Bismuth Telluride, Bi2Te3 (Tellurobismuthite)
Subcategory: Ceramic; Semiconductor; Sulfide/Chalcogenide
Key Words: Chalcogenide; Semiconductor; Tellurium
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
| Physical Properties | Metric | English | Comments |
|
| Density | 7.73 g/cc | 0.279 lb/in³ | |
| a Lattice Constant | 4.38 Å | 4.38 Å | |
| c Lattice Constant | 30.45 Å | 30.45 Å | |
| Formula Units/Cell (Z) | 3 | 3 | |
| Molecular Weight | 800.76 g/mol | 800.76 g/mol | |
Mechanical Properties |
|
| Knoop Microhardness | 155 | 155 | N/mm² |
| Hardness, Mohs | 1.8 | 1.8 | |
Electrical Properties |
|
| Band Gap | 0.21 eV | 0.21 eV | |
| Electron Mobility, cm²/V-s | 1140 | 1140 | |
| Hole Mobility, cm²/V-s | 680 | 680 | |
Thermal Properties |
|
| Specific Heat Capacity | 0.016 J/g-°C | 0.00382 BTU/lb-°F | |
| Thermal Conductivity | 3 W/m-K | 20.8 BTU-in/hr-ft²-°F | |
| Melting Point | 585 °C | 1090 °F | |
Descriptive Properties | |
| CAS Number | 1304-82-1 | |
| Color | Gray | |
| Crystal Structure | Hexagonal-Rhombohedral | Tetradymite Structure - R(-3)M |
| Solubility | Insoluble in H2O; Soluble in EtOH | |
|
Printer friendly version |
References for this datasheet.
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.

|