Platinum, Pt, CP Grade, Annealed
Subcategory: Metal; Nonferrous Metal; Precious Metal; Pure Element
| Component | Wt. % |  | | | Pt | 99.95 | |
|
Material Notes: CP Grade (Commercially Pure) is 99.95% pure.
Click here to view available vendors for this material.
| Physical Properties | Original Value | Comments |
|
| Density | 21.45 g/cc | |
Mechanical Properties |
|
| Hardness, Vickers | 40 | |
| Tensile Strength, Ultimate | 125 - 165 MPa | |
| Elongation at Break | 35 % | in 50 mm |
| Modulus of Elasticity | 171 GPa | static in tension |
| Poisson's Ratio | 0.39 | |
| Shear Modulus | 62 GPa | Calculated value |
Electrical Properties |
|
| Electrical Resistivity | 1.06e-005 ohm-cm | Temperature Coefficient of resistivity is 0.0039/K. |
| Magnetic Susceptibility | 1.1e-006 | cgs/g |
Thermal Properties |
|
| Heat of Fusion | 113 J/g | |
| CTE, linear 20°C | 9.1 µm/m-°C | |
| Specific Heat Capacity | 0.134 J/g-°C | |
| Thermal Conductivity | 69.1 W/m-K | |
| Melting Point | 1769 °C | |
Optical Properties |
|
| Emissivity (0-1) | 0.152 | at 1000°C for total hemispherical |
| Emissivity (0-1) | 0.3 | 650 nm |
| Reflection Coefficient, Visible (0-1) | 0.7 | bulk Pt; 589 nm |
|