Antimony Telluride, Sb2Te3

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Ceramic; Semiconductor; Sulfide/Chalcogenide

Key Words: Chalcogenide; Semiconductor; Tellurium

Physical PropertiesOriginal ValueComments
Density6.44 g/cc 
a Lattice Constant4.25 Å 
c Lattice Constant30.3 Å 
Molecular Weight626.32 g/mol 

Electrical Properties
Band Gap0.3 eV 
Hole Mobility, cm²/V-s360 

Thermal Properties
Melting Point622 °C 

Descriptive Properties
CAS Number1327-50-0 
ColorGray 
Crystal StructureHexagonal-Rhombohedral Tetradymite Structure - R(-3)M
Printer friendly version Printer friendly version

References for this datasheet.


Free Trade Publications, Click Here!

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。