 Scientific equipment and supplies for use in materials analysis.
AISI 1018 Steel, cold drawn
Subcategory: AISI 1000 Series Steel; Carbon Steel; Ferrous Metal; Low Carbon Steel; Metal
Key Words: carbon steels, AMS 5069, ASTM A108, UNS G10180, AS 1442 K1018 (Australia), AS 1443 K1018, CSN 12020 (Czech), CSN 12022, AFNOR NF A33-101 AF42C20, DIN 1.0453, DIN C16.8, DGN B-301 1018 (Mexico), COPANT 331 1018 (Pan America), COPANT 333 1018, MST.T (Russia), ST.20A, ST.3, ST.3T, GOST M18S, GOST 23570 18ps, GOST 23570 18sp, GOST 5520 18K, GOST 5521 S, NBN 629 D37-2 (Belgium), NBN 630 E37-1, NBN 630 E37-2, NBN A21-221 C17KD, BDS 9801 S (Bulgaria), GB 715 ML3 (China), TS 302 Fe35.2 (Turkey), TS 346 Fe35, BS 970 080A17, DEF STAN95-1-1 C1018
| Component | Wt. % |  | | | C | 0.14 - 0.2 | | | Fe | 98.81 - 99.26 | | | Mn | 0.6 - 0.9 | | | P | Max 0.04 | | | S | Max 0.05 | |
|
Material Notes: Medium low-carbon steel, has good weldability and slightly better machinability than the lower carbon steels.
| Physical Properties | Metric | English | Comments |
|
| Density | 7.87 g/cc | 0.284 lb/in³ | |
Mechanical Properties |
|
| Hardness, Brinell | 126 | 126 | |
| Hardness, Knoop | 145 | 145 | Converted from Brinell hardness. |
| Hardness, Rockwell B | 71 | 71 | Converted from Brinell hardness. |
| Hardness, Vickers | 131 | 131 | Converted from Brinell hardness. |
| Tensile Strength, Ultimate | 440 MPa | 63800 psi | |
| Tensile Strength, Yield | 370 MPa | 53700 psi | |
| Elongation at Break | 15 % | 15 % | In 50 mm |
| Reduction of Area | 40 % | 40 % | |
| Modulus of Elasticity | 205 GPa | 29700 ksi | Typical for steel |
| Bulk Modulus | 140 GPa | 20300 ksi | Typical for steel |
| Poisson's Ratio | 0.29 | 0.29 | Typical For Steel |
| Machinability | 70 % | 70 % | Based on AISI 1212 steel. as 100% machinability |
| Shear Modulus | 80 GPa | 11600 ksi | Typical for steel |
Electrical Properties |
|
| Electrical Resistivity | 1.59e-005 ohm-cm | 1.59e-005 ohm-cm | annealed condition; 0°C (32°F) |
| Electrical Resistivity at Elevated Temperature | 2.19e-005 ohm-cm | 2.19e-005 ohm-cm | annealed condition; 100°C (212°F) |
| Electrical Resistivity at Elevated Temperature | 2.93e-005 ohm-cm | 2.93e-005 ohm-cm | annealed condition; 200°C (390°F) |
Thermal Properties |
|
| Specific Heat Capacity | 0.486 J/g-°C | 0.116 BTU/lb-°F | annealed; 50-100°C (122-212°F) |
| Thermal Conductivity | 51.9 W/m-K | 360 BTU-in/hr-ft²-°F | estimated based on similar materials |
|
Printer friendly version |
References for this datasheet.
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.