FeSi 0.10 Al
- Elkem Low Carbon Ferrosilicon LC FeSi 75
- Elkem Low Carbon Ferrosilicon ULC FeSi 75
- Elkem Low Carbon Ferrosilicon LC FeSi 65
- Elkem Low Carbon Ferrosilicon ULC FeSi 65
- Elkem Injectsil® additive
- Elkem High Purity Ferrosilicon HP FeSi 75 0.05 Ti
- Elkem High Purity Ferrosilicon HP FeSi 75 0.025 Ti
- Elkem High Purity Ferrosilicon HP FeSi 75 0.02 Ti
- Terfenol-D Magnetostrictive Iron Alloy (Tb0.3Dy0.7Fe1. 92)
- NewMerc, Liquid Mercury Replacement Alloy
- Nickel Foam
- FiberNide Nickel Aluminide Foam Atomic 10% Aluminum
- FiberNide Nickel Aluminide Foam Atomic 15% Aluminum
- FiberNide Nickel Aluminide Foam Atomic 20% Aluminum
- FiberNide Nickel Aluminide Foam Atomic 22% Aluminum
- Aluchrom O® Resistance Alloy
- Goodfellow Aluminum-Copper/SiC Metal Matrix Composite
- Goodfellow Aluminum 50/Iron 50 Alloy
- Goodfellow Aluminum-Lithium/SiC Metal Matrix Composite
- Goodfellow Aluminum 50/Nickel 50 Alloy
- Goodfellow Aluminum 99/Silicon 1 Alloy
- Goodfellow Aluminum 75/Silicon 25 Alloy
- Goodfellow Aluminum 65.7/Silicon 34.3 Alloy
- Chromaloy O® Resistance Alloy
- Goodfellow Chromium 80/Aluminum 20 Alloy
- Goodfellow Chromium 70/Titanium 30 Alloy
- Goodfellow Cobalt 90/Aluminum 10 Alloy
- Goodfellow Cobalt 79/Aluminum 21 Alloy
- Goodfellow Cobalt/Boron/Silicon/Iron/Molybdenum/Nickel Alloy
- Goodfellow Cobalt/Silicon/Boron/Iron/Nickel Alloy
- Goodfellow Cobalt/Silicon/Boron/Manganese Alloy
- Goodfellow Copper 70/Iron 30 Alloy
- Goodfellow Copper 80/Lead 20 Alloy
- Goodfellow Copper 85/Silicon 15 Alloy
- Goodfellow Copper 98/Silver 2 Alloy
- Goodfellow Copper 80/Tin 20 Alloy
- Goodfellow Copper 90/Titanium 10 Alloy
- Goodfellow Copper 70/Titanium 30 Alloy
- Goodfellow Copper 56.4/Titanium 43.6 Alloy
- Goodfellow Copper 70/Zirconium 30 Alloy
- Goodfellow Copper 87/Zirconium 13 Alloy
- Dural® Aluminum /Copper/Magnesium Alloy
- Evanohm® Precision Resistance Alloy
- Goodfellow Gold 88/Germanium 12 Eutectic Alloy
- Nioro® Gold 82/Nickel 18 Alloy
- Goodfellow Gold 75/ Palladium 25 Alloy
- Havar® High-Strength Non-Magnetic Cobalt-Base Alloy
- Goodfellow High Permeability Nickel Magnetic Alloy
- Goodfellow Iron 81/Boron 13.5/Silicon 3.5 Alloy
- Goodfellow Iron 78/Boron 13/Silicon 9 Alloy
- Goodfellow Iron 79/Boron 16/Silicon 5 Alloy
- Goodfellow Iron 77.5/Boron 15/Silicon 7.5 Alloy
- Goodfellow Iron 90/Chromium 9/Molybdenum 1 Alloy
- Goodfellow Iron 40/Nickel 38/Boron 18 Alloy
- Goodfellow Iron 50/Nickel 50 Alloy
- Goodfellow Iron 58/Nickel 42 Alloy
- Goodfellow Iron 55/Nickel 45 Alloy
- Audiolloy® Iron 52/Nickel 48 Alloy
- Goodfellow Iron 91/Silicon 9 Alloy
- Goodfellow Iron 83/Silicon 17 Alloy
- Goodfellow Iron 60/Titanium 40 Alloy
- Goodfellow Lead 75/Tin 25 Alloy
- Goodfellow Magnetic Copper Alloy
- Goodfellow Magnetic Shielding Alloy - Nickel Base
- Goodfellow Manganese 70/Nickel 30 Alloy
- Goodfellow Manganese 80/Nickel 20 Alloy
- Manganin® Copper Resistance Alloy
- Goodfellow TZM Molybdenum High Temperature Alloy
- Awa®, Nickeloid®, Simlet®, Spedex® Nickel Silver
- Goodfellow Molybdenum 80/Titanium 20 Alloy
- Goodfellow Molybdenum 90/Titanium 10 Alloy
- Goodfellow Nanocrystalline Nickel
- Goodfellow Nickel 59/Aluminum 41 Alloy
- Goodfellow Nickel 79/Aluminum 21 Alloy
- Goodfellow Nickel 85/Boron 15 Alloy
- Goodfellow Nickel 78/Boron 14/Silicon 8 Alloy
- Nichrome®, Tophet A® Nickel 80 Chromium 20 Alloy
- Goodfellow Nickel 70/Copper 30 Alloy
- Goodfellow Nickel 52/Iron 48 Alloy
- Goodfellow Nickel/Iron/Molybdenum Alloy
- Goodfellow Nickel/Iron/Silicon/Boron Alloy
- Goodfellow Nickel 55/Titanium 45 Shape Memory Alloy
- Goodfellow Nickel 80/Iron 20 Alloy
- Goodfellow Nickel 81/Iron 19 Alloy
- Goodfellow Nickel 92/Manganese 8 Alloy
- Goodfellow Nickel 75/Manganese 25 Alloy
- Goodfellow Nickel 80/Molybdenum 20 Alloy
- Goodfellow Nickel 84/Molybdenum 16 Alloy
- Goodfellow Nickel 62/Silicon 38 Alloy
- Goodfellow Nickel 70/Titanium 30 Alloy
- Goodfellow Nickel 60/Titanium 40 Alloy
- Goodfellow Nickel 90/Titanium 10 Alloy
- Goodfellow Nickel 70/Zirconium 30 Alloy
- Goodfellow Niobium 56/Titanium 44 Alloy
- Goodfellow Niobium 99/Zirconium 1 Alloy
- Permendur 49® Cobalt Iron Magnetic Alloy
- Goodfellow Phosphor Bronze
- Goodfellow Platinum 90/Iridium 10 Alloy
- Goodfellow Platinum 90/Rhodium 10 Thermocouple Alloy
- Goodfellow Platinum 87/Rhodium 13Thermocouple Alloy
- Goodfellow Platinum 70/Rhodium 30 Thermocouple Alloy
- Goodfellow Platinum 94/Rhodium 6 Thermocouple Alloy
- Goodfellow Platinum 92/Tungsten 8 Alloy
- Goodfellow Roses Metal (Bi, Pb, Sn) Alloy
- Goodfellow Tantalum 90/Tungsten 10 Alloy
- Goodfellow T1-Thermocouple Alloy
- Goodfellow T2-Thermocouple Alloy
- Goodfellow Tin 60/Lead 39/Antimony 1 Alloy
- Goodfellow Titanium Bronze
- Goodfellow Titanium 65/Aluminum 35 Alloy
- Goodfellow Titanium 88/Aluminum 12 Alloy
- Goodfellow Titanium 78/Aluminum 22 Alloy
- Goodfellow Titanium 80/Chromium 20 Alloy
- Goodfellow Titanium 50/Iron 50 Alloy
- Goodfellow Titanium 84/Molybdenum 16 Alloy
- Goodfellow Titanium 92/Silicon 8 Alloy
- Goodfellow Titanium 90/Vanadium 10 Alloy
- Goodfellow Tungsten 90/Chromium 10 Alloy
- Goodfellow Tungsten 95/Titanium 5 Alloy
- Goodfellow Tungsten 75/Vanadium 25 Alloy
- Copelmet® Tungsten 72/Copper 28 Alloy
- Goodfellow Tungsten 60/Copper 40 Alloy
- Goodfellow Tungsten 75/Rhenium 25 Alloy
- Goodfellow Vanadium 75/Chromium 25 Alloy
- Goodfellow Zinc 50/Aluminum 50 Alloy
- Goodfellow Zinc 95/Copper 5 Alloy
- Goodfellow Zinc 90/Nickel 10 Alloy
- Goodfellow Zirconium 90/Aluminum 10 Alloy
- Goodfellow Zirconium 70/Nickel 30 Alloy
- Goodfellow Zirconium 56.5/Vanadium 43.5 Alloy
- Haynes® HR-120™ alloy, solution heat-treated plate, tested at RT
- Haynes® HR-120™ alloy, solution heat-treated plate, tested at 540°C (1000°F)
- Haynes® HR-120™ alloy, solution heat-treated plate, tested at 650°C (1200°F)
- Haynes® HR-120™ alloy, solution heat-treated plate, tested at 760°C (1400°F)
- Haynes® HR-120™ alloy, solution heat-treated plate, tested at 870°C (1600°F)
- Haynes® HR-120™ alloy, solution heat-treated plate, tested at 980°C (1800°F)
- Haynes® HR-120™ alloy, solution heat-treated plate, tested at 1095°C (2000°F)
- Haynes® HR-120™ alloy, solution heat-treated plate, tested at 1205°C (2200°F)
- Haynes® HR-120™ alloy, solution heat-treated
- Haynes® HR-120™ alloy, solution heat-treated aged at 1200°F for 1000 hours
- Haynes® HR-120™ alloy, solution heat-treated aged at 1400°F for 1000 hours
- Haynes® HR-120™ alloy, solution heat-treated aged at 1600°F for 1000 hours
- Haynes® HR-120™ alloy, solution heat-treated aged at 1800°F for 1000 hours
- Haynes® HR-160® alloy, hot rolled and solution annealed plate, tested at 21°C (70°F)
- Haynes® HR-160® alloy, hot rolled and solution annealed plate, tested at 93°C (200°F)
- Haynes® HR-160® alloy, hot rolled and solution annealed plate, tested at 204°C (400°F)
- Haynes® HR-160® alloy, hot rolled and solution annealed plate, tested at 316°C
- Haynes® HR-160® alloy, hot rolled and solution annealed plate, tested at 427°C (800°F)
- Haynes® HR-160® alloy, hot rolled and solution annealed plate, tested at 538°C (1000°F)
- Haynes® HR-160® alloy, hot rolled and solution annealed plate, tested at 649°C (1200°F)
- Haynes® HR-160® alloy, hot rolled and solution annealed plate, tested at 760°C (1400°F)
- Haynes® HR-160® alloy, hot rolled and solution annealed plate, tested at 871°C (1600°F)
- Haynes® HR-160® alloy, hot rolled and solution annealed plate, tested at 982°C
- Haynes® HR-160® alloy, hot rolled and solution annealed plate, tested at 1093°C
- Haynes® HR-160® alloy, hot rolled and solution annealed plate, tested at 11491°C
- Haynes® HR-160® alloy, hot rolled and solution annealed plate, tested at 1204°C (2200°F)
- Haynes® HR-160® alloy, solution annealed sheet, tested at 21°C (70°F)
- Haynes® HR-160® alloy, solution annealed sheet, tested at 538°C (1000°F)
- Haynes® HR-160® alloy, solution annealed sheet, tested at 649°C (1200°F)
- Haynes® HR-160® alloy, solution annealed sheet, tested at 760°C (1400°F)
- Haynes® HR-160® alloy, solution annealed sheet, tested at 871°C (1600°F)
- Haynes® HR-160® alloy, solution annealed sheet, tested at 982°C
- Haynes® HR-160® alloy, solution annealed sheet, tested at 1093°C
- Haynes® HR-160® alloy, solution annealed sheet, tested at 1149°C (2100°F)
- Haynes® HR-160® alloy, solution annealed sheet, tested at 1204°C (2200°F)
- Haynes® HR-160® alloy, annealed plate
- Haynes® HR-160® alloy, plate, aged 1000 hours at 649°C (1200°F)
- Haynes® HR-160® alloy, plate, aged 4000 hours at 649°C (1200°F)
- Haynes® HR-160® alloy, plate, aged 8000 hours at 649°C (1200°F)
- Haynes® HR-160® alloy, plate, aged 1000 hours at 760°C (1400°F)
- Haynes® HR-160® alloy, plate, aged 4000 hours at 760°C (1400°F)
- Haynes® HR-160® alloy, plate, aged 8000 hours at 760°C (1400°F)
- Haynes® HR-160® alloy, plate, aged 1000 hours at 871°C (1600°F)
- Haynes® HR-160® alloy, plate, aged 4000 hours at 871°C (1600°F)
- Haynes® HR-160® alloy, plate, aged 8000 hours at 871°C (1600°F)
- Haynes® 188 alloy, cold rolled and 1175°C solution annealed sheet, tested at RT
- Haynes® 188 alloy, cold rolled and 1175°C solution annealed sheet, tested at 540°C (1000°F)
- Haynes® 188 alloy, cold rolled and 1175°C solution annealed sheet, tested at 650°C (1200°F)
- Haynes® 188 alloy, cold rolled and 1175°C solution annealed sheet, tested at 760°C (1400°F)
- Haynes® 188 alloy, cold rolled and 1175°C solution annealed sheet, tested at 870°C (1600°F)
- Haynes® 188 alloy, cold rolled and 1175°C solution annealed sheet, tested at 980°C (1800°F)
- Haynes® 188 alloy, cold rolled and 1175°C solution annealed sheet, tested at 1095°C (2000°F)
- Haynes® 188 alloy, hot rolled and 1175°C solution annealed plate, tested at RT
- Haynes® 188 alloy, hot rolled and 1175°C solution annealed plate, tested at 540°C (1000°F)
- Haynes® 188 alloy, hot rolled and 1175°C solution annealed plate, tested at 650°C (1200°F)
- Haynes® 188 alloy, hot rolled and 1175°C solution annealed plate, tested at 760°C (1400°F)
- Haynes® 188 alloy, hot rolled and 1175°C solution annealed plate, tested at 870°C (1600°F)
- Haynes® 188 alloy, hot rolled and 1175°C solution annealed plate, tested at 980°C (1800°F)
- Haynes® 188 alloy, hot rolled and 1175°C solution annealed plate, tested at 1095°C (2000°F)
- Haynes® 188 alloy, hot rolled and 1175°C solution annealed plate, tested at 1150°C (2100°F)
- Haynes® 188 alloy, hot rolled and 1175°C solution annealed plate, tested at 1205°C (2200°F)
- Haynes® 188 alloy, plate at RT after 0 hours at 650°C (1200°F)
- Haynes® 188 alloy, plate at RT after 8000 hours at 650°C (1200°F)
- Haynes® 188 alloy, plate at RT after 0 hours at 760°C (1400°F)
- Haynes® 188 alloy, plate at RT after 8000 hours at 760°C (1400°F)
- Haynes® 188 alloy, plate at RT after 0 hours at 870°C (1600°F)
- Haynes® 188 alloy, plate at RT after 1000 hours at 870°C (1600°F)
- Haynes® 188 alloy, plate at RT after 4000 hours at 870°C (1600°F)
- Haynes® 188 alloy, plate at RT after 8000 hours at 870°C (1600°F)
- Haynes® 188 alloy, plate at RT after 16000 hours at 870°C (1600°F)
- Haynes® 188 alloy, 0% cold reduction, 3.2 mm thick sheet
- Haynes® 188 alloy, 10% cold reduction, 3.2 mm thick sheet
- Haynes® 188 alloy, 20% cold reduction, 3.2 mm thick sheet
- Haynes® 188 alloy, 30% cold reduction, 3.2 mm thick sheet
- Haynes® 188 alloy, 40% cold reduction, 3.2 mm thick sheet
- Haynes® 188 alloy, 10% cold reduction, 3.2 mm thick sheet, 1065°C for 5 minutes
- Haynes® 188 alloy, 20% cold reduction, 3.2 mm thick sheet, 1065°C for 5 minutes
- Haynes® 188 alloy, 30% cold reduction, 3.2 mm thick sheet, 1065°C for 5 minutes
- Haynes® 188 alloy, 40% cold reduction, 3.2 mm thick sheet, 1065°C for 5 minutes
- Haynes® 188 alloy, 10% cold reduction, 3.2 mm thick sheet, 1120°C for 5 minutes
- Haynes® 188 alloy, 20% cold reduction, 3.2 mm thick sheet, 1120°C for 5 minutes
- Haynes® 188 alloy, 30% cold reduction, 3.2 mm thick sheet, 1120°C for 5 minutes
- Haynes® 188 alloy, 40% cold reduction, 3.2 mm thick sheet, 1120°C for 5 minutes
- Haynes® 188 alloy, 10% cold reduction, 3.2 mm thick sheet, 1175°C for 5 minutes
- Haynes® 188 alloy, 20% cold reduction, 3.2 mm thick sheet, 1175°C for 5 minutes
- Haynes® 188 alloy, 30% cold reduction, 3.2 mm thick sheet, 1175°C for 5 minutes
- Haynes® 188 alloy, 40% cold reduction, 3.2 mm thick sheet, 1175°C for 5 minutes
- Haynes® 214™ alloy, cold rolled annealed sheet 2.0-3.2 mm thick, tested at RT
- Haynes® 214™ alloy, cold rolled annealed sheet 2.0-3.2 mm thick, tested at 540°C (1000°F)
- Haynes® 214™ alloy, cold rolled annealed sheet 2.0-3.2 mm thick, tested at 650°C (1200°F)
- Haynes® 214™ alloy, cold rolled annealed sheet 2.0-3.2 mm thick, tested at 760°C (1400°F)
- Haynes® 214™ alloy, cold rolled annealed sheet 2.0-3.2 mm thick, tested at 870°C (1600°F)
- Haynes® 214™ alloy, cold rolled annealed sheet 2.0-3.2 mm thick, tested at 980°C (1800°F)
- Haynes® 214™ alloy, cold rolled annealed sheet 2.0-3.2 mm thick, tested at 1095°C (2000°F)
- Haynes® 214™ alloy, cold rolled annealed sheet 2.0-3.2 mm thick, tested at 1150°C (2100°F)
- Haynes® 214™ alloy, cold rolled annealed sheet 2.0-3.2 mm thick, tested at 1205°C (2200°F)
- Haynes® 214™ alloy, hot rolled solution annealed plate 12.7 mm (1/2 in.) thick, tested at RT
- Haynes® 214™ alloy, hot rolled solution annealed plate 12.7 mm (1/2 in.) thick, tested at 540°C (1000°F)
- Haynes® 214™ alloy, hot rolled solution annealed plate 12.7 mm (1/2 in.) thick, tested at 650°C (1200°F)
- Haynes® 214™ alloy, hot rolled solution annealed plate 12.7 mm (1/2 in.) thick, tested at 760°C (1400°F)
- Haynes® 214™ alloy, hot rolled solution annealed plate 12.7 mm (1/2 in.) thick, tested at 870°C (1600°F)
- Haynes® 214™ alloy, hot rolled solution annealed plate 12.7 mm (1/2 in.) thick, tested at 980°C (1800°F)
- Haynes® 214™ alloy, hot rolled solution annealed plate 12.7 mm (1/2 in.) thick, tested at 1095°C (2000°F)
- Haynes® 214™ alloy, hot rolled solution annealed plate 12.7 mm (1/2 in.) thick, tested at 1150°C (2100°F)
- Haynes® 214™ alloy, hot rolled solution annealed plate 12.7 mm (1/2 in.) thick, tested at 1205°C (2200°F)
- Haynes® 214™ alloy, sheet, 0 hours exposure at 760°C (1400°F)
- Haynes® 214™ alloy, sheet, 32 hours exposure at 760°C (1400°F)
- Haynes® 214™ alloy, sheet, 100 hours exposure at 760°C (1400°F)
- Haynes® 214™ alloy, sheet, 1000 hours exposure at 760°C (1400°F)
- Haynes® 214™ alloy, sheet, 32 hours exposure at 870°C (1600°F)
- Haynes® 214™ alloy, sheet, 100 hours exposure at 870°C (1600°F)
- Haynes® 214™ alloy, sheet, 1000 hours exposure at 870°C (1600°F)
- Haynes® 214™ alloy, sheet, 32 hours exposure at 980°C (1800°F)
- Haynes® 214™ alloy, sheet, 100 hours exposure at 980°C (1800°F)
- Haynes® 214™ alloy, sheet, 1000 hours exposure at 980°C (1800°F)
- Haynes® 214™ alloy, 0% cold reduction
- Haynes® 214™ alloy, 10% cold reduction
- Haynes® 214™ alloy, 20% cold reduction
- Haynes® 214™ alloy, 30% cold reduction
- Haynes® 214™ alloy, 40% cold reduction
- Haynes® 214™ alloy, 50% cold reduction
- Haynes® 214™ alloy, 10% cold reduction, 980°C (1800°F) for 5 minutes
- Haynes® 214™ alloy, 20% cold reduction, 980°C (1800°F) for 5 minutes
- Haynes® 214™ alloy, 30% cold reduction, 980°C (1800°F) for 5 minutes
- Haynes® 214™ alloy, 40% cold reduction, 980°C (1800°F) for 5 minutes
- Haynes® 214™ alloy, 50% cold reduction, 980°C (1800°F) for 5 minutes
- Haynes® 214™ alloy, 10% cold reduction, 925°C for 5 minutes
- Haynes® 214™ alloy, 20% cold reduction, 925°C for 5 minutes
- Haynes® 214™ alloy, 30% cold reduction, 925°C for 5 minutes
- Haynes® 214™ alloy, 40% cold reduction, 925°C for 5 minutes
- Haynes® 214™ alloy, 50% cold reduction, 925°C for 5 minutes
- Haynes® 214™ alloy, 10% cold reduction, 1095°C (2000°F) for 5 minutes
- Haynes® 214™ alloy, 20% cold reduction, 1095°C (2000°F) for 5 minutes
- Haynes® 214™ alloy, 30% cold reduction, 1095°C (2000°F) for 5 minutes
- Haynes® 214™ alloy, 40% cold reduction, 1095°C (2000°F) for 5 minutes
- Haynes® 214™ alloy, 50% cold reduction, 1095°C (2000°F) for 5 minutes
- Haynes® 230® alloy, cold rolled and 1232°C solution annealed sheet, tested at RT
- Haynes® 230® alloy, cold rolled and 1232°C solution annealed sheet, tested at 538°C (1000°F)
- Haynes® 230® alloy, cold rolled and 1232°C solution annealed sheet, tested at 649°C (1200°F)
- Haynes® 230® alloy, cold rolled and 1232°C solution annealed sheet, tested at 760°C (1400°F)
- Haynes® 230® alloy, cold rolled and 1232°C solution annealed sheet, tested at 871°C (1600°F)
- Haynes® 230® alloy, cold rolled and 1232°C solution annealed sheet, tested at 982°C
- Haynes® 230® alloy, cold rolled and 1232°C solution annealed sheet, tested at 1093°C
- Haynes® 230® alloy, cold rolled and 1232°C solution annealed sheet, tested at 1149°C (2100°F)
- Haynes® 230® alloy, cold rolled and 1232°C solution annealed sheet, tested at 1204°C (2200°F)
- Haynes® 230® alloy, hot rolled and 1232°C solution annealed plate, tested at RT
- Haynes® 230® alloy, hot rolled and 1232°C solution annealed plate, tested at 538°C (1000°F)
- Haynes® 230® alloy, hot rolled and 1232°C solution annealed plate, tested at 649°C (1200°F)
- Haynes® 230® alloy, hot rolled and 1232°C solution annealed plate, tested at 760°C (1400°F)
- Haynes® 230® alloy, hot rolled and 1232°C solution annealed plate, tested at 871°C (1600°F)
- Haynes® 230® alloy, hot rolled and 1232°C solution annealed plate, tested at 982°C
- Haynes® 230® alloy, hot rolled and 1232°C solution annealed plate, tested at 1093°C
- Haynes® 230® alloy, hot rolled and 1232°C solution annealed plate, tested at 1149°C (2100°F)
- Haynes® 230® alloy, hot rolled and 1232°C solution annealed plate, tested at 1204°C (2200°F)
- Haynes® 230® alloy, as cast vacuum investment casting, tested at RT
- Haynes® 230® alloy, as cast vacuum investment casting, tested at 538°C (1000°F)
- Haynes® 230® alloy, as cast vacuum investment casting, tested at 649°C (1200°F)
- Haynes® 230® alloy, as cast vacuum investment casting, tested at 760°C (1400°F)
- Haynes® 230® alloy, as cast vacuum investment casting, tested at 871°C (1600°F)
- Haynes® 230® alloy, as cast vacuum investment casting, tested at 982°C
- Haynes® 230® alloy, as cast vacuum investment casting, tested at 1093°C
- Haynes® 230® alloy, plate, 0 hours exposure at 649°C (1200°F)
- Haynes® 230® alloy, plate, 1000 hours exposure at 649°C (1200°F)
- Haynes® 230® alloy, plate, 4000 hours exposure at 649°C (1200°F)
- Haynes® 230® alloy, plate, 8000 hours exposure at 649°C (1200°F)
- Haynes® 230® alloy, plate, 16000 hours exposure at 649°C (1200°F)
- Haynes® 230® alloy, plate, 1000 hours exposure at 760°C (1400°F)
- Haynes® 230® alloy, plate, 4000 hours exposure at 760°C (1400°F)
- Haynes® 230® alloy, plate, 8000 hours exposure at 760°C (1400°F)
- Haynes® 230® alloy, plate, 16000 hours exposure at 760°C (1400°F)
- Haynes® 230® alloy, plate, 1000 hours exposure at 871°C (1600°F)
- Haynes® 230® alloy, plate, 4000 hours exposure at 871°C (1600°F)
- Haynes® 230® alloy, plate, 8000 hours exposure at 871°C (1600°F)
- Haynes® 230® alloy, plate, 16000 hours exposure at 871°C (1600°F)
- Haynes® 230® alloy, 0% cold reduction
- Haynes® 230® alloy, 10% cold reduction
- Haynes® 230® alloy, 20% cold reduction
- Haynes® 230® alloy, 30% cold reduction
- Haynes® 230® alloy, 40% cold reduction
- Haynes® 230® alloy, 50% cold reduction
- Haynes® 230® alloy, 10% cold reduction, 1066°C anneal for 5 minutes
- Haynes® 230® alloy, 20% cold reduction, 1066°C anneal for 5 minutes
- Haynes® 230® alloy, 30% cold reduction, 1066°C anneal for 5 minutes
- Haynes® 230® alloy, 40% cold reduction, 1066°C anneal for 5 minutes
- Haynes® 230® alloy, 50% cold reduction, 1066°C anneal for 5 minutes
- Haynes® 230® alloy, 10% cold reduction, 1121°C anneal for 5 minutes
- Haynes® 230® alloy, 20% cold reduction, 1121°C anneal for 5 minutes
- Haynes® 230® alloy, 30% cold reduction, 1121°C anneal for 5 minutes
- Haynes® 230® alloy, 40% cold reduction, 1121°C anneal for 5 minutes
- Haynes® 230® alloy, 50% cold reduction, 1121°C anneal for 5 minutes
- Haynes® 230® alloy, 10% cold reduction, 1177°C anneal for 5 minutes
- Haynes® 230® alloy, 20% cold reduction, 1177°C anneal for 5 minutes
- Haynes® 230® alloy, 30% cold reduction, 1177°C anneal for 5 minutes
- Haynes® 230® alloy, 40% cold reduction, 1177°C anneal for 5 minutes
- Haynes® 230® alloy, 50% cold reduction, 1177°C anneal for 5 minutes
- Haynes® 230® alloy, GMAW deposit weld metal, tested at RT
- Haynes® 230® alloy, GMAW deposit weld metal, tested at 538°C (1000°F)
- Haynes® 230® alloy, GMAW deposit weld metal, tested at 871°C (1600°F)
- Haynes® 242™ alloy, bar and rings, annealed and aged, tested at RT
- Haynes® 242™ alloy, bar and rings, annealed and aged, tested at 95°C (200°F)
- Haynes® 242™ alloy, bar and rings, annealed and aged, tested at 205°C (400°F)
- Haynes® 242™ alloy, bar and rings, annealed and aged, tested at 315°C (600°F)
- Haynes® 242™ alloy, bar and rings, annealed and aged, tested at 425°C (800°F)
- Haynes® 242™ alloy, bar and rings, annealed and aged, tested at 540°C (1000°F)
- Haynes® 242™ alloy, bar and rings, annealed and aged, tested at 650°C (1200°F)
- Haynes® 242™ alloy, bar and rings, annealed and aged, tested at 760°C (1400°F)
- Haynes® 242™ alloy, bar and rings, annealed and aged, tested at 870°C (1600°F)
- Haynes® 242™ alloy, bar and rings, annealed and aged, tested at 980°C (1800°F)
- Haynes® 242™ alloy, hot rolled plate, annealed and aged, tested at RT
- Haynes® 242™ alloy, hot rolled plate, annealed and aged, tested at 95°C (200°F)
- Haynes® 242™ alloy, hot rolled plate, annealed and aged, tested at 205°C (400°F)
- Haynes® 242™ alloy, hot rolled plate, annealed and aged, tested at 315°C (600°F)
- Haynes® 242™ alloy, hot rolled plate, annealed and aged, tested at 425°C (800°F)
- Haynes® 242™ alloy, hot rolled plate, annealed and aged, tested at 540°C (1000°F)
- Haynes® 242™ alloy, hot rolled plate, annealed and aged, tested at 650°C (1200°F)
- Haynes® 242™ alloy, hot rolled plate, annealed and aged, tested at 705°C (1300°F)
- Haynes® 242™ alloy, hot rolled plate, annealed and aged, tested at 760°C (1400°F)
- Haynes® 242™ alloy, hot rolled plate, annealed and aged, tested at 870°C (1600°F)
- Haynes® 242™ alloy, hot rolled plate, annealed and aged, tested at 980°C (1800°F)
- Haynes® 242™ alloy, cold rolled sheet, annealed and aged, tested at RT
- Haynes® 242™ alloy, cold rolled sheet, annealed and aged, tested at 95°C (200°F)
- Haynes® 242™ alloy, cold rolled sheet, annealed and aged, tested at 205°C (400°F)
- Haynes® 242™ alloy, cold rolled sheet, annealed and aged, tested at 315°C (600°F)
- Haynes® 242™ alloy, cold rolled sheet, annealed and aged, tested at 425°C (800°F)
- Haynes® 242™ alloy, cold rolled sheet, annealed and aged, tested at 540°C (1000°F)
- Haynes® 242™ alloy, cold rolled sheet, annealed and aged, tested at 650°C (1200°F)
- Haynes® 242™ alloy, cold rolled sheet, annealed and aged, tested at 705°C (1300°F)
- Haynes® 242™ alloy, cold rolled sheet, annealed and aged, tested at 760°C (1400°F)
- Haynes® 242™ alloy, cold rolled sheet, annealed and aged, tested at 870°C (1600°F)
- Haynes® 242™ alloy, cold rolled sheet, annealed and aged, tested at 980°C (1800°F)
- Haynes® 242™ alloy, cold reduced sheet, annealed, tested at RT
- Haynes® 242™ alloy, cold reduced sheet, annealed and 20% cold work, tested at RT
- Haynes® 242™ alloy, cold reduced sheet, annealed and 40% cold work, tested at RT
- Haynes® 242™ alloy, cold reduced sheet, annealed and aged, tested at RT
- Haynes® 242™ alloy, cold reduced sheet, annealed, 20% cold work, aged, tested at RT
- Haynes® 242™ alloy, cold reduced sheet, annealed, 40% cold work, aged, tested at RT
- Haynes® 242™ alloy, cold reduced sheet, annealed, 40% cold work, aged, tested at 595°C (900°F)
- Haynes® 242™ alloy, cold reduced sheet, annealed, 40% cold work, aged, tested at 650°C (1200°F)
- Haynes® 242™ alloy, cold reduced sheet, annealed, 40% cold work, aged, tested at 705°C (1300°F)
- Haynes® 242™ alloy, cold reduced sheet, annealed, 40% cold work, aged, tested at 760°C (1400°F)
- Haynes® 242™ alloy, after 0 hours exposure at 650°C (1200°F)
- Haynes® 242™ alloy, after 1000 hours exposure at 650°C (1200°F)
- Haynes® 242™ alloy, after 4000 hours exposure at 650°C (1200°F)
- Haynes® 242™ alloy, after 8000 hours exposure at 650°C (1200°F)
- Haynes® 25 alloy, cold rolled and 1205°C (2200°F) solution annealed sheet, tested at RT
- Haynes® 25 alloy, cold rolled and 1205°C (2200°F) solution annealed sheet, tested at 540°C (1000°F)
- Haynes® 25 alloy, cold rolled and 1205°C (2200°F) solution annealed sheet, tested at 650°C (1200°F)
- Haynes® 25 alloy, cold rolled and 1205°C (2200°F) solution annealed sheet, tested at 760°C (1400°F)
- Haynes® 25 alloy, cold rolled and 1205°C (2200°F) solution annealed sheet, tested at 870°C (1600°F)
- Haynes® 25 alloy, cold rolled and 1205°C (2200°F) solution annealed sheet, tested at 980°C (1800°F)
- Haynes® 25 alloy, cold rolled and 1205°C (2200°F) solution annealed sheet, tested at 1095°C (2000°F)
- Haynes® 25 alloy, hot rolled and 1230°C solution annealed sheet, tested at RT
- Haynes® 25 alloy, hot rolled and 1230°C solution annealed sheet, tested at 540°C (1000°F)
- Haynes® 25 alloy, hot rolled and 1230°C solution annealed sheet, tested at 650°C (1200°F)
- Haynes® 25 alloy, hot rolled and 1230°C solution annealed sheet, tested at 760°C (1400°F)
- Haynes® 25 alloy, hot rolled and 1230°C solution annealed sheet, tested at 870°C (1600°F)
- Haynes® 25 alloy, hot rolled and 1230°C solution annealed sheet, tested at 980°C (1800°F)
- Haynes® 25 alloy, vacuum investment castings, solution treated, tested at RT
- Haynes® 25 alloy, vacuum investment castings, solution treated, tested at 425°C (800°F)
- Haynes® 25 alloy, vacuum investment castings, solution treated, tested at 650°C (1200°F)
- Haynes® 25 alloy, vacuum investment castings, solution treated, tested at 760°C (1400°F)
- Haynes® 25 alloy, vacuum investment castings, solution treated, tested at 870°C (1600°F)
- Haynes® 25 alloy, vacuum investment castings, solution treated, tested at 980°C (1800°F)
- Haynes® 25 alloy, cold worked sheet, 10 % cold reduction, tested at 20°C (68°F)
- Haynes® 25 alloy, cold worked sheet, 10 % cold reduction, tested at 540°C (1000°F)
- Haynes® 25 alloy, cold worked sheet, 10 % cold reduction, tested at 650°C (1200°F)
- Haynes® 25 alloy, cold worked sheet, 10 % cold reduction, tested at 760°C (1400°F)
- Haynes® 25 alloy, cold worked sheet, 10 % cold reduction, tested at 870°C (1600°F)
- Haynes® 25 alloy, cold worked sheet, 10 % cold reduction, tested at 980°C (1800°F)
- Haynes® 25 alloy, cold worked sheet, 15 % cold reduction, tested at 20°C (68°F)
- Haynes® 25 alloy, cold worked sheet, 15 % cold reduction, tested at 540°C (1000°F)
- Haynes® 25 alloy, cold worked sheet, 15 % cold reduction, tested at 650°C (1200°F)
- Haynes® 25 alloy, cold worked sheet, 15 % cold reduction, tested at 760°C (1400°F)
- Haynes® 25 alloy, cold worked sheet, 15 % cold reduction, tested at 870°C (1600°F)
- Haynes® 25 alloy, cold worked sheet, 15 % cold reduction, tested at 980°C (1800°F)
- Haynes® 25 alloy, cold worked sheet, 20 % cold reduction, tested at 20°C (68°F)
- Haynes® 25 alloy, cold worked sheet, 20 % cold reduction, tested at 540°C (1000°F)
- Haynes® 25 alloy, cold worked sheet, 20 % cold reduction, tested at 650°C (1200°F)
- Haynes® 25 alloy, cold worked sheet, 20 % cold reduction, tested at 760°C (1400°F)
- Haynes® 25 alloy, cold worked sheet, 20 % cold reduction, tested at 980°C (1800°F)
- Haynes® 25 alloy, cold worked sheet, 15% cold reduction, aged at 370°C (700°F) for 1 hour, tested at 20°C (68°F)
- Haynes® 25 alloy, cold worked sheet, 15% cold reduction, aged at 370°C (700°F) for 1 hour, tested at 650°C (1200°F)
- Haynes® 25 alloy, cold worked sheet, 20% cold reduction, aged at 370°C (700°F) for 1 hour, tested at 20°C (68°F)
- Haynes® 25 alloy, cold worked sheet, 20% cold reduction, aged at 370°C (700°F) for 1 hour, tested at 540°C (1000°F)
- Haynes® 25 alloy, cold worked sheet, 20% cold reduction, aged at 370°C (700°F) for 1 hour, tested at 650°C (1200°F)
- Haynes® 25 alloy, cold worked sheet, 20% cold reduction, aged at 370°C (700°F) for 1 hour, tested at 760°C (1400°F)
- Haynes® 25 alloy, cold worked sheet, 20% cold reduction, aged at 370°C (700°F) for 1 hour, tested at 870°C (1600°F)
- Haynes® 25 alloy, cold worked sheet, 20% cold reduction, aged at 370°C (700°F) for 1 hour, tested at 980°C (1800°F)
- Haynes® 25 alloy, cold worked sheet, 20% cold reduction, aged at 595°C (1100°F) for 2 hours, tested at 20°C (68°F)
- Haynes® 25 alloy, cold worked sheet, 20% cold reduction, aged at 595°C (1100°F) for 2 hours, tested at 315°C (600°F)
- Haynes® 25 alloy, cold worked sheet, 20% cold reduction, aged at 595°C (1100°F) for 2 hours, tested at 540°C (1000°F)
- Haynes® 25 alloy, cold worked sheet, 20% cold reduction, aged at 595°C (1100°F) for 2 hours, tested at 650°C (1200°F)
- Haynes® 25 alloy, cold worked sheet, 20% cold reduction, aged at 595°C (1100°F) for 2 hours, tested at 760°C (1400°F)
- Haynes® 25 alloy, cold worked sheet, 20% cold reduction, aged at 595°C (1100°F) for 2 hours, tested at 870°C (1600°F)
- Haynes® 25 alloy, cold worked sheet, 20% cold reduction, aged at 595°C (1100°F) for 2 hours, tested at 980°C (1800°F)
- Haynes® 25 alloy, room temperature sheet
- Haynes® 25 alloy, room temperature sheet after 500 hours of 650°C exposure
- Haynes® 25 alloy, room temperature sheet after 1000 hours of 650°C exposure
- Haynes® 25 alloy, room temperature sheet after 2500 hours of 650°C exposure
- Haynes® 25 alloy, room temperature sheet after 100 hours of 760°C exposure
- Haynes® 25 alloy, room temperature sheet after 100 hours of 870°C exposure
- Haynes® 25 alloy, room temperature sheet after 500 hours of 870°C exposure
- Haynes® 25 alloy, room temperature sheet after 1000 hours of 870°C exposure
- Haynes® 25 alloy, room temperature after 0% cold reduction
- Haynes® 25 alloy, room temperature after 10% cold reduction
- Haynes® 25 alloy, room temperature after 15% cold reduction
- Haynes® 25 alloy, room temperature after 20% cold reduction
- Haynes® 25 alloy, room temperature after 25% cold reduction
- Haynes® 25 alloy, room temperature after 10% cold reduction, 1065°C anneal for 5 minutes
- Haynes® 25 alloy, room temperature after 15% cold reduction, 1065°C anneal for 5 minutes
- Haynes® 25 alloy, room temperature after 20% cold reduction, 1065°C anneal for 5 minutes
- Haynes® 25 alloy, room temperature after 25% cold reduction, 1065°C anneal for 5 minutes
- Haynes® 25 alloy, room temperature after 10% cold reduction, 1120°C anneal for 5 minutes
- Haynes® 25 alloy, room temperature after 15% cold reduction, 1120°C anneal for 5 minutes
- Haynes® 25 alloy, room temperature after 20% cold reduction, 1120°C anneal for 5 minutes
- Haynes® 25 alloy, room temperature after 25% cold reduction, 1120°C anneal for 5 minutes
- Haynes® 25 alloy, room temperature after 10% cold reduction, 1175°C anneal for 5 minutes
- Haynes® 25 alloy, room temperature after 15% cold reduction, 1175°C anneal for 5 minutes
- Haynes® 25 alloy, room temperature after 20% cold reduction, 1175°C anneal for 5 minutes
- Haynes® 25 alloy, room temperature after 25% cold reduction, 1175°C anneal for 5 minutes
- Haynes® 263 alloy, cold rolled sheet, solution treated and aged, tested at RT
- Haynes® 263 alloy, cold rolled sheet, solution treated and aged, tested at 540°C (1000°F)
- Haynes® 263 alloy, cold rolled sheet, solution treated and aged, tested at 650°C (1200°F)
- Haynes® 263 alloy, cold rolled sheet, solution treated and aged, tested at 760°C (1400°F)
- Haynes® 263 alloy, cold rolled sheet, solution treated and aged, tested at 870°C (1600°F)
- Haynes® 263 alloy, cold rolled sheet, solution treated and aged, tested at 980°C (1800°F)
- Haynes® 263 alloy, cold rolled sheet, solution treated and aged, tested at 1095°C (2000°F)
- Hastelloy® C-276 alloy, solution heat treated sheet, 2.0 mm thick, tested at RT
- Hastelloy® C-276 alloy, solution heat treated sheet, 2.0 mm thick, tested at 204°C (400°F)
- Hastelloy® C-276 alloy, solution heat treated sheet, 2.0 mm thick, tested at 316°C
- Hastelloy® C-276 alloy, solution heat treated sheet, 2.0 mm thick, tested at 427°C (800°F)
- Hastelloy® C-276 alloy, solution heat treated sheet, 2.4 mm thick, tested at 204°C (400°F)
- Hastelloy® C-276 alloy, solution heat treated sheet, 2.4 mm thick, tested at 316°C
- Hastelloy® C-276 alloy, solution heat treated sheet, 2.4 mm thick, tested at 427°C (800°F)
- Hastelloy® C-276 alloy, solution heat treated sheet, 1.6-4.7 mm thick, tested at 204°C (400°F)
- Hastelloy® C-276 alloy, solution heat treated sheet, 1.6-4.7 mm thick, tested at 316°C
- Hastelloy® C-276 alloy, solution heat treated sheet, 1.6-4.7 mm thick, tested at 427°C (800°F)
- Hastelloy® C-276 alloy, solution heat treated sheet, 1.6-4.7 mm thick, tested at 538°C (1000°F)
- Hastelloy® C-276 alloy, solution heat treated sheet, 4.8-25.4 mm thick, tested at 204°C (400°F)
- Hastelloy® C-276 alloy, solution heat treated sheet, 4.8-25.4 mm thick, tested at 316°C
- Hastelloy® C-276 alloy, solution heat treated sheet, 4.8-25.4 mm thick, tested at 427°C (800°F)
- Hastelloy® C-276 alloy, solution heat treated sheet, 4.8-25.4 mm thick, tested at 538°C (1000°F)
- Hastelloy® C-276 alloy, solution heat treated sheet, 25.4 mm thick, tested at RT
- Hastelloy® C-276 alloy, solution heat treated sheet, 25.4 mm thick, tested at 316°C
- Hastelloy® C-276 alloy, solution heat treated sheet, 25.4 mm thick, tested at 427°C (800°F)
- Haynes® 556™ alloy, cold rolled, solution annealed sheet, 0.8-2.8 mm thick, tested at RT
- Haynes® 556™ alloy, cold rolled, solution annealed sheet, 0.8-2.8 mm thick, tested at 540°C (1000°F)
- Haynes® 556™ alloy, cold rolled, solution annealed sheet, 0.8-2.8 mm thick, tested at 650°C (1200°F)
- Haynes® 556™ alloy, cold rolled, solution annealed sheet, 0.8-2.8 mm thick, tested at 760°C (1400°F)
- Haynes® 556™ alloy, cold rolled, solution annealed sheet, 0.8-2.8 mm thick, tested at 870°C (1600°F)
- Haynes® 556™ alloy, cold rolled, solution annealed sheet, 0.8-2.8 mm thick, tested at 980°C (1800°F)
- Haynes® 556™ alloy, cold rolled, solution annealed sheet, 0.8-2.8 mm thick, tested at 1095°C (2000°F)
- Haynes® 556™ alloy, hot rolled, solution annealed plate, 6.4-12.7 mm (1/2 in.) thick, tested at RT
- Haynes® 556™ alloy, hot rolled, solution annealed plate, 6.4-12.7 mm (1/2 in.) thick, tested at 540°C (1000°F)
- Haynes® 556™ alloy, hot rolled, solution annealed plate, 6.4-12.7 mm (1/2 in.) thick, tested at 650°C (1200°F)
- Haynes® 556™ alloy, hot rolled, solution annealed plate, 6.4-12.7 mm (1/2 in.) thick, tested at 760°C (1400°F)
- Haynes® 556™ alloy, hot rolled, solution annealed plate, 6.4-12.7 mm (1/2 in.) thick, tested at 870°C (1600°F)
- Haynes® 556™ alloy, hot rolled, solution annealed plate, 6.4-12.7 mm (1/2 in.) thick, tested at 980°C (1800°F)
- Haynes® 556™ alloy, hot rolled, solution annealed plate, 6.4-12.7 mm (1/2 in.) thick, tested at 1095°C (2000°F)
- Haynes® 556™ alloy, bar, after 0 hours at 650°C (1200°F)
- Haynes® 556™ alloy, bar, after 1000 hours at 650°C (1200°F)
- Haynes® 556™ alloy, bar, after 4000 hours at 650°C (1200°F)
- Haynes® 556™ alloy, bar, after 8000 hours at 650°C (1200°F)
- Haynes® 556™ alloy, bar, after 1000 hours at 760°C (1400°F)
- Haynes® 556™ alloy, bar, after 4000 hours at 760°C (1400°F)
- Haynes® 556™ alloy, bar, after 8000 hours at 760°C (1400°F)
|